Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 110 °C | 230 °F | Internal method |
Polimeri Europa Clearflex® CH G0 Very Low Density Polyethylene Clearflex CH G0 is a linear low density polyethylene, with antioxidants, characterized by a very low density (VLDPE).The resin has an excellent compatibility with polyolefins and fillers.Main Applic.. |
|||
Melting Point | 110 °C | 230 °F | Crystalline, Peak; ASTM D3418 |
Quadrant EPP Proteus® LDPE - Low Density Polyethylene (ASTM Product Data Sheet) |
|||
Melting Point | 110 - 200 °C | 230 - 392 °F | Average value: 151 °C Grade Count:29 |
Overview of materials for Thermoplastic Polyurethane, Elastomer, Ether Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Ether Grade". Each property range of values reported is minimum a.. |
|||
Melting Point | 110 °C | 230 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil LD 135.09 Cast Packaging Film Resin
(discontinued **) LD 135.09 is a homopolymer film resin with good clarity. It is suitable for processing in cast film equipment. Applications include food packaging, light to medium duty bags, and textile packaging.. |
|||
Melting Point | 110 °C | 230 °F | Exxon Method |
ExxonMobil Escorene® LD-102 LDPE Drawdown Resin, 1.25 mil Film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A homopolymer, good clarity, laundry and dry cleaning film resin capable of providing a tough film in very thin gauges.Applications: Dry cleaning es.. |
|||
Melting Point | 110 °C | 230 °F | Exxon Method |
ExxonMobil Escorene® LD-134 LDPE Packaging Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A homopolymer film resin with good clarity. It is suitable for processing in blown film equipment and can be drawn down to 1.0 mil.Applications: Fo.. |
|||
Melting Point | 110 °C | 230 °F | NOVA |
NOVA Chemicals Novapol® LF-0222-A LDPE Wire and Cable Resin
(discontinued **) NOVA Chemicals NOVAPOL® LF-0222-A is a medium molecular weight low density polyethylene. Resin consistency and purity are very high which make it suitable as a base resin in Wire and Cable applicat.. |
|||
Melting Point | 110 - 220 °C | 230 - 428 °F | Average value: 214 °C Grade Count:19 |
Overview of materials for Nylon 6 Fiber This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6 Fiber". Each property range of values reported is minimum and maximum values of appropriate MatW.. |
|||
Melting Point | 110 °C | 230 °F | ASTM D3418 |
LyondellBasell Microthene® F FN51000 Low Density Polyethylene General DescriptionMicrothene F polyolefin powders are ultra-fine, spherically shaped particles with narrow size distribution suitable for use in a broad range of specialty applications. Microthene.. |
|||
Melting Point | 110 - 164 °C | 230 - 327 °F | Huntsman/TMA |
Huntsman IROGRAN® A 65 P 4324 N TPU-Polyether Excellent resistance to hydrolysis and microbial attack. Suggested for injection molding and extrusion.Information provided by Huntsman |
|||
Melting Point | 110 - 130 °C | 230 - 266 °F | 0.025" extruded film, |
Huntsman IROGRAN® PS455-200 TPU-Polyester Introduction: IROGRAN PS455-200 is a polyester based thermoplastic polyurethane intended for extrusion applications. IROGRAN PS455-200 is part of the HUNTSMAN film and sheet product range and offers.. |
|||
Melting Point | 110 - 150 °C | 230 - 302 °F | ISO 3146-C |
FKuR Kunststoff Bio-Flex® S 6540 Compostable PLA Blend The BIO-FLEX® trade name indicates blends of co-polyester and PLA* with, depending on the particular grade, a very high content of natural resource material. BIO-FLEX® does not contain any sta.. |
|||
Melting Point | 110 - 143 °C | 230 - 289 °F | 0.025" extruded film, |
Huntsman IROGRAN® A 60 E 4902 TPU-Polyester Introduction: IROGRAN A 60 E 4902 is a soft, high performance polyester based thermoplastic polyurethane intended for extrusion and molding applications. IROGRAN A 60 E 4902 is part of the HUNTSMAN .. |
|||
Melting Point | 110 °C | 230 °F | ASTM D2117 |
SCG Chemicals EL-Leneâ„¢ LD1905F Low Density Polyethylene Film Key Characteristics:High productivityGood optical propertiesCan be blended with HDPE, LLDPEContains 1500 ppm slip agent and 2600 ppm antiblocking agentRecommended Applications:General purpose bagVeg.. |
|||
Melting Point | 110 °C | 230 °F | ISO 11357-3 |
Borealis FT3200 Low Density Polyethylene FT3200 is a Low Density Polyethylene for Film Extrusion. Applications heavy-duty bags, shrink film, construction films, and agricultural films. FT3200 contains no additives.Information provided by.. |
|||
Melting Point | 110 - 120 °C | 230 - 248 °F | DSC |
EMS-Griltech Griltex® D 1694A Copolyamide Hotmelt Adhesive (Apparel Interlinings) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Melting Point | 110 - 120 °C | 230 - 248 °F | DSC |
EMS-Griltech Griltex® D 1712A Copolyamide Hotmelt Adhesive (Apparel Interlinings) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Melting Point | 110 °C | 230 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil LD 516.LN Molding, Extrusion and Compounding Resin Product Description: LD 516.LN is a medium MI, low density polyethylene resin designed for use in color concentrates and masterbatches where its flow properties ensure improved processability and un.. |
|||
Melting Point | 110 - 120 °C | 230 - 248 °F | Sheath |
EMS-Griltech Grilon® BA 115 White Nylon 6/CoPA Bi-Component Fiber Description: GRILON BA 115 is the new core / sheath bi-component fiber based on PA 6/CoPA with a sheath melting range from 110 - 120 °C. The fine count bi-component fiber guarantees an even distrib.. |
|||
Melting Point | 110 - 120 °C | 230 - 248 °F | DSC |
BASF Ecoflex® 1200 F Blend Biodegradable Polyester Description: A flexible plastic designed for film extrusion and extrusion coating. Ecoflex® F Blend 1200 comes closer than any other biodegradable plastic to the processing properties of LDPE and L.. |
|||
Melting Point | 110 - 126 °C | 230 - 259 °F | |
3M Dyneon™ Dynamar™ FX 5911 Polymer Processing Additive Dynamar FX 5911 is a free-flowing fluoropolymer processing aid that is designed for use at very low levels (typically 250-1000 ppm) necessary to improve processing, it does not alter or detract from.. |
|||
Melting Point | 110 - 126 °C | 230 - 259 °F | |
3M Dyneon™ FX 5912 Dynamar™ Polymer Processing Additive Dynamar FX 5912 is a free-flowing fluorothermoplastic processing aid that is designed for use at very low levels to improve the processing of thermoplastics. Typical use levels of 200 to 1000 ppm ha.. |
|||
Melting Point | 110 - 120 °C | 230 - 248 °F | DSC |
BASF Ecovio® C2224 F Blend Biodegradable Polyester Description: Ecovio® F Blend C2224 is our biodegradable film product containing renewable resources. It is basically a compound of our biodegradable copolyester Ecoflex® F Blend and polylactic aci.. |
|||
Melting Point | 110 °C | 230 °F | Exxon Method |
ExxonMobil Escorene® LD-332 EVA Packaging Film Resin, High Clarity
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 1% vinyl acetate copolymer packaging film resin. Film made from LD-332 offers improved impact strength and heat sealability compared to homopolym.. |