Okulen® 2000 PE-UHMW, 588 Blue

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), UHMW PE Ultra High Molecular Weight
Manufacturer Okulen
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Okulen® 2000 PE-UHMW, 588 Blue.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
OKULEN® 2000 is an ultra high molecular low pressure polythylene with a molecular weight of > 7.000.000 g/mol plus additives for the improvement of specific material properties. It has an antistatic finish and additional lubricant for the conveyor industry. With added antioxidants, for example, which can be used at high temperatures. With additional flame retardant properties for use in rail vehicle, machinery and mining construction. With enhanced antibacterial effects.
Physical Properties Metric English Comments
Density 0.940 g/cc
0.0340 lb/in³
ISO 1183-A
Mechanical Properties Metric English Comments
Hardness, Shore D 64
64
ISO 868
Tensile Strength, Yield >= 17.0 MPa
>= 2470 psi
ISO/R 527
Elongation at Break >= 50 %
>= 50 %
ISO/R 527
Creep Strength 10.0 MPa
1450 psi
Coefficient of Friction, Dynamic 0.12

@Pressure 2.00 MPa
0.12

@Pressure 290 psi
Metal=Rz 2.5, V = 150 mm/min; ASTM D1894
Coefficient of Friction, Static 0.16

@Pressure 2.00 MPa
0.16

@Pressure 290 psi
PE-metal, V = 10 m/min; ASTM D1894
Abrasion 74
74
Slurry-Test rel to GUR 4120 = 100%; DIN 58836
Thermal Properties Metric English Comments
CTE, linear 200 µm/m-°C
111 µin/in-°F
DIN 53752
Melting Point 135 - 137 °C
275 - 279 °F
ISO 3146
Maximum Service Temperature, Air 80.0 °C
176 °F
Electrical Properties Metric English Comments
Volume Resistivity <= 1.00e+14 ohm-cm
<= 1.00e+14 ohm-cm
Teil 30; IEC 600093 / VDE 0303
Descriptive Properties Value Comments
Color Blue
FDA Approved No