Polymer Property : Melting Point = 137 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 135 - 137 °C
275 - 279 °F
ISO 3146
Okulen® 1000 PE-UHMW, Black
OKULEN® 1000 is an ultra high molecular low pressure polyethylene with a molecular weight of < 3.5 g/mol. It has great wear resistance, high impact strength, and excellent sliding properties ideal ..
Melting Point 135 - 137 °C
275 - 279 °F
DSC ISO 3146
Okulen® 1000 PE-UHMW, Conductive
OKULEN® 1000 is an ultra high molecular low pressure polyethylene with a molecular weight of < 3.5 g/mol. It has great wear resistance, high impact strength, and excellent sliding properties ideal ..
Melting Point 135 - 137 °C
275 - 279 °F
DSC ISO 3146
Okulen® 1000 PE-UHMW, Green Black
OKULEN® 1000 is an ultra high molecular low pressure polyethylene with a molecular weight of < 3.5 g/mol. It has great wear resistance, high impact strength, and excellent sliding properties ideal ..
Melting Point 135 - 137 °C
275 - 279 °F
DSC ISO 3146
Okulen® 1000 PE-UHMW, MoS2 -Moly-
OKULEN® 1000 is an ultra high molecular low pressure polyethylene with a molecular weight of < 3.5 g/mol. It has great wear resistance, high impact strength, and excellent sliding properties ideal ..
Melting Point 135 - 137 °C
275 - 279 °F
DSC ISO 3146
Okulen® 1000 PE-UHMW, Multi-color
OKULEN® 1000 is an ultra high molecular low pressure polyethylene with a molecular weight of < 3.5 g/mol. It has great wear resistance, high impact strength, and excellent sliding properties ideal ..
Melting Point 135 - 137 °C
275 - 279 °F
ISO 3146
Okulen® 2000 PE-UHMW, 588 Blue
OKULEN® 2000 is an ultra high molecular low pressure polythylene with a molecular weight of > 7.000.000 g/mol plus additives for the improvement of specific material properties. It has an antistati..
Melting Point 135 - 137 °C
275 - 279 °F
ISO 3146
Okulen® 2000 PE-UHMW, 589 Blue
OKULEN® 2000 is an ultra high molecular low pressure polythylene with a molecular weight of > 7.000.000 g/mol plus additives for the improvement of specific material properties. It has an antistati..
Melting Point 135 - 137 °C
275 - 279 °F
ISO 3146
Okulen® 2000 PE-UHMW, AB
OKULEN® 2000 is an ultra high molecular low pressure polythylene with a molecular weight of > 7.000.000 g/mol plus additives for the improvement of specific material properties. It has an antistati..
Melting Point 135 - 137 °C
275 - 279 °F
ISO 3146
Okulen® 2000 PE-UHMW, DG
OKULEN® 2000 is an ultra high molecular low pressure polythylene with a molecular weight of > 7.000.000 g/mol plus additives for the improvement of specific material properties. It has an antistati..
Melting Point 135 - 137 °C
275 - 279 °F
ISO 3146
Okulen® 2000 PE-UHMW, DryRun
OKULEN® 2000 is an ultra high molecular low pressure polythylene with a molecular weight of > 7.000.000 g/mol plus additives for the improvement of specific material properties. It has an antistati..
Melting Point 135 - 137 °C
275 - 279 °F
ISO 3146
Okulen® 2000 PE-UHMW, F-Ex
OKULEN® 2000 is an ultra high molecular low pressure polythylene with a molecular weight of > 7.000.000 g/mol plus additives for the improvement of specific material properties. It has an antistati..
Melting Point 135 - 137 °C
275 - 279 °F
ISO 3146
Okulen® 2000 PE-UHMW, GB
OKULEN® 2000 is an ultra high molecular low pressure polythylene with a molecular weight of > 7.000.000 g/mol plus additives for the improvement of specific material properties. It has an antistati..
Melting Point 135 - 137 °C
275 - 279 °F
ISO 3146
Okulen® 2000 PE-UHMW, GB
OKULEN® 2000 is an ultra high molecular low pressure polythylene with a molecular weight of > 7.000.000 g/mol plus additives for the improvement of specific material properties. It has an antistati..
Melting Point 135 - 137 °C
275 - 279 °F
ISO 3146
Okulen® 2000 PE-UHMW, L
OKULEN® 2000 is an ultra high molecular low pressure polythylene with a molecular weight of > 7.000.000 g/mol plus additives for the improvement of specific material properties. It has an antistati..
Melting Point 135 - 137 °C
275 - 279 °F
ISO 3146
Okulen® 2000 PE-UHMW, Q
OKULEN® 2000 is an ultra high molecular low pressure polythylene with a molecular weight of > 7.000.000 g/mol plus additives for the improvement of specific material properties. It has an antistati..
Melting Point 135 - 137 °C
275 - 279 °F
ISO 3146
Okulen® 2000 PE-UHMW, SG
OKULEN® 2000 is an ultra high molecular low pressure polythylene with a molecular weight of > 7.000.000 g/mol plus additives for the improvement of specific material properties. It has an antistati..
Melting Point 135 - 137 °C
275 - 279 °F
ISO 3146
Okulen® 2000 PE-UHMW, SGB
OKULEN® 2000 is an ultra high molecular low pressure polythylene with a molecular weight of > 7.000.000 g/mol plus additives for the improvement of specific material properties. It has an antistati..
Melting Point 135 - 137 °C
275 - 279 °F
ISO 3146
Okulen® 2000 PE-UHMW, SL
OKULEN® 2000 is an ultra high molecular low pressure polythylene with a molecular weight of > 7.000.000 g/mol plus additives for the improvement of specific material properties. It has an antistati..
Melting Point 135 - 137 °C
275 - 279 °F
ISO 3146
Okulen® 2000 PE-UHMW, T
OKULEN® 2000 is an ultra high molecular low pressure polythylene with a molecular weight of > 7.000.000 g/mol plus additives for the improvement of specific material properties. It has an antistati..
Melting Point 135 - 137 °C
275 - 279 °F
ISO 3146
Okulen® 2000 PE-UHMW, CL
OKULEN® 2000 is an ultra high molecular low pressure polythylene with a molecular weight of > 7.000.000 g/mol plus additives for the improvement of specific material properties. It has an antistati..
Melting Point 135 - 137 °C
275 - 279 °F
ISO 3146
Okulen® 2000 PE-UHMW, OF
OKULEN® 2000 is an ultra high molecular low pressure polythylene with a molecular weight of > 7.000.000 g/mol plus additives for the improvement of specific material properties. It has an antistati..
Melting Point 135 - 137 °C
275 - 279 °F
ISO 3146
Okulen® 2000 PE-UHMW, W
OKULEN® 2000 is an ultra high molecular low pressure polythylene with a molecular weight of > 7.000.000 g/mol plus additives for the improvement of specific material properties. It has an antistati..
Melting Point 95.0 - 137 °C
203 - 279 °F
Indium Corp. Indalloy 80 Bismuth-Lead-Tin Solder Alloy
Information Provided by Indium Corporation
Melting Point 96.0 - 137 °C
205 - 279 °F
Indium Corp. Indalloy 81 Bismuth-Lead-Tin Solder Alloy
Information Provided by Indium Corporation
Melting Point 135 - 137 °C
275 - 279 °F
Addcomp PRIEX® Ionomer 48101 PP random copolymer
Ionomers will be used toStrengthen rigidity and hardness while maintaining impact resistance in polyolefinsMaintain adhesion even under contaminated conditions especially in fatty substratesReduce t..
Melting Point 135 - 137 °C
275 - 279 °F
Addcomp PRIEX® Ionomer 45101 PP random copolymer
Ionomers will be used toStrengthen rigidity and hardness while maintaining impact resistance in polyolefinsMaintain adhesion even under contaminated conditions especially in fatty substratesReduce t..