Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 65.0 - 70.0 µm/m-°C | 36.1 - 38.9 µin/in-°F | Average value: 65.5 µm/m-°C Grade Count:16 |
Overview of materials for Polycarbonate, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Extruded". Each property range of values reported is minimum and maximum values of approp.. |
|||
CTE, linear, Transverse to Flow | 65.0 - 70.0 µm/m-°C | 36.1 - 38.9 µin/in-°F | Average value: 69.3 µm/m-°C Grade Count:21 |
Overview of materials for Polycarbonate, High Heat This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, High Heat". Each property range of values reported is minimum and maximum values of appro.. |
|||
CTE, linear, Transverse to Flow | 60.0 - 70.0 µm/m-°C | 33.3 - 38.9 µin/in-°F | Average value: 67.9 µm/m-°C Grade Count:11 |
Overview of materials for Polycarbonate, Optical Grade This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Optical Grade". Each property range of values reported is minimum and maximum values of a.. |
|||
CTE, linear, Transverse to Flow | 57.0 - 70.0 µm/m-°C | 31.7 - 38.9 µin/in-°F | Average value: 62.3 µm/m-°C Grade Count:6 |
Overview of materials for Polycarbonate, Gamma Radiation Resistant This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Gamma Radiation Resistant". Each property range of values reported is minimum and maximum.. |
|||
CTE, linear, Transverse to Flow | 36.0 - 70.0 µm/m-°C @Temperature 50.0 - 300 °C |
20.0 - 38.9 µin/in-°F @Temperature 122 - 572 °F |
Average value: 51.9 µm/m-°C Grade Count:10 |
Overview of materials for Polyimide This property data is a summary of similar materials in the MatWeb database for the category "Polyimide". Each property range of values reported is minimum and maximum values of appropriate MatWeb e.. |
|||
CTE, linear, Transverse to Flow | 45.0 - 70.0 µm/m-°C | 25.0 - 38.9 µin/in-°F | Average value: 59.8 µm/m-°C Grade Count:7 |
Overview of materials for Epoxy Encapsulant, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Encapsulant, Unreinforced". Each property range of values reported is minimum and maximum values o.. |
|||
CTE, linear, Transverse to Flow | 20.0 - 70.0 µm/m-°C | 11.1 - 38.9 µin/in-°F | Average value: 52.9 µm/m-°C Grade Count:11 |
Overview of materials for Nylon 6-3 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6-3". Each property range of values reported is minimum and maximum values of appropriate MatWeb e.. |
|||
CTE, linear, Transverse to Flow | 60.0 - 70.0 µm/m-°C | 33.3 - 38.9 µin/in-°F | Average value: 66.7 µm/m-°C Grade Count:3 |
Overview of materials for Nylon 63, 35% Glass-Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 63, 35% Glass-Filled". Each property range of values reported is minimum and maximum values of app.. |
|||
CTE, linear, Transverse to Flow | 60.0 - 70.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
33.3 - 38.9 µin/in-°F @Temperature 73.4 - 176 °F |
DIN 11359-1/-2 |
BASF Ultramid® B3EG5 25% Glass Filled PA6 (Dry) Description: 25% glass-fiber reinforced injection-molding grade for industrial articles and electrical insulating partsInformation provided by BASF |
|||
CTE, linear, Transverse to Flow | 60.0 - 70.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
33.3 - 38.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-1/-2 |
BASF Ultramid® B3EG6 30% Glass Filled PA6 (Dry) Ultramid B3EG6 is a 30% glass fiber reinforced injection molding PA6 grade. It conforms to FDA requirements of 21 CFR 177.1500. |
|||
CTE, linear, Transverse to Flow | 60.0 - 70.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
33.3 - 38.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-1/-2 |
BASF Ultramid® B3EG6 LS BK 23189 30% Glass Filled PA6 (Dry) Information provided by BASF |
|||
CTE, linear, Transverse to Flow | 60.0 - 70.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
33.3 - 38.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-1/-2 |
BASF Ultramid® B3EG7 35% Glass Filled PA6 (Dry) Description: 35% Glass fiber reinforced injection molding grade for industrial articles and electrical insulating parts.Information provided by BASF |
|||
CTE, linear, Transverse to Flow | 60.0 - 70.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
33.3 - 38.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-1/-2 |
BASF Ultramid® B3EG7 BK 00564 35% Glass Filled PA6 (Dry) Description: 35% Glass fiber reinforced injection molding grade for industrial articles and electrical insulating parts.Information provided by BASF |
|||
CTE, linear, Transverse to Flow | 55.0 - 70.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
30.6 - 38.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-1/-2 |
BASF Ultramid® B3G8 BK00564 40% Glass Filled PA6 (Dry) Ultramid B3G8 BK00564 is a 40% glass filled, pigmented black, injection molding PA6 grade. |
|||
CTE, linear, Transverse to Flow | 50.0 - 70.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
27.8 - 38.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-1/-2 |
BASF Ultramid® B3M6 BK 23213 30% Mineral Filled PA6 (Dry) Description: 30% Mineral-filled injection molding grade for high impact industrial items having very high dimensional stability, such as automobile wheel covers.Information provided by BASF |
|||
CTE, linear, Transverse to Flow | 60.0 - 70.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
33.3 - 38.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-1/-2 |
BASF Ultramid® B3ZG6 30% Glass Filled PA6 (Dry) Ultramid B3ZG6 is an impact-modified, 30% glass fiber reinforced injection molding PA6 grade for industrial items having very high impact strength and rigidity. |
|||
CTE, linear, Transverse to Flow | 60.0 - 70.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
33.3 - 38.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-1/-2 |
BASF Ultramid® B3ZG6 BK30564 30% Glass Filled PA6 (Dry) Ultramid B3ZG6 BK30564 is an impact-modified, pigmented black, 30% glass fiber reinforced injection molding PA6 grade for industrial items having very high impact strength and rigidity. |
|||
CTE, linear, Transverse to Flow | 60.0 - 70.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
33.3 - 38.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-1/-2 |
BASF Ultramid® A3EG5 25% Glass Filled PA66 (Dry) Description: Glass fiber reinforced injection molding grade for machinery components and housings of high stiffness and dimensional stability such as coil formers and bearing cages. Also used for el.. |
|||
CTE, linear, Transverse to Flow | 60.0 - 70.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
33.3 - 38.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359 |
BASF Ultramid® A3EG6 30% Glass Filled PA66 (Dry) Ultramid A3EG6 is a 30% glass fiber reinforced injection molding PA66 grade for machinery components and housings of high stiffness and dimensional stability. |
|||
CTE, linear, Transverse to Flow | 60.0 - 70.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
33.3 - 38.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-1/-2 |
BASF Ultramid® A3EG7 35% Glass Filled PA66 (Dry) Ultramid A3EG6 is a 35% glass fiber reinforced injection molding PA66 grade for machinery components and housings of high stiffness and dimensional stability. |
|||
CTE, linear, Transverse to Flow | 60.0 - 70.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
33.3 - 38.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-1/-2 |
BASF Ultramid® A3X2G7 35% Glass Filled PA66 (Dry) Ultramid A3X2G7 is a 35% glass fiber reinforced injection molding PA66 grade with improved flame retardance and enhanced long-term stability. Flame retardant based on red phosphorus; very high stif.. |
|||
CTE, linear, Transverse to Flow | 60.0 - 70.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
33.3 - 38.9 µin/in-°F @Temperature 73.4 - 176 °F |
DIN 11359-1/-2 |
BASF Ultramid® B3WG7 BK 00564 30% Glass Filled PA6 (Dry) Description: 35% glass-fiber reinforced and heat aging resistant injection-molding grade, e.g. for automotive manifolds and pedals.Information provided by BASF |
|||
CTE, linear, Transverse to Flow | 60.0 - 70.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
33.3 - 38.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-1/-2 |
BASF Ultramid® A3HG5 LS BK 23189 25% Glass Filled PA66 (Dry) Description: 25% glass fiber reinforced injection molding grade for machinery components and housings of high stiffness and dimensional stability such as coil formers and bearing cages. Also used fo.. |
|||
CTE, linear, Transverse to Flow | 50.0 - 70.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
27.8 - 38.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-1/-2 |
BASF Ultramid® B3M6 BK60564 30% Mineral Filled PA6 (Dry) ultramid B3M6 BK60564 is a 30% mineral reinforced, pigmented black injection molding PA6 grade for industrial items requiring high impact strength and very high dimensional stability, excellent lase.. |
|||
CTE, linear, Transverse to Flow | 50.0 - 70.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
27.8 - 38.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-1/-2 |
BASF Ultramid® B3M6 Grey 22319 Q94 30% Mineral Filled PA6 (Dry) Description: 30% Mineral-filled injection molding grade for high impact industrial items having very high dimensional stability, such as automobile wheel covers.Information provided by BASF |
|||
CTE, linear, Transverse to Flow | 64.0 - 70.0 µm/m-°C | 35.6 - 38.9 µin/in-°F | Average value: 66.0 µm/m-°C Grade Count:3 |
Overview of materials for Polycarbonate/ABS Alloy, Antistat/Conductive This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Antistat/Conductive". Each property range of values reported is minimum and max.. |
|||
CTE, linear, Transverse to Flow | 60.0 - 70.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
33.3 - 38.9 µin/in-°F @Temperature 73.4 - 176 °F |
DIN 11359-1/-2 |
BASF Ultramid® B3WG5 25% Glass Filled PA6 (Dry) Description: 25% glass-fiber reinforced and heat aging resistant injection-molding grade, for instance, for fan impeller glass-fiber reinforced injection-molding grade for industrial articles and el.. |
|||
CTE, linear, Transverse to Flow | 60.0 - 70.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
33.3 - 38.9 µin/in-°F @Temperature 73.4 - 176 °F |
DIN 11359-1/-2 |
BASF Ultramid® B3WG5 BK 00654 PA6 25% Glass Filled BK (Dry) Description: 25% glass-fiber reinforced and heat aging resistant injection-molding grade, for instance, for fan impeller glass-fiber reinforced injection-molding grade for industrial articles and el.. |
|||
CTE, linear, Transverse to Flow | 60.0 - 70.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
33.3 - 38.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-1/-2 |
BASF Ultramid® B3WG6 30% Glass Filled PA6 (Dry) Ultramid B3WG6 is a 30% glass fiber reinforced, heat stabilized injection molding PA6 grade. |
|||
CTE, linear, Transverse to Flow | 60.0 - 70.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
33.3 - 38.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-1/-2 |
BASF Ultramid® B3WG6 BK00564 30% Glass Filled PA6 (Dry) Ultramid B3WG6 BK00564 is a 30% glass fiber reinforced, pigmented black, heat stabilized injection molding PA6 grade. |