Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 110 - 210 °C | 230 - 410 °F | Average value: 176 °C Grade Count:14 |
Overview of materials for Nylon 612, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Unreinforced". Each property range of values reported is minimum and maximum values of approp.. |
|||
Vicat Softening Point | 50.0 - 210 °C | 122 - 410 °F | Average value: 145 °C Grade Count:55 |
Overview of materials for Polyether Ester Elastomer This property data is a summary of similar materials in the MatWeb database for the category "Polyether Ester Elastomer". Each property range of values reported is minimum and maximum values of appr.. |
|||
Vicat Softening Point | 165 - 210 °C | 329 - 410 °F | Average value: 183 °C Grade Count:5 |
Overview of materials for Polybutylene Terephthalate (PBT), PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), PTFE Filled". Each property range of values reported is minimum and ma.. |