Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 122 °C | 252 °F | STN EN ISO 306 |
Plastcom PLASTALEN® PH 91 SDU Polypropylene Modified homopolymer PP for injection molding. General use in all industry branches. Delivered in natural mode and in full RAL color.Information Provided by Plastcom spol. s r.o. |
|||
Vicat Softening Point | 122 °C | 252 °F | ASTM D1525 |
Network Polymers NPP 50-2053 Description: High Density Polyethylene (HDPE)Information provided by Network Polymers Inc. |
|||
Vicat Softening Point | 122 °C | 252 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Cycoloy® CE8510 PC+ABS (Europe-Africa-Middle East) Extrusion grade PC/ABS. Low viscosity, high impact and ductility.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Vicat Softening Point | 122 °C | 252 °F | Rate B/50; ASTM D 1525 |
SABIC Innovative Plastics Cycoloy® CY200FC PC+ABS (Europe-Africa-Middle East) High flow PC+ABS material designed for local Pacific Automotive applicationsThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Vicat Softening Point | 122 °C | 252 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Cycoloy® LG9000 PC+ABS (Europe-Africa-Middle East) CYCOLOY LG9000 is a low gloss PC+ABS injection moulding grade. LG9000 combines good impact / heat and UV resistance with a low gloss surface appearence. It is suitable for automotive interior applic.. |
|||
Vicat Softening Point | 122 °C | 252 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Lexan® ML1010 PC (Europe-Africa-Middle East) Superior performance, improved flow over standard grades at lower temperatures. Internal mold release.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Vicat Softening Point | 122 °C | 252 °F | |
Plastcom SLOVALEN PC 93 T 5 PP reinforced with 5% mineral filler Features: Modified PP for injection moulding with the content of 5% mineral filling. Increased rigidity, strength and thermal. Decreased shrinkage. General application in all industry branches.Packa.. |
|||
Vicat Softening Point | 122 °C | 252 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Cycoloy® CY200FC PC+ABS (Asia Pacific) High flow PC+ABS material designed for local Pacific Automotive applications |
|||
Vicat Softening Point | 122 °C | 252 °F | ASTM D1525 |
Chevron Phillips HiD® 9632 HDPE Blown Film Resin
(discontinued **) Characteristics: Copolymerization Enhances Film Toughness, Excellent Film Drawdown Ideally Suited for Thin Films Production, Lower Melt Index (Higher Molecular Weight) Results in Increased Film Stre.. |
|||
Vicat Softening Point | 122 °C | 252 °F | ASTM D1525 |
Chevron Phillips HiD® 9330 HDPE Natural Pipe Resin
(discontinued **) Resin Type: gas phase linear hexane copolymer; ASTM D3350 Classification 335520A; ASTM D4976 Classification: PE 235, A 55701Applications: base resin for use in utility and conduit pipe applicationsI.. |
|||
Vicat Softening Point | 122 °C | 252 °F | ASTM D1525 |
Chevron Phillips LX8119 HDPE Injection Molding Resin
(discontinued **) Resin Type: linear copolymer; ASTM D4976 Classification: PE 233, A 56700Characteristics: warp resistant, excellent impact strength, excellent ESCR, moderate shrinkage resistanceApplications: seats, .. |
|||
Vicat Softening Point | 122 °C | 252 °F | ASTM D1525 |
NOVA Chemicals Sclair® 35BE HDPE Extrusion Resin
(discontinued **) Features: Medium molecular weight HDPE, excellent ESCR, excellent toughness, good processability, outstanding abrasion resistance.Applications: Extrusion on to metal pipes to produce a corrosion res.. |
|||
Vicat Softening Point | 122 °C | 252 °F | ASTM D1525 |
NOVA Chemicals Sclair® 2607-UV14 HDPE Injection Molding Resin Excellent stiffness, Good impact resistance, Low warpageApplications: Roll-out cartsAdditives: Elevated levels of ultraviolet stabilizer packages, Elevated levels of antioxidantsInformation provided.. |
|||
Vicat Softening Point | 122 - 134 °C | 252 - 273 °F | Average value: 127 °C Grade Count:5 |
Overview of materials for High Density Polyethylene (HDPE), Sheet/Thermoforming Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Sheet/Thermoforming Grade". Each property range of values reported is .. |
|||
Vicat Softening Point | 122 °C | 252 °F | ASTM D1525 |
Iran Petrochemical (PCC) 52511 High Density Polyethylene 52511 is a HDPE copolymer injection molding grade for applications requiring a good balance between physical properties and flowability, like housewares and toys.Application: houseware, injection m.. |
|||
Vicat Softening Point | 122 °C | 252 °F | 10N, 50°C/hr; ISO 306 |
SABIC Innovative Plastics SABIC PPCOMPOUND 8620A PP SABIC® PPcompound 8620A is a mineral filled, impact modified polypropylene TPO. It was originally designed for painted automotive bumper fascia applications where a combination of good flow, hig.. |
|||
Vicat Softening Point | 122 °C | 252 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Valox® 364 PBT (Asia Pacific) Designed for outdoor telecommunications enclosure applications. |
|||
Vicat Softening Point | 122 °C | 252 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Xenoy® 1105 PBT+PC (Asia Pacific) PBT/PC blend, injection molding grade, non-reinforced, impact modified, excellent toughness at low temperatures, very good paintability |
|||
Vicat Softening Point | 122 °C | 252 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Xenoy® 5220U PBT+PC Unreinforced PBT+PC Alloy. Impact Modified. Improved retention of mechanical properties under UV exposure. Excellent low temperature impact and chemical resistance. |
|||
Vicat Softening Point | 122 °C | 252 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Xenoy® X3515 PC+POLYESTER (Asia Pacific) Flame Retardant, Impact Modified, Opaque, Designed for outdoor telecommunication enclosure applications.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Vicat Softening Point | 122 °C | 252 °F | ISO 306 |
Total Lumicene® mPE M 4040 Metallocene Polyethylene, Cast Film Lumicene® mPE M 4040 is a Lumicene® metallocene based Polyethylene with hexene as comonomer.Lumicene® mPE M 4040 can be processed at high output rates with low extrusion pressure, low neck-in, ex.. |
|||
Vicat Softening Point | 122 °C @Load 1.02 kg |
252 °F @Load 2.25 lb |
A50; ISO 306 |
Borealis BorPURE™ RD208CF Polypropylene Random Copolymer BorPure™ RD208CF is a random copolymer. This grade is suitable for the manufacturing of unoriented films on chill roll processes. This grade is suitable for the manufacturing of unoriented films o.. |
|||
Vicat Softening Point | 122 °C | 252 °F | 50°C/h 50N; ISO 306 |
Covestro Makroblend® KU 2-7940 Polycarbonate + PBT, Impact Grade Developmental productISO 7792-1-PC/PBT,MHPR,-020(PC+PBT)-blendsimpact modifiedInjection molding gradehigh toughness at low temperaturesunreinforcedPreprocessingMax. Water content |
|||
Vicat Softening Point | 122 °C @Load 5.10 kg |
252 °F @Load 11.2 lb |
120°C/h; ISO 306 |
Covestro Makroblend® UT5207 PC/PBT Blend Main characteristics:• High toughness even at low temperatures• Good chemical resistance• Good paintability• Good flowability• Low moisture intakeGrade characteristics:• Impact modified•.. |
|||
Vicat Softening Point | 122 °C | 252 °F | Rate A (50°C/h), Loading 1 (10 N); ASTM D1525 |
Entec Hypel® PEHD4/.955 HDPE Available in North America Features: Food Contact Acceptable and High DensityAgency Ratings: FDA 21 CFR 177.1520RoHS Compliant Form: Pellets Information provided by Entec |
|||
Vicat Softening Point | 122 °C | 252 °F | ASTM D1525 |
Dow DMDA-8980 NT 7 High Density Polyethylene Resin DOW DMDA-8980 NT 7 is produced using UNIPOL™ process technology. It is intended for use in thin wall injection molding applications such as food containers. Information provided by Dow |
|||
Vicat Softening Point | 122 °C | 252 °F | Method B; ASTM D-1525 |
Bhansali Engineering Abstron KU-650M ABS Super Heat Resistant High Heat Resistant Grades with Better Flow characteristicInformation provided by Bhansali |
|||
Vicat Softening Point | 122 °C | 252 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics NORYL PX2355 PPE+HIPS (Europe-Africa-Middle East) NORYL PX2355 is an unfilled, medium heat, low odour and low emission material with excellent heat aging performance. It has been developed for automotive interior applications, such as instrument pa.. |
|||
Vicat Softening Point | 122 °C | 252 °F | Method B; ASTM D-1525 |
Bhansali Engineering Abstron KU-650 ABS Super Heat Resistant High Heat Resistant Grades with Better Flow characteristicInformation provided by Bhansali |
|||
Vicat Softening Point | 122 °C | 252 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Valox® V3900WX PBT+PC (Europe-Africa-Middle East) PBT/PC blend - Unreinforced - Flame Retardant. This is a UV-stabilized grade designed for outdoor enclosure applications requiring UL 746C F1 weatherability performance. |