Thermal Properties Metric English Comments
Glass Transition Temp, Tg 77.0 - 81.0 °C
171 - 178 °F
QCD--W1-21
Pearl Engineering PEPLPET D-101-SH Monofilament Resin
Used in the paper industry as paper pulp nets.
Glass Transition Temp, Tg 77.0 - 81.0 °C
171 - 178 °F
QCD--W1-21
Pearl Engineering PEPLPET FR-101-H Monofilament Resin
Used as textile grade flame retardant for furniture, car and plane upholstery.
Glass Transition Temp, Tg 77.0 °C
171 °F
Eastman Eastapak 7352 PET  (discontinued **)
Unreinforced Low IV. ISO data as provided by the manufacturer, Eastman Chemical.This product is discontinued; 2003.
Glass Transition Temp, Tg 77.0 - 81.0 °C
171 - 178 °F
QCD--W1-21
Pearl Engineering PEPLPET B101H Monofilament Resin
Generally used in monofilament v-belts, zips and other technical applications.
Glass Transition Temp, Tg 77.0 °C
171 °F
Ultimate Tg
Tra-Con Tra-Bond 2113 Clear Low Viscosity Epoxy Adhesive
TRA-BOND 2113 is a clear, low viscosity epoxy adhesive system that contains no solvents, cures at room temperature, has excellent flowability and wetting characteristics, and adheres strongly to gla..
Glass Transition Temp, Tg 77.0 °C
171 °F
Ultimate Tg
Tra-Con Tra-Bond 2114 Water White Transparent Epoxy Adhesive
TRA-BOND 2114 is a transparent, low viscosity epoxy resin formulation recommended for industrial adhesive and laminating applications where sparkling clarity and excellent structural, mechanical and..
Glass Transition Temp, Tg 77.0 °C
171 °F
Dry
Hexcel® HexPly® F185 Epoxy Resin
HexPly® F185 is an advanced epoxy formulation designed for autoclave curing to offer very high sandwich and metal bonding strengths with moderate laminate strengths. HexPly® F185 is a structural a..
Glass Transition Temp, Tg 77.0 °C
171 °F
Eastman Eastar EN058 PET Copolymer
ISO data as provided by the manufacturer, Eastman Chemical
Glass Transition Temp, Tg 77.0 °C
171 °F
Internal Method
Eastman Embrace HY1000 Copolyester for Shrink Film
Applications:Beverage packagingCosmetics/personal care packagingDairy packagingFood packagingJuice packagingPharmaceutical packagingKey Attributes:Eye catching 360° graphic capabilityNoise-free shr..
Glass Transition Temp, Tg 77.0 °C
171 °F
Armstrong A-1/V Epoxy Adhesive
A brown epoxy paste formulated with enhanced wetting capabilities to hard rubbers and rigid thermoplastics. Has low outgassing characteristics at temperatures below 250°FInformation provided by El..
Glass Transition Temp, Tg 77.0 °C
171 °F
TM R050-25
Resinlab® EP11HT Gray Filled Epoxy Adhesive
Resinlab™ EP11HT Gray is a two part filled epoxy adhesive designed for bonding metals and plastics. It cures at room temperature to a tough, semi-rigid material. It has good wetting to most surfa..