Material Notes:
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 30% Filler by WeightAdditive: LubricantFeatures: Flame Retardant and LubricatedInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.68 g/cc
0.0607 lb/in³
ASTM D792
Water Absorption 0.90 %

@Time 86400 sec
0.90 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.014 cm/cm

@Thickness 3.17 mm
0.014 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 119
119
ASTM D785
Tensile Strength, Yield 72.4 MPa
10500 psi
ASTM D638
Elongation at Break 3.0 %
3.0 %
ASTM D638
Flexural Strength 110 MPa
16000 psi
ASTM D790
Flexural Modulus 4.14 GPa
600 ksi
ASTM D790
Izod Impact, Notched 0.320 J/cm

@Thickness 3.17 mm
0.600 ft-lb/in

@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched 2.03 J/cm

@Thickness 3.17 mm
3.80 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 59.4 µm/m-°C
33.0 µin/in-°F
ASTM D696
Melting Point 255 °C
491 °F
Deflection Temperature at 0.46 MPa (66 psi) 232 °C
450 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 210 °C
410 °F
Unannealed; ASTM D648
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
ASTM D257
Dielectric Strength 16.1 kV/mm
410 kV/in
Method A (Short-Time); ASTM D149
Users viewing this material also viewed the following: