Thermal Properties Metric English Comments
Melting Point 155 - 161 °C
311 - 322 °F
Oceanchem Group Antioxidant 1098
Molecular Formula: C40H64O4N4Cas No.: 23128-74-7Use: This product is a non-color-degrading, nonpolluting, heat-resisting, extraction-resisting, high-performance all-purpose antioxidant, mainly appli..
Melting Point 146 - 161 °C
295 - 322 °F
TMA Melt Range, 25 mil film
Huntsman IROGRAN® A 85 P 5004 TPU-Polyether
IROGRAN® A 85 P 5004 is a polyether based thermoplastic polyurethane intended for injection molding and extrusion applications.Information provided by Alliance Polymers
Melting Point 156 - 161 °C
313 - 322 °F
Shandong Dongyue Shenzhou New Material Co DS201 Polyvinylidene Fluoride Powder
Conformable with: Q/DYS 014-2007Polyvinylidene fluoride (PVDF) powder (DS201) PVDF is the homopolymer of vinylidene fluoride, which is excellent chemical corrosion-resistant, high temperature resist..