Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Industrial Laminates/Norplex NP424 Laminate

Category Polymer , Thermoset , Carbon Fiber/Thermoset Composite
Manufacturer Industrial Laminates/Norplex
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Industrial Laminates/Norplex NP424 Laminate.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: Composite material composed of woven glass fabric surfaces and paper core combined with epoxy resin. Primarily used in the printed circuit board industry. Easy punching and excellent electrical properties and higher flexural strength than paper based grades. Provides excellent mechanical and electrical properties, and punches well up to .093".Thickness Tested: 0.062", 0.125" and 0.500"
Physical Properties Metric English Comments
Moisture Absorption at Equilibrium 0.25 %

@Thickness 1.57 mm
0.25 %

@Thickness 0.0620 in
ASTM D229
Mechanical Properties Metric English Comments
Hardness, Rockwell M 90 - 110

@Thickness 1.57 mm
90 - 110

@Thickness 0.0620 in
ASTM D785
Tensile Strength, Yield 235 MPa

@Thickness 1.57 mm
34100 psi

@Thickness 0.0620 in
CW; ASTM D638
310 MPa

@Thickness 1.57 mm
44900 psi

@Thickness 0.0620 in
LW; ASTM D638
Modulus of Elasticity 14.5 GPa

@Thickness 1.57 mm
2100 ksi

@Thickness 0.0620 in
CW; ASTM D229
17.2 GPa

@Thickness 1.57 mm
2500 ksi

@Thickness 0.0620 in
LW; ASTM D229
Flexural Strength 276 MPa

@Thickness 1.57 mm
40000 psi

@Thickness 0.0620 in
CW; ASTM D790
331 MPa

@Thickness 1.57 mm
48000 psi

@Thickness 0.0620 in
LW; ASTM D790
Compressive Strength 345 MPa

@Thickness 12.7 mm
50000 psi

@Thickness 0.500 in
ASTM D695
Shear Strength 86.2 MPa

@Thickness 15.7 mm
12500 psi

@Thickness 0.620 in
ASTM D732
Izod Impact, Unnotched 0.694 J/cm

@Thickness 12.7 mm
1.30 ft-lb/in

@Thickness 0.500 in
CW, Cond E-48/50; ASTM D256
0.908 J/cm

@Thickness 12.7 mm
1.70 ft-lb/in

@Thickness 0.500 in
LW, Cond E-48/50; ASTM D256
Thermal Properties Metric English Comments
CTE, linear 13.0 µm/m-°C

@Thickness 1.57 mm,
Temperature 20.0 °C
7.22 µin/in-°F

@Thickness 0.0620 in,
Temperature 68.0 °F
x-axis; IPC-TM 650-2.4.24
CTE, linear, Transverse to Flow 16.0 µm/m-°C

@Thickness 1.57 mm,
Temperature 20.0 °C
8.89 µin/in-°F

@Thickness 0.0620 in,
Temperature 68.0 °F
x-axis; IPC-TM 650-2.4.24
Maximum Service Temperature, Air 130 °C
266 °F
Flammability, UL94 V-0

@Thickness 1.57 mm
V-0

@Thickness 0.0620 in
Electrical Properties Metric English Comments
Arc Resistance 121 sec

@Thickness 3.17 mm
121 sec

@Thickness 0.125 in
ASTM D495
Comparative Tracking Index 300 V

@Thickness 3.17 mm
300 V

@Thickness 0.125 in
ASTM D3638
Descriptive Properties Value Comments
Bond Strength 1400 lb
0.5", ASTM D229
Color Tan