NOVA Chemicals Sclair® 35BE HDPE Extrusion Resin  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Extruded
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NOVA Chemicals Sclair® 35BE HDPE Extrusion Resin  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: Medium molecular weight HDPE, excellent ESCR, excellent toughness, good processability, outstanding abrasion resistance.Applications: Extrusion on to metal pipes to produce a corrosion resistant coating for buried pipe systems.Data provided by the manufacturer.
Physical Properties Metric English Comments
Density 0.946 g/cc
0.0342 lb/in³
ASTM D792
ESCR 100% Igepal® >= 1000 hour
>= 1000 hour
F50, condition B; ASTM D1693
Melt Flow 0.38 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.38 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 62
62
ASTM D2240
Tensile Strength, Yield 20.0 MPa
2900 psi
ASTM D638
Elongation at Break 500 %
500 %
ASTM D638
Flexural Modulus 0.565 GPa
81.9 ksi
ASTM D790
Thermal Properties Metric English Comments
Melting Point 129 °C
264 °F
ASTM D3417
Vicat Softening Point 122 °C
252 °F
ASTM D1525
Brittleness Temperature <= -70.0 °C
<= -94.0 °F
ASTM D696
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+17 ohm-cm
1.00e+17 ohm-cm
ASTM D257
Surface Resistance 1.00e+17 ohm
1.00e+17 ohm
insulation resistance
Dielectric Constant 2.34
2.34
ASTM 1531
Dissipation Factor 0.00010
0.00010
ASTM 1531
Processing Properties Metric English Comments
Melt Temperature 210 - 230 °C
410 - 446 °F