Tra-Con Tra-Bond FDA2 Food and Drug Application Epoxy Adhesive

Category Polymer , Adhesive , Thermoset , Epoxy
Manufacturer Tra-Con, Inc.
Trade Name Tra-Bond
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Tra-Con Tra-Bond FDA2 Food and Drug Application Epoxy Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TRA-BOND FDA-2 is a medium viscosity epoxy resin system specifically developed for medical device applications. It has been tested in accordance with USP biological reactivity tests, in vivo and received Class VI approval. This two-part amber adhesive is easily mixed, used and cured at room temperature for bonding, laminating and repair applications by manufacturers of food preparation, processing and packaging equipment, and by manufacturers of catheters, hearing aids, dental products and other biomedical instruments and devices. TRA-BOND FDA-2 is an effective electrical insulator, and it provides low permeability to gases and vapors, and good resistance to water, weather, galvanic action, to petroleum solvents, lubricants, and fuels, to mild acids and alkalis, and to many other organic and inorganic compounds.Information provided by Tra-Con Inc.
Physical Properties Metric English Comments
Specific Gravity 1.12 g/cc
1.12 g/cc
Mixed
Solids Content 100 %
100 %
Reactive Solids Content
Viscosity 14000 cP

@Temperature 25.0 °C
14000 cP

@Temperature 77.0 °F
After mixing
Mechanical Properties Metric English Comments
Hardness, Shore D 80
80
Elongation at Yield 9.0 %
9.0 %
Adhesive Bond Strength 12.4 MPa
1800 psi
Lap shear, alum to alum
Thermal Properties Metric English Comments
CTE, linear 53.0 µm/m-°C

@Temperature 20.0 °C
29.4 µin/in-°F

@Temperature 68.0 °F
Maximum Service Temperature, Air 145 °C
293 °F
Minimum Service Temperature, Air -70.0 °C
-94.0 °F
Glass Transition Temp, Tg 54.0 °C
129 °F
Ultimate Tg
Electrical Properties Metric English Comments
Volume Resistivity 1.20e+14 ohm-cm
1.20e+14 ohm-cm
Dielectric Constant 3.4

@Frequency 1000 Hz
3.4

@Frequency 1000 Hz
Dielectric Strength 16.5 kV/mm
420 kV/in
Dissipation Factor 0.020

@Frequency 1000 Hz
0.020

@Frequency 1000 Hz
Processing Properties Metric English Comments
Cure Time 60.0 - 240 min

@Temperature 65.0 °C
1.00 - 4.00 hour

@Temperature 149 °F
1440 min

@Temperature 25.0 °C
24.0 hour

@Temperature 77.0 °F
Pot Life 45 min
45 min
Descriptive Properties Value Comments
Color Amber
Mix Ratio, parts by weight 100/100
Resin/Hardener
Working Life hours 3