Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 210 µm/m-°C

@Temperature 20.0 °C
117 µin/in-°F

@Temperature 68.0 °F
LyondellBasell Lupolen® UHM 201 MDPE, Ultra-High Molecular Weight
For the production of very high abrasion and impact resistant parts with lower slip/stick friction, as well as higher stress crack and chemical resistance. Apart from anticorrosion products, this m..
CTE, linear, Parallel to Flow 210 µm/m-°C

@Temperature 20.0 °C
117 µin/in-°F

@Temperature 68.0 °F
LyondellBasell Lupolen® UHM 301 MDPE, Ultra-High Molecular Weight
For the production of very high abrasion and impact resistant parts with lower slip/stick friction, as well as higher stress crack and chemical resistance. Apart from anticorrosion products, this m..
CTE, linear, Parallel to Flow 210 µm/m-°C

@Temperature 23.0 - 60.0 °C
117 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP HX00059 PA11 (Europe-Africa-Middle East)
LNP * Lubricomp * HX00059 is a compound based on PA 11 resin, containing a Proprietary Lubricant. Added features include: Internally Lubricated.
CTE, linear, Parallel to Flow 210 µm/m-°C

@Temperature 20.0 °C
117 µin/in-°F

@Temperature 68.0 °F
Covestro Desmopan® 150 Thermoplastic Polyurethane
Desmopan 150 is a TPU on the basis of a standard ester.Applications: Ski boots, castors, shoe heels, technical injection molding parts.Information provided by Bayer.As of 1 September 2015, Bayer Mat..
CTE, linear, Parallel to Flow 210 µm/m-°C

@Temperature 20.0 °C
117 µin/in-°F

@Temperature 68.0 °F
Covestro Desmopan® 786 Thermoplastic Polyurethane
Desmopan 786 is a TPU on the basis of a special carbonate with very good microbe-resistance.Applications: Tabular films, films, profiles.Information provided by Bayer.As of 1 September 2015, Bayer M..
CTE, linear, Parallel to Flow 210 µm/m-°C
117 µin/in-°F
ISO 11359-1/-2
DuPont Performance Polymers Hytrel® HTR8685 BK022A Polyester Elastomer TPC-ET  (Unverified Data**)
44 Shore D Lubricated High Viscosity Polyester Elastomer with Superior Fatigue Resistance Developed for Blow Molding Hytrel HTR8685 BK022A is designed for blow molding or processing techniques requi..
CTE, linear, Parallel to Flow 210 µm/m-°C
117 µin/in-°F
ISO 11359-1/-2
DuPont Performance Polymers Hytrel® RS 40F3 NC010 Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D Renewably Sourced High Flow Polyester Elastomer Developed for Injection Molding Hytrel RS 40F3 NC010 is a high flow low modulus grade containing at least 50% renewably sourced ingredients..
CTE, linear, Parallel to Flow 210 µm/m-°C
117 µin/in-°F
ISO 11359-1/-2
DuPont Performance Polymers Hytrel® RS 40F5 NC010 Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D Renewably Sourced Medium Viscosity Polyester Elastomer Information provided by DuPont Performance Polymers
CTE, linear, Parallel to Flow 210 µm/m-°C

@Temperature 20.0 °C
117 µin/in-°F

@Temperature 68.0 °F
Arkema Group Pebax® 3533 SN 01 Polyether Block Amide (PEBA) (Conditioned)
POLYETHER BLOCK AMIDE (PEBA) hardness 35 shore D Non plasticized flexible Polyamide Outstanding mechanical properties at low temperature (-40°C) Applications: molded parts for sport goods (softness..
CTE, linear, Parallel to Flow 211 µm/m-°C

@Temperature -40.0 - 60.0 °C
117 µin/in-°F

@Temperature -40.0 - 140 °F
ASTM E 831
SABIC Innovative Plastics NORYL EM6100 PPE+PS (Asia Pacific)
Medium heat, high impact PPO/HIPS alloy used in the automotive industry.