Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 315 °C | 599 °F | DSC |
Rogers Corporation Ultralam® 3850 Liquid Crystalline Polymer Circuit Material ULTRALAM® 3850 laminate circuit materials utilize highly temperature resistant liquid crystalline polymer (LCP) as the dielectric film.Features & Benefits:Excellent high frequency propertiesStable .. |
|||
Melting Point | 315 °C | 599 °F | Peak; ASTM D3418 |
Solvay Specialty Polymers Amodel® AT-1002 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AT-1002 HS is a neat, toughened, heat stabilized polyphthalamide (PPA) resin that offers superior retention of properties after humid thermal aging; high impact at low temperature and better .. |
|||
Melting Point | 315 °C | 599 °F | ISO 11357-3 |
Solvay Specialty Polymers Amodel® AT-1002 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AT-1002 HS is a neat, toughened, heat stabilized polyphthalamide (PPA) resin that offers superior retention of properties after humid thermal aging; high impact at low temperature and better .. |
|||
Melting Point | 315 °C | 599 °F | |
Indium Corp. Indalloy 167 Lead Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 315 °C | 599 °F | Peak; Dry; ASTM D3418 |
Solvay Specialty Polymers Amodel® AT-1002 HS Polyphthalamide (PPA) Amodel® AT-1002 HS is a neat, toughened, heat stabilized polyphthalamide (PPA) resin that offers superior retention of properties after humid thermal aging; high impact at low temperature and bet.. |
|||
Melting Point | 315 °C | 599 °F | Dry; ISO 11357-3 |
Solvay Specialty Polymers Amodel® AT-1002 HS Polyphthalamide (PPA) Amodel® AT-1002 HS is a neat, toughened, heat stabilized polyphthalamide (PPA) resin that offers superior retention of properties after humid thermal aging; high impact at low temperature and bet.. |
|||
Melting Point | 315 °C | 599 °F | ASTM D3418 |
Solvay Specialty Polymers Amodel® AT-1002 HS Polyphthalamide (PPA) Amodel® AT-1002 HS is a neat, toughened, heat stabilized polyphthalamide (PPA) resin that offers superior retention of properties after humid thermal aging; high impact at low temperature and bet.. |
|||
Melting Point | 315 °C | 599 °F | ISO 11357-3 |
Solvay Specialty Polymers Amodel® AT-1002 HS Polyphthalamide (PPA) Amodel® AT-1002 HS is a neat, toughened, heat stabilized polyphthalamide (PPA) resin that offers superior retention of properties after humid thermal aging; high impact at low temperature and bet.. |
|||
Melting Point | 315 °C | 599 °F | DSC |
Wolf Kunststoff ZEDEX® ZX-410V7T A4T Polymer Alloy, Fiber Reinforced, Friction Modified Main Characteristics: Fiber-reinforced; Friction-modified; Very high stiffness (higher than that of fiber-reinforced PEEK); Very low thermal expansion coefficient; Low friction; High wear resistance.. |
|||
Melting Point | 315 °C | 599 °F | 10°C/min; ISO 11357-1/-3 |
EMS-Grivory Grivory® XE 4120 black 9916 PA*-GF30 Product description: Grivory XE 4120 black 9916 is a 30% glass fiber reinforced flame retardant (UL 94 V-0) engineering thermoplastic material based on a semi-crystalline, partially aromatic copolya.. |
|||
Melting Point | 315 °C | 599 °F | 10°C/min; ISO 11357-1/-3 |
EMS-Grivory Grivory® XE 4185 black 9453 PA* Product description: Grivory XE 4185 is a non-reinforced heat stabilized engineering thermoplastic material based on a semicrystalline, partially aromatic copolyamide. ISO polymer designation: PA 10.. |
|||
Melting Point | 315 °C | 599 °F | [10 K/min], ISO 11357 |
Eurotec® Tecomid® NT40 CR30 BK111 HS PPA, 30% carbon fiber reinforced, heat stabilized, natural Information provided by Eurotec® |
|||
Melting Point | 315 °C | 599 °F | [10 K/min], ISO 11357 |
Eurotec® Tecomid® NT40 GR15 NL HS PPA, 15% glass fiber reinforced, heat stabilized, natural Information provided by Eurotec® |
|||
Melting Point | 315 °C | 599 °F | [10 K/min], ISO 11357 |
Eurotec® Tecomid® NT40 GR30 NL HS PPA, 30% glass fiber reinforced, heat stabilized, natural Information provided by Eurotec® |
|||
Melting Point | 315 °C | 599 °F | [10 K/min], ISO 11357 |
Eurotec® Tecomid® NT40 GR30 NL XA60 PPA, 30% glass fiber reinforced, flame retardant - halogen & red phosphorus free, heat stabilized, natural Information provided by Eurotec® |
|||
Melting Point | 315 °C | 599 °F | [10 K/min], ISO 11357 |
Eurotec® Tecomid® NT40 GR30 NL XA60 PPA, 30% glass fiber reinforced, flame retardant - halogen & red phosphorus free, heat stabilized, natural Information provided by Eurotec® |
|||
Melting Point | 315 °C | 599 °F | [10 K/min], ISO 11357 |
Eurotec® Tecomid® NT40 GR50 NL HS PPA, 50% glass fiber reinforced, heat stabilized, natural Information provided by Eurotec® |
|||
Melting Point | 315 °C | 599 °F | [10 K/min], ISO 11357 |
Eurotec® Tecomid® NT40 GR60 NL HS PPA, 60% glass fiber reinforced, heat stabilized, natural Information provided by Eurotec® |
|||
Melting Point | 315 °C | 599 °F | [10 K/min], ISO 11357 |
Eurotec® Tecomid® NT40 MR40 NL HS PPA, 40% mineral reinforced, heat stabilized, natural Information provided by Eurotec® |
|||
Melting Point | 315 °C | 599 °F | [10 K/min], ISO 11357 |
Eurotec® Tecomid® NT40 NL MB PPA, impact modified, heat stabilized, natural Information provided by Eurotec® |
|||
Melting Point | 315 °C | 599 °F | [10 K/min], ISO 11357 |
Eurotec® Tecomid® NT40 NL PPA, unfilled, natural Information provided by Eurotec® |
|||
Melting Point | 315 °C | 599 °F | [10 K/min], ISO 11357 |
Eurotec® Tecomid® NT40 NL XA60 PPA, unfilled, flame retardant - halogen & red phosphorus free, heat stabilized, natural Information provided by Eurotec® |