Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 210 µm/m-°C @Temperature 20.0 °C |
117 µin/in-°F @Temperature 68.0 °F |
|
LyondellBasell Lupolen® UHM 201 MDPE, Ultra-High Molecular Weight For the production of very high abrasion and impact resistant parts with lower slip/stick friction, as well as higher stress crack and chemical resistance. Apart from anticorrosion products, this m.. |
|||
CTE, linear, Parallel to Flow | 210 µm/m-°C @Temperature 20.0 °C |
117 µin/in-°F @Temperature 68.0 °F |
|
LyondellBasell Lupolen® UHM 301 MDPE, Ultra-High Molecular Weight For the production of very high abrasion and impact resistant parts with lower slip/stick friction, as well as higher stress crack and chemical resistance. Apart from anticorrosion products, this m.. |
|||
CTE, linear, Parallel to Flow | 210 µm/m-°C @Temperature 23.0 - 60.0 °C |
117 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP HX00059 PA11 (Europe-Africa-Middle East) LNP * Lubricomp * HX00059 is a compound based on PA 11 resin, containing a Proprietary Lubricant. Added features include: Internally Lubricated. |
|||
CTE, linear, Parallel to Flow | 210 µm/m-°C @Temperature 20.0 °C |
117 µin/in-°F @Temperature 68.0 °F |
|
Covestro Desmopan® 150 Thermoplastic Polyurethane Desmopan 150 is a TPU on the basis of a standard ester.Applications: Ski boots, castors, shoe heels, technical injection molding parts.Information provided by Bayer.As of 1 September 2015, Bayer Mat.. |
|||
CTE, linear, Parallel to Flow | 210 µm/m-°C @Temperature 20.0 °C |
117 µin/in-°F @Temperature 68.0 °F |
|
Covestro Desmopan® 786 Thermoplastic Polyurethane Desmopan 786 is a TPU on the basis of a special carbonate with very good microbe-resistance.Applications: Tabular films, films, profiles.Information provided by Bayer.As of 1 September 2015, Bayer M.. |
|||
CTE, linear, Parallel to Flow | 210 µm/m-°C | 117 µin/in-°F | ISO 11359-1/-2 |
DuPont Performance Polymers Hytrel® HTR8685 BK022A Polyester Elastomer TPC-ET
(Unverified Data**) 44 Shore D Lubricated High Viscosity Polyester Elastomer with Superior Fatigue Resistance Developed for Blow Molding Hytrel HTR8685 BK022A is designed for blow molding or processing techniques requi.. |
|||
CTE, linear, Parallel to Flow | 210 µm/m-°C | 117 µin/in-°F | ISO 11359-1/-2 |
DuPont Performance Polymers Hytrel® RS 40F3 NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D Renewably Sourced High Flow Polyester Elastomer Developed for Injection Molding Hytrel RS 40F3 NC010 is a high flow low modulus grade containing at least 50% renewably sourced ingredients.. |
|||
CTE, linear, Parallel to Flow | 210 µm/m-°C | 117 µin/in-°F | ISO 11359-1/-2 |
DuPont Performance Polymers Hytrel® RS 40F5 NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D Renewably Sourced Medium Viscosity Polyester Elastomer Information provided by DuPont Performance Polymers |
|||
CTE, linear, Parallel to Flow | 210 µm/m-°C @Temperature 20.0 °C |
117 µin/in-°F @Temperature 68.0 °F |
|
Arkema Group Pebax® 3533 SN 01 Polyether Block Amide (PEBA) (Conditioned) POLYETHER BLOCK AMIDE (PEBA) hardness 35 shore D Non plasticized flexible Polyamide Outstanding mechanical properties at low temperature (-40°C) Applications: molded parts for sport goods (softness.. |