Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 165 - 220 °C | 329 - 428 °F | Average value: 206 °C Grade Count:23 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant". Each property range of values re.. |
|||
Vicat Softening Point | 165 - 220 °C | 329 - 428 °F | Average value: 208 °C Grade Count:18 |
Overview of materials for Nylon 6, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of a.. |
|||
Vicat Softening Point | 217 - 220 °C | 423 - 428 °F | Average value: 219 °C Grade Count:3 |
Overview of materials for Nylon 610, Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610, Glass Reinforced". Each property range of values reported is minimum and maximum values of ap.. |
|||
Vicat Softening Point | 215 - 220 °C | 419 - 428 °F | Average value: 219 °C Grade Count:8 |
Overview of materials for Polyethersulfone (PES), 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% a.. |
|||
Vicat Softening Point | 150 - 220 °C | 302 - 428 °F | Average value: 194 °C Grade Count:7 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass + Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass + Mineral Filled". Each property range of values reported is min.. |
|||
Vicat Softening Point | 210 - 220 °C | 410 - 428 °F | Average value: 217 °C Grade Count:3 |
Overview of materials for Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant". Each property range of values re.. |
|||
Vicat Softening Point | 128 - 220 °C | 262 - 428 °F | Average value: 183 °C Grade Count:3 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified". Each property range of values reported.. |