Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 170 °C | 338 °F | ISO 11357-1 |
Murtfeldt Murytal® C Blue [FS] Acetal Copolymer Thanks to their extremely low absorption of moisture, Murytal® materials are ideally suited for use as electronic isolation components. A fine crystalline structure and high yield strength mean th.. |
|||
Melting Point | 170 °C | 338 °F | ASTM D3418 |
NatureWorks® Ingeo™ AW 300D Injection Grade Biopolymer Specifically designed for use in injection molded food serviceware applications. This opaque, off-white molding grade creates parts that are rigid and heat resistant for tableware used with hot food.. |
|||
Melting Point | 170 °C | 338 °F | 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Hytrel® 3078FG TPC-ET
(Unverified Data**) Hytrel® 3078FG is a high performance thermoplastic elastomer with food compliance specificity.Information provided by DuPont Performance Polymers |
|||
Melting Point | 170 °C | 338 °F | Flow temperature, ASTM D569 |
Rotuba H4 Cellulose Acetate Property values at 50% RH.Data provided by the manufacturer. |
|||
Melting Point | 170 - 180 °C | 338 - 356 °F | MQSA 111 |
Lubrizol Advanced Materials PEARLTHANE® D16N90UV Thermoplastic Polyurethane Elastomer
(discontinued **) PEARLTHANE® D16N90UV is a polyether-based TPU, containing an anti-UV additive, supplied in form of transparent, colorless pellets, offering adequate hardness, excellent mechanical properties and go.. |
|||
Melting Point | 170 °C | 338 °F | |
Hybrid Plastics POSS® MA0734 MethacrylPhenyl-POSS® POSS® Nanostructured Chemical Technology has two unique features: (1) the chemical composition is a hybrid, intermediate (RSiO1.5) between that of silica (SiO2) and silicones (R2SiO). (2) POSS®.. |
|||
Melting Point | 170 °C | 338 °F | DIN 53736; ASTM D789 |
Kolon KOLEFIN® KO133GM40 M/F Reinforced Polypropylene KOLEFIN® has excellent mechanical properties and its cost is lower than other engineering plastics. KOLEFIN® is widely used in the automotive industry and business applications.Good mechanica.. |
|||
Melting Point | 170 °C | 338 °F | DIN 53736; ASTM D789 |
Kolon KOLEFIN® KO133MT20 M/F Reinforced Polypropylene KOLEFIN® has excellent mechanical properties and its cost is lower than other engineering plastics. KOLEFIN® is widely used in the automotive industry and business applications.Good mechanica.. |
|||
Melting Point | 170 - 185 °C | 338 - 365 °F | Huntsman/TMA |
Huntsman IROGRAN® A 92 H 4656 Polyester-Based TPU-Injection Molding Grade Introduction: IROGRAN A 92 H 4656 is a thermoplastic polyester- polyurethane for injection molding applications. Additional characteristics of the product are short cycle times, good melt flow and e.. |
|||
Melting Point | 170 - 174 °C | 338 - 345 °F | DSC |
Solvay Specialty Polymers Solef® 6012 Polyvinylidene Fluoride (PVDF) Solef® 6012 PVDF homopolymer is a high-viscosity PVDF resin and is typically processed by extrusion or compression molding.Features: High Viscosity; HomopolymerAdditional Properties: Crystallizat.. |
|||
Melting Point | 170 - 174 °C | 338 - 345 °F | DSC |
Solvay Specialty Polymers Solef® 60512 Polyvinylidene Fluoride (PVDF) Solef® 60512 PVDF copolymer has high viscosity of the melt and it is a grade for offshore piping.Features: Copolymer; High ViscosityUses: PipingAdditional Properties: Crystallization Heat - ASTM .. |
|||
Melting Point | 170 °C | 338 °F | |
Techmer ES HiFill® PP GB10 10% Glass Beads Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 10% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Melting Point | 170 °C | 338 °F | |
Techmer ES HiFill® PP GB20 20% Glass Beads Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 20% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Melting Point | 170 °C | 338 °F | |
Techmer ES HiFill® PP GB60 60% Glass Beads Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 60% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Melting Point | 170 °C | 338 °F | |
Unitika TERRAMAC TE-8210 Polylactic Acid (PLA) High-durability, Injection grade. Bio-based materials produced from annually renewable raw materials.Information provided by Unitika Ltd. |
|||
Melting Point | 170 °C | 338 °F | DSC |
Toyobo Pelprene™ P-150M Polyester TPE Key Feature: Pelprene P typePelprene™ can be processed into a wide variety of articles from ultra-small precision parts to sheets by injection, extrusion, and blow molding. The 'P' type is a block.. |
|||
Melting Point | 170 °C | 338 °F | Kofler |
Lubrizol ESTANE® 58219 Ether Based Thermoplastic Polyurethane Features: Excellent physical properties, hydrolysis resistance, low temperature performance and clarity. Wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injection .. |
|||
Melting Point | 170 °C | 338 °F | DSC |
Lubrizol Estane® 58246 Thermoplastic Polyurethane Features: High stiffness grade with excellent chemical and oil resistance.Uses: Flat Die/Cast Film Extrusion and Injection Molding.Available in Americas, Europe, Middle East, Africa, India and AsiaI.. |
|||
Melting Point | 170 °C | 338 °F | |
Unitika TERRAMAC TE-7000 Polylactic Acid (PLA) Heat-resisting grade, Injection grade. Bio-based materials produced from annually renewable raw materials.Information provided by Unitika Ltd. |
|||
Melting Point | 170 °C | 338 °F | |
Unitika TERRAMAC TE-7307 Polylactic Acid (PLA) Heat-resisting grade, Injection grade. Bio-based materials produced from annually renewable raw materials.Information provided by Unitika Ltd. |
|||
Melting Point | 170 °C | 338 °F | |
Unitika TERRAMAC TP-4030 Polylactic Acid (PLA) Soft, Extrusion, blow, and foam sheet grade. Bio-based materials produced from annually renewable raw materials.Information provided by Unitika Ltd. |
|||
Melting Point | 170 °C | 338 °F | 10°C/min; ISO 11357-1/-3 |
EMS-Grivory Grivory® XE 3982 PA12 Product description: Grilamid XE 3982 is a highly flexible extrusion grade, based on Polyamide 12 with following main attributes: High flexibilityLow plasticizer migration (low blooming)Very good ch.. |
|||
Melting Point | 170 °C | 338 °F | ISO 3146 |
Eurostar Star L POM D51 POM, Injection Molded Star L POM D51 is a PTFE Lubricated, POM Copolymer Injection Molding ResinInformation provided by Eurostar. |
|||
Melting Point | 170 °C | 338 °F | DIN 53765 |
BASF Ultraform® N2200 G43 POM Description: Is a POM, injection-molding grade for parts requiring high stiffness and strength together with good mold release.Information provided by BASF |
|||
Melting Point | 170 °C | 338 °F | 10°C/min.; ISO 3146 |
Azoty Tarnow™ TARNOFORM 300 CI2 POM Impact modified injection molding grade based on Tarnoform 300 reinforced with 10% MBS rubber yielding good cold impact strength and good strength of weld lines combined with good weatherability.Inf.. |
|||
Melting Point | 170 - 174 °C | 338 - 345 °F | ASTM D3418 |
Solvay Specialty Polymers Solef® 60512 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 60512 PVDF copolymer has high viscosity of the melt and it is a grade for offshore piping.Information provided by Solvay Specialty Polymers. |
|||
Melting Point | 170 - 175 °C | 338 - 347 °F | ASTM D789 |
Lucent Polymers POM-500 Acetal Homopolymer, General Purpose, Injection Grade Add "U" for UV StabilizedInformation provided by Lucent Polymers, Inc. |