Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 111 °C | 232 °F | Internal method |
Polimeri Europa Clearflex® MQ F0 Very Low Density Polyethylene Clearflex MQ F0 is a linear polyethylene, with antioxidants, characterized by a very low density (VLDPE).The resin shows an excellent balance between flexibility and impact resistance.Main Applicati.. |
|||
Melting Point | 111 °C | 232 °F | Internal method |
Polimeri Europa Riblene® FF 24 Low Density Polyethylene - Blown Film Extrusion Riblene FF 24 is a high molecular weight low density polyethylene (LDPE), with added slip and antiblocking agents, suitable for blown film extrusion. Riblene FF 24 is characterized by a good melt s.. |
|||
Melting Point | 111 °C | 232 °F | Internal method |
Polimeri Europa Riblene® GM 20 R Low Density Polyethylene - Coating Grade Riblene GM 20 R is a medium fluidity low density polyethylene resin (LDPE).Main Applications: Riblene GM 20 R is suitable for coating applications where a low neck-in is required. Moreover, for it.. |
|||
Melting Point | 111 °C | 232 °F | Internal method |
Polimeri Europa Riblene® MR 30 Low Density Polyethylene - Injection Molding Riblene MR 30 is a high fluidity low density polyethylene resin (LDPE) characterized by a high flowability and a medium rigidity.Parts made with Riblene MR 30 are characterized by good mechanical an.. |
|||
Melting Point | 111 °C | 232 °F | ASTM D3418 |
Petroquimica Triunfo Trithene® SX 7010 LDPE - Blow Molding The Trithene® SX 7010 resin is a medium molecular weight, low-density polyethylene (LDPE) which allows the production of flasks with an adequate combination of mechanical and impact strength, flexi.. |
|||
Melting Point | 111 °C | 232 °F | ASTM D3418 |
Petroquimica Triunfo Trithene® SX 7012 LDPE - Blow Molding The Trithene SX 7012 resin is a low density polyethylene (LDPE) with medium molecular weight which allows the production of flasks with an adequate combination of mechanical and impact strength, fle.. |
|||
Melting Point | 111 °C | 232 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil LD 136.NI Packaging Film Resin
(discontinued **) LD 136 series resins are homopolymer film resins with good clarity. They are suitable for processing in cast film equipment. Applications include food packaging, textile packaging, and other packa.. |
|||
Melting Point | 111 °C | 232 °F | |
LyondellBasell Lupolen® 2210 H SK LDPE Cable sheathingData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Melting Point | 111 °C | 232 °F | |
LyondellBasell Lupolen® 2410 T LDPE, Injection Molding Grade Injection moldingsData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Melting Point | 111 °C | 232 °F | |
LyondellBasell Lupolen® 2420 F LDPE Film, blow moldings.Data was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Melting Point | 111 °C | 232 °F | |
LyondellBasell Lupolen® 2420 K LDPE, Film Grade FilmData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Melting Point | 111 °C | 232 °F | |
LyondellBasell Lupolen® 2426 F LDPE, Film Grade FilmData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Melting Point | 111 °C | 232 °F | |
LyondellBasell Lupolen® 2452 D SW 413 LDPE Cable sheathingData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Melting Point | 111 °C | 232 °F | DSC; ASTM D3418 |
ICO Polymers ICOFLOâ„¢ 510-5018 400 Micron LDPE Powder Description: ICOFLO 510-5018 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Melting Point | 111 °C | 232 °F | DSC; ASTM D3418 |
ICO Polymers ICOFLOâ„¢ 510-5054 800 Micron LDPE Powder Description: ICOFLO 510-5054 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Melting Point | 111 °C | 232 °F | DSC; ASTM D3418 |
ICO Polymers ICOFLOâ„¢ 510-5055 1200 Micron LDPE Powder Description: ICOFLO 510-5055 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Melting Point | 111 °C | 232 °F | ISO 11357-3 |
Borealis FA6224 Low Density Polyethylene FA6224 is a Low Density Polyethylene for Film Extrusion. Autoclave Technology. Contains Antioxidant, Anti-block and Medium Slip additives. This grade is developed for the production of thin blown f.. |
|||
Melting Point | 111 °C | 232 °F | ISO 11357-3 |
Borealis FA7220 Low Density Polyethylene FA7220 is a Low Density Polyethylene for Film Extrusion. Includes Antioxidant. This grade is developed for production of blown film or cast film with good optical properties. When cast on a polish.. |
|||
Melting Point | 111 °C | 232 °F | ISO 11357-3 |
Borealis FA7224 Low Density Polyethylene FA7224 has been developed for applications such as: Thin bags with excellent optical and slip properties, and laundry and other textile bags. Contains antioxidant.Information provided by Borealis AG.. |
|||
Melting Point | 111 °C | 232 °F | ISO 11357-3 |
Borealis FA7229 Low Density Polyethylene FA7229 is a Low Density Polyethylene for Film Extrusion. Includes Antioxidant and Cling additive. Applications: food wrap film, lamination films, blending, and other blown cling film.Information pr.. |
|||
Melting Point | 111 °C | 232 °F | Freezing point via DSC/ASTM D3418 |
DuPont Bynel® 41E556 Anhydride-Modified LLDPE Adhesive Resin Bynel® Series 4100 resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All 4100 Series resins are available in pellet form for use in conventional extrusion and coextrusi.. |
|||
Melting Point | 111 °C | 232 °F | ISO 11357 |
Total LDPE LD 0304 Low Density Polyethylene - Extrusion Coating LDPE LA 0304 is a low density polyethylene made by a high pressure autoclave process without antioxidant.Application examples: coating of paper, paperboard, aluminum.Information provided by Total Pe.. |
|||
Melting Point | 111 °C | 232 °F | ASTM D-3418 |
Chevron Phillips MarFlex® 2121 Polyethylene; LDPE Low density polyethylene. This LDPE is tailored for cast film applications that require: Good processabilityGood drawdownEdge tear resistanceLow neck-in Applications: Typical cast film applicatio.. |
|||
Melting Point | 111 °C | 232 °F | ASTM D3418 |
Chevron Phillips MarFlex® 5430 Low Density Polyethylene, Cast Film This LDPE is tailored for cast film applications that require:Excellent opticsEasy processingHigh coefficient of frictionTypical cast film applications include:OverwrapCoextruded filmGeneral purpose.. |
|||
Melting Point | 111 °C | 232 °F | ASTM D3418 |
Chevron Phillips MarFlex® 5440 Low Density Polyethylene, Cast Film This LDPE is tailored for cast film applications that require:Suited for high speed convertingGood clarityLow coefficient of frictionTypical cast film applications include:Coextruded filmGeneral pur.. |
|||
Melting Point | 111 °C | 232 °F | Freezing Point; ASTM D3418 |
DuPont™ Fusabond® E265 Polymer Modifier DuPont™ Fusabond® E265 is an anhydride modified high density polyethylene. Used as a polymer modifier |
|||
Melting Point | 111 °C | 232 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil LD 105.30 Very High Clarity Packaging Film Resin Product Description: LD 105 resins are homopolymer packaging film resins designed for applications requiring outstanding clarity with good stiffness. These resins can be processed in either blown or.. |
|||
Melting Point | 111 °C | 232 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil LD 105.BR Very High Clarity Packaging Film Resin Product Description: LD 105 resins are homopolymer packaging film resins designed for applications requiring outstanding clarity with good stiffness. These resins can be processed in either blown or.. |
|||
Melting Point | 111 °C | 232 °F | |
LyondellBasell Lupolen® 2424 H LDPE, Film Grade FilmData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Melting Point | 111 °C | 232 °F | Freezing Point, DSC; ASTM D3418 |
DuPont Bynel® 50E631 Adhesive Resin
(discontinued **) Bynel® Series 5000 resins are anhydride-modified polypropylene. Bynel® 50E631 is based on polypropylene homopolymer. They are available in pellet form for use in conventional extrusion and coextru.. |