Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 1.40 J/g-°C | 0.335 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® DMX1435 PC Copolymer (Europe-Africa-Middle East) This product will be phased out per January 2015 -- Lexan* DMX1435 is a UV stabilized standard flow polycarbonate copolymer resin with improved scratch resistance. |
|||
Specific Heat Capacity | 1.40 J/g-°C | 0.335 BTU/lb-°F | ASTM C 351 |
SABIC Innovative Plastics Lexan® DMX2415 PC Lexan* DMX2415 is a polycarbonate resin with improved scratch resistance. Lexan* DMX2415 is available in transparent, translucent, and opaque colors.This data was supplied by SABIC-IP for the Americ.. |
|||
Specific Heat Capacity | 1.40 J/g-°C | 0.335 BTU/lb-°F | ASTM C 351 |
SABIC Innovative Plastics Lexan® DMX2415 PC (Asia Pacific) Lexan* DMX2415 is a polycarbonate resin with improved scratch resistance. Lexan* DMX2415 is available in transparent, translucent, and opaque colors.This data was supplied by SABIC-IP for the Asia P.. |
|||
Specific Heat Capacity | 1.40 J/g-°C | 0.335 BTU/lb-°F | ASTM C 351 |
SABIC Innovative Plastics Lexan® DMX2415 PC (Europe-Africa-Middle East) Lexan* DMX2415 is a polycarbonate resin with improved scratch resistance. Lexan* DMX2415 is available in transparent, translucent, and opaque colors.This data was supplied by SABIC-IP for the Europe.. |
|||
Specific Heat Capacity | 1.40 J/g-°C | 0.335 BTU/lb-°F | ASTM C 351 |
SABIC Innovative Plastics Lexan® DMX9455 PC Copolymer (Europe-Africa-Middle East) Lexan* DMX9455 is a standard flow, flame retardant, V0/1.5mm, opaque polycarbonate copolymer resin with improved scratch resistance.This data was supplied by SABIC-IP for the Europe-Africa-Middle Ea.. |
|||
Specific Heat Capacity | 1.40 J/g-°C | 0.335 BTU/lb-°F | ASTM C 351 |
SABIC Innovative Plastics Lexan® DMX9455A PC Copolymer Lexan* DMX9455A is a standard flow, flame retardant, transparent polycarbonate copolymer resin with improved scratch resistance.This data was supplied by SABIC-IP for the Americas region. |
|||
Specific Heat Capacity | 1.40 J/g-°C | 0.335 BTU/lb-°F | ASTM C 351 |
SABIC Innovative Plastics Lexan® HPB3144G PC Copolymer Standard flow, transparent, high purity polycarbonate copolymer resin with reduced oxygen permeability and water vapor transmission rate. For medical devices and pharmaceutical applications. Health.. |
|||
Specific Heat Capacity | 1.40 J/g-°C @Temperature 80.0 °C |
0.335 BTU/lb-°F @Temperature 176 °F |
ASTM E1269 |
Eastman Aqua 20837 PET
(discontinued **) Voridian Aqua thermoplastic polyesters are condensation polymers produced by a continuous melt-phase polymerization process followed by a solid-state polymerization process. Voridian Aqua polymer 20.. |
|||
Specific Heat Capacity | 1.40 J/g-°C @Temperature 100 °C |
0.335 BTU/lb-°F @Temperature 212 °F |
ASTM E1269 |
Eastman 15041 PET
(discontinued **) Voridian polymer 15041 is a PET thermoplastic polyester.Applications/UsesCrystallized PET (CPET) trays |
|||
Specific Heat Capacity | 1.40 J/g-°C @Temperature 100 °C |
0.335 BTU/lb-°F @Temperature 212 °F |
ASTM E1269 |
Eastman 7352 PET
(discontinued **) VORIDIAN PET thermoplastic polyesters are condensation polymers produced by a continuous melt-phase polymerization process followed by a solid-state polymerization process. VORIDIAN PET polyester 73.. |
|||
Specific Heat Capacity | 1.40 J/g-°C @Temperature 100 °C |
0.335 BTU/lb-°F @Temperature 212 °F |
ASTM E1269 |
Eastman 9921 PET Film
(discontinued **) VORIDIAN polymer 9921 is a copolymer PET that has been crystallized. Color concentrates of polymer 9921 are available on request.Applications/UsesAutomotive parts containersFood packagingHousehold p.. |
|||
Specific Heat Capacity | 1.40 J/g-°C @Temperature 100 °C |
0.335 BTU/lb-°F @Temperature 212 °F |
ASTM E1269 |
Eastman 9921 PET Injection Molded
(discontinued **) VORIDIAN polymer 9921 is a copolymer PET that has been crystallized. Color concentrates of polymer 9921 are available on request.Applications/UsesAutomotive parts containersFood packagingHousehold p.. |
|||
Specific Heat Capacity | 1.40 J/g-°C | 0.335 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics NORYL GTX GTX678 PPE+PA Noryl GTX678 resin is a high performance blend of PPE/PA that exhibits an excellent balance on non-halogenated flame retardance, conductivity, ductility, and high-heat resistance. This grade can be.. |
|||
Specific Heat Capacity | 1.40 J/g-°C | 0.335 BTU/lb-°F | |
Goodfellow Polyhydroxybutyrate / Polyhydroxyvalerate (PHB 92/PHV 8) See also PHB. PHB/PHV copolymers are used in preference to PHB homopolymer for general purposes (e.g. molding containers) in order to obtain a better balance of stiffness and toughness. PHV contents.. |
|||
Specific Heat Capacity | 1.40 J/g-°C @Temperature 80.0 °C |
0.335 BTU/lb-°F @Temperature 176 °F |
DSC |
Eastman Eastar A150 Copolyester, Film Eastar A150 Copolyester is a poly(1,4-cyclohexylene-dimethylene terephthalate/isophthalate). It is produced by reacting terephthalic acid and isophthalic acid with the glycol 1,4-cyclohexanedimethan.. |
|||
Specific Heat Capacity | 1.40 J/g-°C | 0.335 BTU/lb-°F | |
BASF Ultramid® B3G8 BK00564 40% Glass Filled PA6 (Conditioned) Ultramid B3G8 BK00564 is a 40% glass filled, pigmented black, injection molding PA6 grade. |
|||
Specific Heat Capacity | 1.40 J/g-°C | 0.335 BTU/lb-°F | |
BASF Ultramid® B3G8 BK00564 40% Glass Filled PA6 (Dry) Ultramid B3G8 BK00564 is a 40% glass filled, pigmented black, injection molding PA6 grade. |
|||
Specific Heat Capacity | 1.40 J/g-°C | 0.335 BTU/lb-°F | |
BASF Ultramid® B3WG7 BK 00564 35% Glass Filled PA6 (Conditioned) Description: 35% glass-fiber reinforced and heat aging resistant injection-molding grade, e.g. for automotive manifolds and pedals.Information provided by BASF |
|||
Specific Heat Capacity | 1.40 J/g-°C | 0.335 BTU/lb-°F | |
BASF Ultramid® A3X2G7 35% Glass Filled PA66 (Dry) Ultramid A3X2G7 is a 35% glass fiber reinforced injection molding PA66 grade with improved flame retardance and enhanced long-term stability. Flame retardant based on red phosphorus; very high stif.. |
|||
Specific Heat Capacity | 1.40 J/g-°C | 0.335 BTU/lb-°F | |
BASF Ultramid® B3WG7 BK 00564 30% Glass Filled PA6 (Dry) Description: 35% glass-fiber reinforced and heat aging resistant injection-molding grade, e.g. for automotive manifolds and pedals.Information provided by BASF |
|||
Specific Heat Capacity | 1.40 J/g-°C | 0.335 BTU/lb-°F | |
Goodfellow Cellophane, Rayophane Regenerated Cellulose Fiber All forms of cellulose degrade before they melt but natural cellulose can be regenerated by the xanthate process to manufacture fibres, commonly called rayon or viscose, and film, commonly called by.. |
|||
Specific Heat Capacity | 1.40 J/g-°C | 0.335 BTU/lb-°F | |
Goodfellow Cellophane, Rayophane Regenerated Cellulose Film All forms of cellulose degrade before they melt but natural cellulose can be regenerated by the xanthate process to manufacture fibres, commonly called rayon or viscose, and film, commonly called by.. |
|||
Specific Heat Capacity | 1.40 J/g-°C | 0.335 BTU/lb-°F | |
BASF Ultramid® B3M6 BK60564 30% Mineral Filled PA6 (Conditioned) Ultramid B3M6 BK60564 is a 30% mineral reinforced, pigmented black injection molding PA6 grade for industrial items requiring high impact strength and very high dimensional stability, excellent lase.. |
|||
Specific Heat Capacity | 1.40 J/g-°C | 0.335 BTU/lb-°F | |
BASF Ultramid® B3M6 BK60564 30% Mineral Filled PA6 (Dry) ultramid B3M6 BK60564 is a 30% mineral reinforced, pigmented black injection molding PA6 grade for industrial items requiring high impact strength and very high dimensional stability, excellent lase.. |
|||
Specific Heat Capacity | 1.40 J/g-°C @Temperature 100 °C |
0.335 BTU/lb-°F @Temperature 212 °F |
ASTM E1269 |
Eastman VersaTray 12822 Plastic
(discontinued **) VersaTray plastic 12822 is a polyethylene terephthalate resin designed for use as a base resin for crystallized PET (CPET) food trays and other high temperature food packaging applications. CPET foo.. |
|||
Specific Heat Capacity | 1.40 J/g-°C @Temperature 100 °C |
0.335 BTU/lb-°F @Temperature 212 °F |
ASTM E1269 |
Eastman 5214A PET
(discontinued **) Voridian PET 5214A is a bright and transparent amber homopolymer that meets light barrier requirements while maintaining the desirable attributes of PET. This resin is commonly used to mold containe.. |
|||
Specific Heat Capacity | 1.40 J/g-°C @Temperature 100 °C |
0.335 BTU/lb-°F @Temperature 212 °F |
ASTM E1269 |
Eastman 9921W PET Film
(discontinued **) Voridian PET 9921W is a copolymer PET. Typical applications include containers for automotive parts, household products, and pharmaceutical and food packaging. Voridian PET thermoplastic polyesters .. |
|||
Specific Heat Capacity | 1.40 J/g-°C @Temperature 100 °C |
0.335 BTU/lb-°F @Temperature 212 °F |
ASTM E1269 |
Eastman 9921W PET Injection Molded
(discontinued **) Voridian PET 9921W is a copolymer PET. Typical applications include containers for automotive parts, household products, and pharmaceutical and food packaging. Voridian PET thermoplastic polyesters .. |
|||
Specific Heat Capacity | 1.40 J/g-°C | 0.335 BTU/lb-°F | IEC 1006 |
BASF Ultradur® B 4300 G10 50% Glass Filled PBT Description: Injection-molding grades containing 50% of glass fibers, for industrial parts, rigid, tough and dimensionally stable, for example for program switches, thermostat parts, small-motor hou.. |
|||
Specific Heat Capacity | 1.40 J/g-°C | 0.335 BTU/lb-°F | |
BASF Ultramid® B3UGM210 GR 22866 10/50% Glass/Mineral Filled PA6 FR (Dry) Description: Halogen- and phosphorus-free injection-molding grade with very high rigidity, low smoke density and outstanding electrical properties.Information provided by BASF |