Polymer Property : Glass Transition Temp, Tg = 123 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 123 °C
253 °F
TM R050-25
Resinlab® EP950NMF Gray Non-Metallic Filled Rubber Modified Epoxy
Resinlab™ EP950NMF Gray is a non-metallic filled version of EP950G. It is a one-part rubber modified epoxy designed for bonding metal and other structural material subject to stress at elevated tem..
Glass Transition Temp, Tg 123 °C
253 °F
TMA
Lord Adhesives Thermosetâ„¢ ME-455-1 Epoxy Board Level Encapsulant
LORD Thermosetâ„¢ ME-455-1 encapsulant is a low viscosity, one-component, semiconductor grade epoxy designed for the encapsulation of wire-bonded or flip chip die in PPGA, BGA, MCM and other cavi..
Glass Transition Temp, Tg 123 °C
253 °F
Zeon Chemicals Zeonex® 330R Cyclo-Olefin Polymer
Zeonex®330R has a lower birefringence than other Zeonex® products. This grade can satisfy market demands in the optical area where low birefringence and high dimensional stability in precision opt..
Glass Transition Temp, Tg 123 °C
253 °F
Solvay Specialty Polymers Amodel® EXT-1800 Polyphthalamide, extrusion  (discontinued **)
AMODEL EXT-1800 was developed specifically for the extrusion process. Unlike the grades targeted for injection molding, AMODEL EXT-1800 resin can be successfully extruded into tube, pipe, sheet, fil..