Teknor Apex Sinpolene TPP1010 Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 10% Talc Filler
Manufacturer Teknor Apex Company
Trade Name Sinpolene
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex Sinpolene TPP1010 Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: Africa & Middle East; Latin America; Asia Pacific; South America Talc Filler, 10% Filler by Weight Uses: Appliance Components; Housings Forms: Pellets Processing Method: Injection MoldingInformation Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 0.955 g/cc
0.955 g/cc
ASTM D792
Linear Mold Shrinkage 0.010 cm/cm
0.010 in/in
ASTM D955
Melt Flow 12.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
12.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 39.0 MPa
5660 psi
ASTM D638
Elongation at Break 42 %
42 %
ASTM D638
Flexural Strength 50.0 MPa
7250 psi
ASTM D790
Flexural Modulus 2.18 GPa
316 ksi
ASTM D790
Izod Impact, Notched 0.278 J/cm

@Temperature 22.8 °C
0.520 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 126 °C
259 °F
Unannealed; ASTM D648
Vicat Softening Point 153 °C
307 °F
Loading 1 (10N); ASTM D1525