Saint-Gobain CHR® K109 Polyimide Film Backing Acrylic Adhesive Pressure Sensitive Tape

Category Polymer , Tape , Thermoset , Polyimide, TS
Manufacturer Saint-Gobain Perfomance Plastics
Trade Name CHR®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Saint-Gobain CHR® K109 Polyimide Film Backing Acrylic Adhesive Pressure Sensitive Tape.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Polyimide films are employed because of their extreme heat resistance. Service temperatures range from -100°F to 500°F (-73°C to 260°C). These flame retardant films exhibit high tensile strength and conformability, good solvent resistance, excellent dielectric strength and good abrasion resistance. Polyimide tape applications include electrical insulation, capacitor, transformer and coil wrapping, electronic assembly, and wave solder protection. This tape uses an acrylic adhesive system. Acrylic adhesves perform in continuous operating temperatures from -40°F to +375°F (-40°C to +188°C). Benefits include exceptional solvent resistance, excellent adhesion to metal, superior weathering and aging characteristics. Acrylics have an excellent shelf life, and when exposed to elevated temperatures, their ability to wet-out improves thus increasing both adhesion and tack properties. All data based on a 0.0035 inch test sample.(Thickness given is for both backing and adhesive. Backing thickness is .002 inches.) Information provided by Saint Gobain Performance Products.
Mechanical Properties Metric English Comments
Elongation at Break 75 %
75 %
Tear Strength 8.77 kN/m
50.0 pli
Initial Tear Strength
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 177 °C
350 °F
Minimum Service Temperature, Air -28.9 °C
-20.0 °F
Electrical Properties Metric English Comments
Dielectric Strength 112 kV/mm
2850 kV/in
Dielectric Breakdown 10000 V
10000 V
Descriptive Properties Value Comments
Color Amber