Polymer Property : Melting Point = 195 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 185 - 195 °C
365 - 383 °F
High melting point
Oceanchem Group 1,2,5,6,9,10-Hexabromocyclododecane (HBCD)
Molecular Formula: C12H18Br6Cas No.: 3194-55-6Characteristics: The product is white crystalline powder, melting point greater than 180°C, bromine content greater than or equal to 73%. This product..
Melting Point 156 - 195 °C
313 - 383 °F
Average value: 176 °C Grade Count:31
Overview of materials for Ethylene Vinyl Alcohol (EVOH)
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Alcohol". Each property range of values reported is minimum and maximum values of appropr..
Melting Point 180 - 195 °C
356 - 383 °F
Huntsman/TMA
Huntsman IROGRAN® A 92 K 5031 TPU-High Temperature Performance
Polycaprolactone and ether based. Good processability and compression set. Excellent resistance to high temperatures, water, grease, and oils.. Used in seals, wheels, and rollers.Information prov..
Melting Point 165 - 195 °C
329 - 383 °F
Indium Corp. Indalloy 235 Indium Solder Alloy
Information Provided by Indium Corporation
Melting Point 160 - 195 °C
320 - 383 °F
Zeus EFEP Tubing
Melting Point 185 - 195 °C
365 - 383 °F
DSC
EMS-Griltech Griltex® D 1655E Copolyester Hotmelt Adhesive (Technical Applications)
Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo..
Melting Point 175 - 195 °C
347 - 383 °F
DSC Induction Temperature; TM-029
AorTech Biomaterials Elast-Eon™ E2-860 Biomedical Polyurethane Pellets
Elast-Eon™ 2-860 is a polyurethane with a 60% hard segment content and a mixed polyether/siloxane soft segment. It comes in pellet form. The pellets are colorless to yellowish and are soluble in DM..
Melting Point 175 - 195 °C
347 - 383 °F
DSC Induction Temperature; TM-029
AorTech Biomaterials Elast-Eon™ E2-860 Biomedical Polyurethane Pellets
Elast-Eon™ 2-860 is a polyurethane with a 60% hard segment content and a mixed polyether/siloxane soft segment. It comes in pellet form. The pellets are colorless to yellowish and are soluble in DM..
Melting Point 185 - 195 °C
365 - 383 °F
Temperature range at which MFI = 10 g/10 min at 21.6 kg.; MQSA 111
Lubrizol Advanced Materials Pearlthane® ECO D20N88 Thermoplastic Polyurethane  (discontinued **)
PEARLTHANE® ECO D20N88 is a 86 Shore A, High Performance natural TPU based on Renewable Sources with ca. 60% renewable content according to ASTM D6866 for Extrusion and Injection Molding applicatio..