Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arlon 51366X015 0.016" (0.406 mm) Uncured Silicone Rubber with Fiberglass Substrate

Category Polymer , Thermoset , Silicone , Silicone Rubber , Silicone, Molded, Glass Fiber Filled
Manufacturer Arlon
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon 51366X015 0.016" (0.406 mm) Uncured Silicone Rubber with Fiberglass Substrate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Design/Construction: Interleave: Polyethylene Side 1: Cured Silicone RubberSubstrate: Style 7628 Fiberglass Side 2: Uncured Silicone Rubber Flame Resistance: Product is designed to meet Title 14 CFR 25.856(a) Appendix F, Part VI (amdt. 25-111) flame resistance requirements but is not recognized by an FAA test Laboratory.This data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Division
Physical Properties Metric English Comments
Density 1.47 g/cc
0.0531 lb/in³
Silicone Property; Arlon SQA-TMS-024
Thickness 38.1 microns
1.50 mil
Interleave
63.5 microns
2.50 mil
Side 1; Arlon SQA-TMS-003
140 microns
5.50 mil
Side 2; Arlon SQA-TMS-003
203 microns
8.00 mil
Substrate; Arlon SQA-TMS-003
406 microns
16.0 mil
Overall; Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 66
66
Silicone Property; ASTM D2240
Tensile Strength 6.89 MPa
1000 psi
Silicone Property; ASTM D412
Elongation at Break 275 %
275 %
Silicone Property; ASTM D412
Peel Strength 0.526 kN/m
3.00 pli
(S1 to S2), Bond Strength; Arlon-SQA-TMS-011
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 232 °C
450 °F
Minimum Service Temperature, Air -56.7 °C
-70.0 °F
Electrical Properties Metric English Comments
Dielectric Strength 28.7 kV/mm
729 kV/in
ASTM D149
Processing Properties Metric English Comments
Cure Time 15.0 min

@Pressure 0.345 MPa,
Temperature 121 °C
0.250 hour

@Pressure 50.0 psi,
Temperature 250 °F
Recommended Cure Cycle
Shelf Life 6.00 Month

@Temperature 21.1 °C
6.00 Month

@Temperature 70.0 °F
From date of manufacture
Descriptive Properties Value Comments
Color Gray
White
Substrate
Total Product Weight (oz/yd2) 19.6
Arlon SQA-TMS-025