Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 26.0 µm/m-°C @Temperature 40.0 - 120 °C |
14.4 µin/in-°F @Temperature 104 - 248 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP KONDUIT OX11314 PPS (Asia Pacific) Thermally conductive mineral filled PPS FR compound |
|||
CTE, linear, Parallel to Flow | 26.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
14.4 µin/in-°F @Temperature 73.4 - 131 °F |
ASTM E831 |
Lavergne VYPET VNT 840 PET 40% Glass-Mineral Reinforced Vypet VNT 840 is a 40% glass/mineral reinforced PET injection molding compound designed for electrical and structural applications, with High Dielectric Strength Features: High temperature performan.. |
|||
CTE, linear, Parallel to Flow | 26.0 µm/m-°C @Temperature 23.0 - 150 °C |
14.4 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics ULTEM 2100 PEI (Europe-Africa-Middle East) 10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
CTE, linear, Parallel to Flow | 26.0 µm/m-°C @Temperature 23.0 - 150 °C |
14.4 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics ULTEM 2100F PEI (Europe-Africa-Middle East) 10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. US FDA and European Food Contact approved. Effective June, 2007 this grade will no l.. |
|||
CTE, linear, Parallel to Flow | 26.0 µm/m-°C @Temperature 23.0 - 150 °C |
14.4 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics ULTEM 2110 PEI (Europe-Africa-Middle East) 10% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
CTE, linear, Parallel to Flow | 26.0 µm/m-°C @Temperature 23.0 - 150 °C |
14.4 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics ULTEM 2110R PEI (Europe-Africa-Middle East) 10% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C) with internal mold release. Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
CTE, linear, Parallel to Flow | 26.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
14.4 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP WFL36 PBT (Europe-Africa-Middle East) LNP* Lubricomp* WFL36 is a compound based on Polybutylene Terephalate resin containing Glass Fiber, PTFE. |
|||
CTE, linear, Parallel to Flow | 26.0 µm/m-°C @Temperature 23.0 - 150 °C |
14.4 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics ULTEM PW2100 PEI (Europe-Africa-Middle East) 10% Glass fiber filled, standard flow Polyetherimide (Tg 217°C). Specific grade-colors are designed and certified for use in Potable Water applications. KTW, WRAS, ACS, NSF-61 and W270 certified... |
|||
CTE, linear, Parallel to Flow | 26.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
14.4 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP OF008A PPS (Asia Pacific) LNP* Thermocomp* OF008A is a compound based on PPS - Branched resin containing Glass Fiber.This product is also known as Thermocomp* OF-1008. |
|||
CTE, linear, Parallel to Flow | 26.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
14.4 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP OF008AH PPS - Branched LNP* THERMOCOMP* OF008AH is a compound based on PPS - Branched resin containing 40% Glass Fiber. Added features of this grade are: Healthcare. |
|||
CTE, linear, Parallel to Flow | 26.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
14.4 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Thermocomp OF008E PPS LNP* Thermocomp* OF008E is a compound based on Polyphenylene Sulfide resin containing Glass Fiber. Added features of this material include: Easy Molding.This data was supplied by SABIC-IP for the A.. |
|||
CTE, linear, Parallel to Flow | 26.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
14.4 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP OF008E PPS - LINEAR LNP* THERMOCOMP* OF008E is a compound based on PPS - Linear resin containing 40% Glass Fiber. Added features of this material include: Easy Molding. |
|||
CTE, linear, Parallel to Flow | 26.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
14.4 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP RF007ES PA 66 LNP* THERMOCOMP* RF007ES is a compound based on Nylon 66 resin containing 35% Glass Fiber. Added features of this material include: Heat Stabilized, Easy Molding. |
|||
CTE, linear, Parallel to Flow | 26.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
14.4 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP RF009S PA 66 LNP* THERMOCOMP* RF009S is a compound based on Nylon 66 resin containing 45% Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
CTE, linear, Parallel to Flow | 26.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
14.4 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP RF00ASXS PA6.6 (Europe-Africa-Middle East) LNP* Thermocomp* RF00ASXS is a compound based on PA 66 resin containing Glass Fiber. Added features include: Heat Stabilized. |
|||
CTE, linear, Parallel to Flow | 26.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
14.4 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOTUF WF006I PBT (Europe-Africa-Middle East) LNP* Thermotuf* WF006I is a compound based on Polybutylene Terephalate resin containing Glass Fiber. Added features of this material include: High Impact. |
|||
CTE, linear, Parallel to Flow | 26.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
14.4 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP 2F006 ETFE LNP* THERMOCOMP* 2F006 is a compound based on ETFE containing 30% Glass Fiber. |
|||
CTE, linear, Parallel to Flow | 26.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
14.4 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP OF008A PPS - Branched LNP* THERMOCOMP* OF008A is a compound based on PPS - Branched resin containing 40% Glass Fiber. |
|||
CTE, linear, Parallel to Flow | 26.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
14.4 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP OF008A PPS - Branched (Europe-Africa-Middle East) LNP* Thermocomp* OF008A is a compound based on PPS - Branched resin containing Glass Fiber. |
|||
CTE, linear, Parallel to Flow | 26.0 µm/m-°C @Temperature 20.0 °C |
14.4 µin/in-°F @Temperature 68.0 °F |
|
Covestro Bayblend® T 88-4N Polycarbonate/ABS Blend, 20% Glass Fiber Contains 20% glass fiber reinforcement, high stiffness.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – .. |
|||
CTE, linear, Parallel to Flow | 26.0 µm/m-°C | 14.4 µin/in-°F | DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® 73G30HSL BK416 Nylon 6
(Unverified Data**) 30% Glass Reinforced Heat Stabilized Polyamide 6 Zytel 73G30HSL BK416 is a 30% glass fiber reinforced heat stabilized lubricated black polyamide 6 resin for injection molding.Information provided by.. |
|||
CTE, linear, Parallel to Flow | 26.0 µm/m-°C @Temperature -40.0 - 23.0 °C |
14.4 µin/in-°F @Temperature -40.0 - 73.4 °F |
DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® 77G33L BK031 Nylon 612
(Unverified Data**) 33% Glass Reinforced Polyamide 612 Zytel 77G33L BK031 is a 33% glass fiber reinforced black polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
CTE, linear, Parallel to Flow | 26.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
14.4 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP DFL44 PC (Europe-Africa-Middle East) LNP* Lubricomp* DFL44 is a compound based on Polycarbonate resin containing Glass Fiber, PTFE. |
|||
CTE, linear, Parallel to Flow | 26.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
14.4 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP VERTON RX970079 PA 66 (Europe-Africa-Middle East) LNP* VERTON* RX970079 is a compound based on PA 66 resin containing Long Glass Fiber and PTFE. Added features include; Internally Lubricated. |
|||
CTE, linear, Parallel to Flow | 26.0 µm/m-°C @Temperature 20.0 °C |
14.4 µin/in-°F @Temperature 68.0 °F |
ASTM E831 |
Sumitomo Bakelite North America FM 3000 Cellulose Reinforced Phenolic Novolac FM 3000 is a self-lubricated cellulose reinforced phenolic molding compound, modified for applications requiring reduced friction and low wear. Information supplied by Sumitomo Bak North America... |
|||
CTE, linear, Parallel to Flow | 26.0 µm/m-°C @Temperature 20.0 °C |
14.4 µin/in-°F @Temperature 68.0 °F |
ASTM E-831 |
Sumitomo Bakelite North America TEM 9053C Hardware Grade Epoxy Short fiberglass and mineral filled, toughened epoxy molding compound with excellent dimensional stability and high strength properties.Information provided by Vyncolit, a Sumitomo Bak Group |