Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 240 °C | 464 °F | STN EN ISO 306 |
Plastcom PLASTAMID® 66 GF 35 TS 002 PA66 reinforced with glass fiber, heat stabilized PA66 for injection molding, reinforced with 35 % glass fiber, heat stabilized, used in automotive, engineering and electrical industry, eg. intake pipes, cylinder heads, induction coils, carrying pa.. |
|||
Vicat Softening Point | 240 °C | 464 °F | B |
Plastcom SLOVAMID 66 GB 30 GF 20 PA66, 20% glass fibre, 30% glass beads FeaturesPA 66 chemically reinforced with 20% glass fibre and with the content of 30 % glass beads. Improved anisotropy of shrinkage. The relation of the anisotropy to the mechanical properties can b.. |
|||
Vicat Softening Point | 240 °C | 464 °F | B; STN EN ISO 306 |
Plastcom SLOVAMID 66 T 30 Polyamide 66, 30% Mineral Filled FeaturesPA 66 with the content of 30% chemically modified mineral filler. Used for holders of electric hand tools, hobby tools, gears, covers of electric tools, flat products, automobile wheel cove.. |
|||
Vicat Softening Point | 240 °C | 464 °F | 49 N; ISO 306, ASTM D1525 |
Nilit Nilamid A G5 FR PH2 25% Glass Fiber Reinforced, Flame Retardant PA66 (with Red Phosphorous) Description: Nilamid A G5 FR PH2 combines flame retardancy with outstanding mechanical performance. This product has a complete yellow card, with RTI and CTI listings. The formulation has been optim.. |
|||
Vicat Softening Point | 240 °C | 464 °F | 49 N; ISO 306, ASTM D1525 |
Nilit Nilamid A3 H G3 ZB 13% Glass Reinforced High Impact PA66 Description: Nilamid A3 H G3 ZB (13% Glass Reinforced) was developed for applications that require a combination of high stiffness and good elongation or impact resistance. It is widely used for app.. |
|||
Vicat Softening Point | 240 °C | 464 °F | 49 N; ASTM D1525 |
Nilit Polynil® P50 Standard Viscosity Nylon 66 Description: Standard viscosityApplication: CompoundingInformation provided by NILIT. |
|||
Vicat Softening Point | 240 °C @Load 5.001 kg |
464 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB SCANAMID 66 A33^E F45 Nylon 66, Glass Fiber Reinforced, Elastomer Modified Information provided by Polykemi AB |
|||
Vicat Softening Point | 240 °C @Load 5.10 kg |
464 °F @Load 11.2 lb |
50°C/h |
Radici Radiflam® A RV250AF (dry) Nylon 66-25GF Radiflam® A is a range of flame retardant polyamides 66 (PA 66) used for injection molding and extrusion for all applications where high fire resistance is required.Information provided by Radici g.. |
|||
Vicat Softening Point | 240 °C | 464 °F | 49 N; ASTM D1525 |
Nilit Polynil® P50FL Externally Lubricated, Lightly Nucleated Nylon 66 Description: Polynil P50FL is a general purpose injection molding grade that is widely used for gears, bearings, fasteners, clips.Key characteristics: Excellent flowGood toughnessGood overall mechan.. |
|||
Vicat Softening Point | 240 °C @Load 5.10 kg |
464 °F @Load 11.2 lb |
50°C/h |
Radici Radilon® A CF350 (dry) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Vicat Softening Point | 240 °C | 464 °F | DIN ISO 306 |
Lehmann & Voss LUVOCOM® 1301/GF/30/TF/15/BK PPS, linear, with glass fiber and PTFE Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w.. |
|||
Vicat Softening Point | 240 °C | 464 °F | DIN ISO 306 |
Lehmann & Voss LUVOCOM® 1301-7449 PPS, linear, with carbon fiber and PTFE Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.Improved friction and wear behaviour. Emergency runni.. |
|||
Vicat Softening Point | 240 °C | 464 °F | DIN ISO 306 |
Lehmann & Voss LUVOCOM® 1301-8456 PPS, linear, with glass fiber, PTFE, lubricant modified Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w.. |
|||
Vicat Softening Point | 240 °C | 464 °F | DIN ISO 306 |
Lehmann & Voss LUVOCOM® 1301-8524 PPS, linear, with glass fiber and PTFE Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w.. |
|||
Vicat Softening Point | 240 °C | 464 °F | DIN ISO 306 |
Lehmann & Voss LUVOCOM® 1-8379 Polyamide 66, with PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Vicat Softening Point | 240 °C @Load 5.00 kg |
464 °F @Load 11.0 lb |
|
LATI Latamid 66 H-V0 PA 66, Heat Stabilized, Flame Retardant Polyamide 66 (PA66) based compound. Heat stabilized. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin Am.. |
|||
Vicat Softening Point | 240 °C | 464 °F | DIN ISO 306 |
Lehmann & Voss PLASLUBE NY-1/TF/20/BK Polyamide 66, with PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Vicat Softening Point | 240 °C | 464 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Valox® V9280LW PET (Europe-Africa-Middle East) 40% Glassfiber / Mineral Filled PET, Impact Modifier, Mold Release, Heat StabilizedThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Vicat Softening Point | 240 °C | 464 °F | Rate A/50; ISO 306 |
SABIC Innovative Plastics NORYL GTX GTX964 PPE+PA (Europe-Africa-Middle East) NORYL GTX964 is an unfilled impact modified material with optimised processability. |
|||
Vicat Softening Point | 240 °C | 464 °F | ISO 306 |
Tisan TISLAMID® 66 30% Mineral Reinforced Nylon 66 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Vicat Softening Point | 240 °C | 464 °F | ISO 306 |
Tisan TISLAMID® 66 Flame Retardant (V0). Heat Stabilized Nylon 66 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Vicat Softening Point | 240 °C | 464 °F | B/120; ISO 306 |
Eurostar Staramide A28K PA66, Heat Stabilized, Injection Molding Staramide A28K is an Unreinforced and Heat Stabilized, Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Vicat Softening Point | 240 °C | 464 °F | B/120; ISO 306 |
Eurostar Staramide R1000 PA66, Injection Molded Staramide R1000 is an Unreinforced Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Vicat Softening Point | 240 °C | 464 °F | B/120; ISO 306 |
Eurostar Starflam AFR450X1 PA66, 25% Glass Filled, Injection Molded AFR450X1 is a Red Phosphorous, Flame Retardant, Glass Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppli.. |
|||
Vicat Softening Point | 240 °C | 464 °F | DAM; 50°C/h 50N; ISO 306 |
DuPont Performance Polymers Zytel® 101 NC010 Nylon 66
(Unverified Data**) Unreinforced Polyamide 66Zytel 101 NC010 is a general purpose polyamide 66 resin for injection molding and extrusion.Information provided by DuPont Performance Polymers |
|||
Vicat Softening Point | 240 °C @Load 5.10 kg |
464 °F @Load 11.2 lb |
50°C/h |
Radici Radilon® A 38 (dry) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Vicat Softening Point | 240 °C @Load 5.10 kg |
464 °F @Load 11.2 lb |
50°C/h |
Radici Radilon® A 42 (dry) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Vicat Softening Point | 240 °C @Load 5.10 kg |
464 °F @Load 11.2 lb |
50°C/h |
Radici Radilon® A HSK (dry) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Vicat Softening Point | 240 °C @Load 5.00 kg |
464 °F @Load 11.0 lb |
|
LATI Latilub 66-01M PA66, Molybdenum disulphide Filled Self-lubricating product based on Polyamide 66 (PA66). Molybdenum disulphide. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indus.. |
|||
Vicat Softening Point | 240 °C | 464 °F | 50 N; 120 °C/h; ISO 306 |
Lanxess Durethan® AKV 25 F30 000000 Nylon 66, 25% Glass Fiber PA 66, 25% glass fiber, injection molding, flame retardantInformation provided by LANXESS. |