DuPont Bynel® 4003 Anhydride-Modified HDPE Adhesive Resin  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , Anhydride-Modified Polyethylene , HDPE
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Bynel® 4003 Anhydride-Modified HDPE Adhesive Resin  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Bynel® Series 4000 resins are anhydride-modified, high-density polyethylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylene (PE) resins.Applications: Bynel® Series 4000 resins are excellent moisture barriers and have a good hydrocarbon resistance. This unique combination of properties makes them useful in a variety of coextrusion applications. HDPE/EVOH tubing and HDPE/polyamide bottles for agricultural chemicals are two examples. Bynel® Series 4000 resins adhere to a variety of materials. They are most often used in coextrusion with EVA, EVOH, polyamide, and PE. Bynel® 4003 is suitable for blown film with polyamide. Bynel® 4006 is appropriate for coextrusion blow molding with either polyamide or EVOH. Bynel® 40E529 can be used for extrusion coating onto paper or bonding to metal surfaces. It provides strong bonds to nylon and good bonds to EVOH in blown film, cast film, and pipe extrusion processes.Physical properties of Bynel® Series 4000 resins are typical of high-density polyethylene resins with similar density and melt index values. The rheology characteristics of each grade are different, so one may be better suited than the others to a particular extrusion process. Information provided by DuPont Packaging Polymers.
Physical Properties Metric English Comments
Density 0.951 g/cc
0.0344 lb/in³
ASTM D792
Moisture Vapor Transmission 5.40 cc-mm/m²-24hr-atm
13.7 cc-mil/100 in²-24hr-atm
ASTM E96
Viscosity 2.00e+6 cP

@Shear Rate 50.0 1/s,
Temperature 190 °C
2.00e+6 cP

@Shear Rate 50.0 1/s,
Temperature 374 °F
estimated from log-log graph
Melt Flow 1.3 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.3 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Thermal Properties Metric English Comments
Melting Point 115 °C
239 °F
Freezing point via DSC/ASTM D3418
136 °C
277 °F
Melting point via DSC/ASTM D3418
Vicat Softening Point 129 °C
264 °F
ASTM D1525
Processing Properties Metric English Comments
Processing Temperature 235 °C
455 °F
Extruder forward zone and adapter for film or coating with EVA or EVOH
Nozzle Temperature 235 °C
455 °F
Die