Thermal Properties Metric English Comments
Melting Point 136 °C
277 °F
Plastcom SLOVALEN PC 71 GF 10 PP, 10% glass fibre
FeaturesCompouded homopolymer PP, with the content of 10% chemically bound glass fibre and modifier of mechanical properties. Increased strength in comparison with unfilled PP. Use in all industry s..
Melting Point 136 °C
277 °F
Exxon Method
ExxonMobil Escorene® HD-6908 HDPE, Injection Grade  (discontinued **)
Data Provided by Exxon Chemical Canada.Characteristics: Excellent Stiffness, Good ImpactUses: Crates, Pails, Industrial containers
Melting Point 136 °C
277 °F
Melting point via DSC/ASTM D3418
DuPont Bynel® 4003 Anhydride-Modified HDPE Adhesive Resin  (discontinued **)
Bynel® Series 4000 resins are anhydride-modified, high-density polyethylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process..
Melting Point 136 °C
277 °F
Melting point via DSC/ASTM D3418
DuPont Bynel® 4006 Anhydride-Modified HDPE Adhesive Resin  (discontinued **)
Bynel® Series 4000 resins are anhydride-modified, high-density polyethylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process..
Melting Point 136 °C
277 °F
DuPont Fusabond® MB100D High Density Polyethylene  (discontinued **)
Typical Use: CompatibilizerCoupling agent for nonhalogen, flame retarded wire and cable compounds containing fillers such as aluminum trihydrate or magnesium hydroxideNatural fiber wood-plastic comp..
Melting Point 136 °C
277 °F
ASTM D3418
ExxonMobil HD 6908.18 Injection Molding Resin  (discontinued **)
HD 6908 is a homopolymer with outstanding stiffness with a good balance of processability and cold temperature impact performance. This resin is ideally suited for articles requiring very high stif..
Melting Point 136 °C
277 °F
ISO 3146
Total Lacqtene® 2007 TN 61 HDPE pipe  (discontinued **)
LACQTENE® 2007 TN 61 is a high density homopolymer polyethylene produced by the gas phase polymerization process.LACQTENE® 2007 TN 61 is best processed between 190 and 230°C.Information provided ..
Melting Point 136 °C
277 °F
LyondellBasell Lupolen® UHM 201 MDPE, Ultra-High Molecular Weight
For the production of very high abrasion and impact resistant parts with lower slip/stick friction, as well as higher stress crack and chemical resistance. Apart from anticorrosion products, this m..
Melting Point 136 °C
277 °F
LyondellBasell Lupolen® UHM 301 MDPE, Ultra-High Molecular Weight
For the production of very high abrasion and impact resistant parts with lower slip/stick friction, as well as higher stress crack and chemical resistance. Apart from anticorrosion products, this m..
Melting Point 136 °C
277 °F
DSC
Kaneka PHBH Semi-Rigid Bio-based Polymer
A copolymer produced of 3-hydroxybutyrate and 3-hydroxyhexanoate produced by fermentation of plant oils. It has excellent biodegradability (under anaerobic, aerobic, aquatic, and compost conditions..
Melting Point 136 °C
277 °F
ISO R 1218
Schwartz Technical Plastics LAMIGAMID® 700 Ultra High Molecular Weight Polyethylene
Application: wear liners, sliding platesInformation provided by Schwartz Technical Plastics GmbH
Melting Point 136 - 142 °C
277 - 288 °F
DSC; ISO 3146
Borealis BorPURE™ RB501BF Polypropylene Copolymer
BorPure™ RB501BF is a random copolymer. Applications: BorPure™ RB501BF has been developed especially for applications like: food packaging, over wrap film, label film, and shrink film. Additives..
Melting Point 136 - 140 °C
277 - 284 °F
DSC; ISO 3146
Borealis Borseal™ RE239CF Polypropylene Copolymer
Borseal™ RE239CF is a random copolymer. This grade is suitable for the manufacturing of unoriented films for metallization. Applications: Borseal™ RE239CF is recommended for food packaging, high..
Melting Point 136 °C
277 °F
DSC
Total PPC M6823MZ Metallocene Isostatic Propylene Polymer
TOTAL Petrochemicals Polypropylene M6823MZ is an isostatic form of copolymer polypropylene made via TOTAL Petrochemicals proprietary metallocene catalyst technology.Clarity. M6823MZ incorporates th..
Melting Point 136 °C
277 °F
DSC
Lubrizol Estane® MVT 75AT3 Thermoplastic Polyurethane, Moisture Vapor Transmission
Type: Estane® MVT 75AT3 is a 75A aromatic polyether-based thermoplastic polyurethane (TPU).Features: High moisture vapor transmission with low water swell. Excellent low temperature properties and..
Melting Point <= 136 °C
<= 277 °F
Peak Melting Point; ExxonMobil method
ExxonMobil Escorene™ LD 783.CD Ethylene Vinyl Acetate Copolymer
Product Description: Escorene Ultra LD 783.CD is a 31.4% VA copolymer that is suitable for making a variety of specialty molding and extrusion compounds. It has high clarity and very low modulus. L..
Melting Point 136 °C
277 °F
ASTM D3418, ISO 3146
DuPont™ Appeel® 22D843 Ethylene Acrylate
DuPont™ Appeel® 22D843 is a polypropylene modified ethylene acrylate resin designed to function as a masterbatch to achieve peelability in polypropylene based sealant layers. It provides peelable ..
Melting Point 136 °C
277 °F
ASTM D3418
Braskem Idealis 500 High Molecular Weight Polyethylene Powder
Braskem Idealis 500 is the only High Molecular Weight Polyethylene resin in powder form specially designed for the compression molding process; Applications range from food handling cutting boards a..
Melting Point 136 °C
277 °F
ASTM-D3418
Braskem Idealis 500 Compression Molding High Molecular Weight Polyethylene
Braskem Idealis 500 is the only high molecular weight polyethylene resin in powder form specially designed for the compression molding process. Its applications range from food handling, cutting boa..
Melting Point 136 - 170 °C
277 - 338 °F
Average value: 160 °C Grade Count:13
Overview of materials for Polypropylene with 10% Glass Fiber Filler