Thermal Properties Metric English Comments
Glass Transition Temp, Tg 108 °C
226 °F
DAM (SSYS)
Proto3000 ABS-M30 Fused Deposition Modeling Polymer
Description: ABS-M30 is up to 25-70 percent stronger than standard Stratasys ABS and is an ideal material for conceptual modeling, functional prototyping, manufacturing tools, and end-use-parts. ABS..
Glass Transition Temp, Tg 108 °C
226 °F
DAM (SSYS)
Proto3000 ABS-M30i Fused Deposition Modeling Polymer
Description: ABS-M30i is a high strength material well suited for the medical, pharmaceutical and food packaging industries. Parts manufactured with ABS-M30i material are biocompatible (ISO 10993 ce..
Glass Transition Temp, Tg 108 - 127 °C
226 - 261 °F
Average value: 116 °C Grade Count:9
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded". Each property range of values reported i..
Glass Transition Temp, Tg 108 - 109 °C
226 - 228 °F
Average value: 108 °C Grade Count:3
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Extruded". Each property range of values reported is minimum and ..
Glass Transition Temp, Tg 108 °C
226 °F
10°C/min test
Polimeri Europa SINKRAL B633/E ABS, Impact & Heat Stabilized Grade  (discontinued **)
Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,EG,105-04-25-20 High impact extrusion grade with excellent stiffness, good processability and high thermal stabili..
Glass Transition Temp, Tg 108 °C
226 °F
10°C/min test
Polimeri Europa SINKRAL B733/E ABS, Impact & Heat Stabilized Grade  (discontinued **)
Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,EG,095-04-35-15 Very high impact resistant grade for sheet extrusion with good processability and high thermal sta..
Glass Transition Temp, Tg 108 °C
226 °F
10°C/min test
Polimeri Europa SINKRAL PD G523 ABS, Impact Grade  (discontinued **)
Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,095-15-25-20 High impact injection moulding grade. Other characteristics: good flow, excellent thermal stabilit..
Glass Transition Temp, Tg 108 °C
226 °F
Eastman Tenite 132E-28 Cellulose Acetate  (discontinued **)
28% Plasticized with 25% fiber grade ester.ISO data as provided by the manufacturer, Eastman Chemical.
Glass Transition Temp, Tg 108 - 150 °C
226 - 302 °F
Average value: 136 °C Grade Count:5
Overview of materials for Nylon, Amorphous Transparent Alloy
This property data is a summary of similar materials in the MatWeb database for the category "Nylon, Amorphous Transparent Alloy". Each property range of values reported is minimum and maximum value..
Glass Transition Temp, Tg 108 °C
226 °F
ASTM D3418
Kolon DIAMAT® IM
Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl..
Glass Transition Temp, Tg 108 °C
226 °F
SABIC Innovative Plastics XYLEX EXXX0292 PC+POLYESTER (Europe-Africa-Middle East)
XYLEX* EXXX0292 is a transparent copolyester/polycarbonate blend with high flow, V2 UL94 rating at 1.5mm and Tg of 108 C
Glass Transition Temp, Tg 108 °C
226 °F
DSC (SSYS)
Stratasys® ABS-M30
ABS-M30 is 25-70 percent stronger than standard Stratasys ABS and is an ideal material for conceptual prototyping, design verification, and direct digital manufacturing. ABS-M30 has greater tensile,..
Glass Transition Temp, Tg 108 °C
226 °F
DSC
Stratasys® ABS-M30i
ABS-M30i is a high strength material well suited for the medical, pharmaceutical and food packaging industries. Parts manufactured with ABS-M30i material are biocompatible (ISO 10993 certified) an..
Glass Transition Temp, Tg 108 °C
226 °F
10°C/min test
Polimeri Europa SINKRAL F233 ABS, Heat Stabilized  (discontinued **)
Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,105-15-16-25 Medium heat injection moulding grade having high flow and good thermal stability during processing..
Glass Transition Temp, Tg 108 °C
226 °F
10°C/min test
Polimeri Europa SINKRAL PD G120 ABS  (discontinued **)
Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,095-15-09-30 General purpose injection moulding grade. Characteristics: outstanding rigidity very high surface..
Glass Transition Temp, Tg 108 °C
226 °F
10°C/min test
Polimeri Europa SINKRAL G323 ABS  (discontinued **)