Polymer Property : Melting Point = 143 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 96.0 - 143 °C
205 - 289 °F
Indium Corp. Indalloy 85 Bismuth-Lead-Tin Solder Alloy
Information Provided by Indium Corporation
Melting Point 110 - 143 °C
230 - 289 °F
0.025" extruded film,
Huntsman IROGRAN® A 60 E 4902 TPU-Polyester
Introduction: IROGRAN A 60 E 4902 is a soft, high performance polyester based thermoplastic polyurethane intended for extrusion and molding applications. IROGRAN A 60 E 4902 is part of the HUNTSMAN ..
Melting Point -75.0 - 143 °C
-103 - 289 °F
Average value: 74.6 °C Grade Count:34
Overview of materials for Ethylene Butyl Acrylate
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Butyl Acrylate". Each property range of values reported is minimum and maximum values of approp..