Material Notes:
TRA-BOND 2114 is a transparent, low viscosity epoxy resin formulation recommended for industrial adhesive and laminating applications where sparkling clarity and excellent structural, mechanical and electrical properties are required. In addition, this 100% reactive solids (contains no solvents) adhesive system is easily mixed, handled and cured at room temperature, and it readily bonds to a wide variety of modern materials and surfaces (includes metals, glass, glass fabrics and glass products, ceramics, and many plastics). Fully cured TRA-BOND 2114 is a tough, strong, durable and almost water white electrical insulator which is resistant to water, gases and vapors, most petroleum products and fuels, salt solution, mild acids and alkalis, and many other organic and inorganic compounds. Information provided by Tra-Con Inc.
Physical Properties Metric English Comments
Specific Gravity 1.17 g/cc
1.17 g/cc
Mixed
Viscosity 640 cP

@Temperature 25.0 °C
640 cP

@Temperature 77.0 °F
After mixing
Mechanical Properties Metric English Comments
Hardness, Shore D 78
78
Tensile Strength, Yield 49.6 MPa
7200 psi
Adhesive Bond Strength 16.2 MPa
2350 psi
Lap shear, alum to alum, 1 hr @ 100°C
Thermal Properties Metric English Comments
CTE, linear 66.0 µm/m-°C

@Temperature 20.0 °C
36.7 µin/in-°F

@Temperature 68.0 °F
Maximum Service Temperature, Air 110 °C
230 °F
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
Glass Transition Temp, Tg 77.0 °C
171 °F
Ultimate Tg
Optical Properties Metric English Comments
Refractive Index 1.57
1.57
Transmission, Visible 90 %
90 %
transparent; thickness not quantified
Electrical Properties Metric English Comments
Volume Resistivity 3.50e+9 ohm-cm
3.50e+9 ohm-cm
Dielectric Constant 4.79

@Frequency 1000 Hz
4.79

@Frequency 1000 Hz
Dielectric Strength 16.1 kV/mm
410 kV/in
Dissipation Factor 0.010

@Frequency 1000 Hz
0.010

@Frequency 1000 Hz
Processing Properties Metric English Comments
Cure Time 480 min
8.00 hour
4 hrs @ 25°C + 4 hrs @ 65°C-plus
1440 min

@Temperature 25.0 °C
24.0 hour

@Temperature 77.0 °F
Pot Life 60 min
60 min
Descriptive Properties Value Comments
Color Transparent, Clear