Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 106 - 116 °C | 223 - 241 °F | |
Oceanchem Group Bis (2,3-dibromopropyl ether) of TBBA (BDDP) Molecular Formula: C21H20Br8O2Cas No.: 21850-44-2Application: BDDP used for plastics as flame-retardant, is designed for use in PP (homopolymer and copolymer) and high impact polystyrene (HIPS) appl.. |
|||
Melting Point | 106 °C | 223 °F | Internal method |
Polimeri Europa Riblene® MT 10 Low Density Polyethylene - Injection Molding Riblene MT 10 is a low density polyethylene resin (LDPE) having an excellent fluidity.Parts made with Riblene MT 10 are highly flexible.Main Applications: Riblene MT 10 is suitable for injection mo.. |
|||
Melting Point | 106 °C | 223 °F | Internal method |
Polimeri Europa Riblene® MT 10 R Low Density Polyethylene - Injection Molding Riblene MT 10 R is a low density polyethylene resin (LDPE) having an excellent fluidity.Parts made with Riblene MT 10 R are highly flexible.Main Applications: Riblene MT 10 R is suitable for inject.. |
|||
Melting Point | 106 °C | 223 °F | Exxon Method |
ExxonMobil Escorene® LD-144 EVA Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 2% vinyl acetate copolymer packaging film resin. Film made from LD-144 offers improved impact strength and heat sealability compared to homopolym.. |
|||
Melting Point | 106 °C | 223 °F | Exxon Method |
ExxonMobil Escorene® LD-314 EVA Packaging Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 3.5% vinyl acetate copolymer resin for higher clarity films. Film made from LD-314 offers good impact strength, heat sealability, and low tempera.. |
|||
Melting Point | 106 °C | 223 °F | Exxon Method |
ExxonMobil Escorene® LD-325 EVA Film Resin, High Clarity, High Impact
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 3.8% vinyl acetate copolymer, high clarity film resin. The combination of low melt index and comonomer content helps produce films which exhibit .. |
|||
Melting Point | 106 °C | 223 °F | DSC |
LyondellBasell DP 8510M Polybutene Key Features: semi-crystalline high ethylene content random copolymer, miscible with polyproylenesApplications: Hot Melt Adhesives, FDA acceptableMeets FDA requirements in 21 CFR 175.105 for indirec.. |
|||
Melting Point | 106 °C | 223 °F | Melting point via DSC/ASTM D3418 |
DuPont Bynel® 4206 Anhydride-Modified LDPE Adhesive Resin Bynel® Series 4200 resins are anhydride-modified, low-density polyethylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process .. |
|||
Melting Point | 106 °C | 223 °F | Melting point via DSC/ASTM D3418 |
DuPont Bynel® 4288 Anhydride-Modified LDPE Adhesive Resin Bynel® Series 4200 resins are anhydride-modified, low-density polyethylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process .. |
|||
Melting Point | 106 °C | 223 °F | ISO 11357 |
Total LDPE 1200 MN 18 C Low Density Polyethylene - Injection Molding and Compounding LDPE 1200 MN 18 C is a low density polyethylene made by a high pressure autoclave process without antioxidant.Application examples: flexible molding, handles, closures, household items, toys, variou.. |
|||
Melting Point | 106 °C | 223 °F | DSC; ASTM D3418 |
Westlake Tymax™ GT1057 Anhydride Modified Acrylate Copolymer Product Description: Westlake GT1057 is an anhydride modified low density polyethylene designed as an extrusion coating and laminating tie-layer. Westlake GT1057 provides excellent adhesion to pol.. |
|||
Melting Point | 106 °C | 223 °F | ASTM D1525 |
Lubrizol ESTANE® 58091 Ester Based Thermoplastic Polyurethane Features: High stiffness TPU alloyUses: Flat Die/Cast Sheet Extrusion, Profile Extrusion and Injection MoldingAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformation provided b.. |
|||
Melting Point | 106 °C | 223 °F | Freezing Point; ASTM D3418 |
DuPont™ Bynel® 41E865 Anhydride Modified LLDPE BYNEL® Series 4100 series resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All BYNEL Series 4100 series resins are available in pellet form for use in conventional ext.. |
|||
Melting Point | 106 °C | 223 °F | Freezing Point; ASTM D3418 |
DuPont™ Bynel® 41E871 Anhydride Modified LLDPE BYNEL® Series 4100 series resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All BYNEL Series 4100 series resins are available in pellet form for use in conventional ext.. |
|||
Melting Point | 106 °C | 223 °F | Freezing Point; ASTM D3418 |
DuPont™ Fusabond® E589 Polymer Modifier DuPont™ Fusabond® E589 is an anhydride modified polyethylene. Uses: Adhesives Pipe Coating Tie-Layer Features premium adhesive for Pipe Coating tie-layer at high surface temperatures. ( 90°C) |
|||
Melting Point | 106 °C | 223 °F | Dow Method (DSC) |
Dow 4010 Low Density Polyethylene (LDPE) Polyethylene 4010 is used in flexible packaging and paperboard coating applications such as liquid/juice, laminate tube, condiment pouches, dry and moist foods packaging, sugar pouches, lidding stoc.. |
|||
Melting Point | 106 °C | 223 °F | DSC |
Arkema Group OREVAC® 18921A Epoxide Modified Polyethylene OREVAC® 18921A is epoxide modified polyethylene. It is available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylene (PE) resins. OREVAC® 18.. |
|||
Melting Point | 106 °C | 223 °F | ISO 11357-3 |
Addcomp PRIEX® 15005 Maleic Anhydride modified LDPE Functionalised low density polyethylene to be used as compatibiliser for polymer blends or coupling agent for wood flour, natural fibres, or mineral filled polyolefins. Also suitable to reduce pigme.. |
|||
Melting Point | 106 °C | 223 °F | |
BASF N,N’-Dimethylurea Formula: C3H8N2OCAS: 96-31-1Description Dimethylurea is a colorless to white powder, with an amine-like odor.Synonyms: 1,3-DimethylureaApplications: Intermediate used in the production of Pharmaceut.. |
|||
Melting Point | 106 °C | 223 °F | DSC |
Arkema Group LOTADER® AX 8840 Copolymer Ethylene - Glycidyl Methacrylate LOTADER AX 8840 is a random copolymer of Ethylene and Glycidyl Methacrylate, polymerized under high pressure in an autoclave process. Due to the reactivity induced by the Glycidyl methacrylate, LOTA.. |
|||
Melting Point | 106 °C | 223 °F | ASTM D3417 |
DuPont Elvax® PE3507-2 Ethylene Vinyl Acetate
(discontinued **) DuPont™ Elvax® PE3507-2 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins. Applic.. |