Polymer Property : CTE, linear, Parallel to Flow = 22.8 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 41.0 µm/m-°C
22.8 µin/in-°F
ASTM D696
LG Chemical LUMID GP2251AF PA6+GF25%, Flame Retardant
Feature: Injection Molding, PA6+GF25%, Flame RetardantApplication: IT/OA (Micro Switch)CAS No. 25038-54-4, 65997-17-3, 88497-56-7, 1309-64-4 and 138265-88-0Information provided by LG Chemical
CTE, linear, Parallel to Flow 41.0 µm/m-°C
22.8 µin/in-°F
ASTM D696
LG Chemical LUMID GP2259AFL PA6+GF25%, Flame Retardant
Feature: Injection Molding, PA6+GF25%, Flame RetardantApplication: IT/OA (Connector)CAS No. 25038-54-4, 65997-17-3, 1163-19-5, 1309-64-4 and 138265-88-0Information provided by LG Chemical
CTE, linear, Parallel to Flow 41.0 µm/m-°C

@Temperature -30.0 - 100 °C
22.8 µin/in-°F

@Temperature -22.0 - 212 °F
ISO 11359-2
SABIC Innovative Plastics SABIC PPCOMPOUND 8620 PP
SABIC® PPcompound 8620 is a mineral filled, impact modified polypropylene TPO. This material combines scratch resistance and good flow with exterior automotive weathering stability. It was origin..
CTE, linear, Parallel to Flow 41.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
22.8 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP LUBRICOMP UX06425 PPA
LNP* LUBRICOMP* UX06425 is a compound based on Polyphthalamide (PPA) containing 10% Glass Fiber, 10% PTFE. Added features of this material include: Wear Resistant, Hot Water Moldable and Heat Stab..
CTE, linear, Parallel to Flow 41.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
22.8 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRILOY RF203 PA 66 (Europe-Africa-Middle East)
LNP* LUBRILOY* RF203 is a compound based on PA 66 resin containing Glass Fiber, Proprietary Lubricant. Added features include: Internally Lubricated.
CTE, linear, Parallel to Flow 41.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
22.8 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP STAT-KON DFD02EXC PC (Europe-Africa-Middle East)
LNP* Stat-kon* DFD02EXC is a compound based on Polycarbonate resin containing Glass Fiber, Carbon Powder. Added features of this material include: Electrically Conductive.
CTE, linear, Parallel to Flow 41.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
22.8 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP THERMOCOMP RF002SXS PA 66
LNP* THERMOCOMP* RF002SXS is a compound based on Nylon 66 resin contaning 10% Glass Fiber. Characteristcs of this grade are: Heat Stabilized.
CTE, linear, Parallel to Flow 41.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
22.8 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP THERMOCOMP 9X02841 PBT+PC
LNP* Thermocmop* 9X02841 is a PBT/Polycarbonate blend containing proprietary fillers.
CTE, linear, Parallel to Flow 41.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
22.8 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP THERMOTUF VF006U Super Tough Nylon
LNP* Thermotuf* VF006U is a compound based on Super Tough Nylon containing Glass Fiber. Characteristics of this grade are High Impact.
CTE, linear, Parallel to Flow 41.0 µm/m-°C
22.8 µin/in-°F
DAM; ISO 11359-1/-2
DuPont Performance Polymers Minlon® 22C BK086 Nylon 66  (Unverified Data**)
38% Mineral/Glass Reinforced Polyamide 66 Minlon 22C BK086 is a 38% mineral/glass reinforced heat stabilized black polyamide 66 resin for injection molding.Information provided by DuPont Performance..
CTE, linear, Parallel to Flow 41.0 µm/m-°C
22.8 µin/in-°F
DAM; ISO 11359-1/-2
DuPont Performance Polymers Minlon® 73GM40 NC010 Nylon 6  (Unverified Data**)
40% Mineral/Glass Reinforced Polyamide 6 Minlon 73GM40 NC010 is a 40% mineral/glass reinforced heat stabilized polyamide 6 resin for injection molding.Information provided by DuPont Performance Poly..
CTE, linear, Parallel to Flow 41.0 µm/m-°C

@Temperature 20.0 °C
22.8 µin/in-°F

@Temperature 68.0 °F
Arkema Group Rilsan® AZM 15 TLD Nylon 12, 15% Glass Fiber Filled (Dry)
Designation ISO 1874-PA12,MHLR,16-030,GF15Rigid grade with glass fiber filler (15%) for injection molding.Available color: natural. Light and heat stabilized. Mold-release agent.Rigidity combined wi..