Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 73.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
40.6 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Cycoloy® C8080REC PC+ABS (Europe-Africa-Middle East) PC+ABS, Industrial quality resin with good flow, good temperature resistance and moderate ImpactThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
CTE, linear, Transverse to Flow | 73.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
40.6 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® FXD9945A PC UV stabilzed Visualfx FR PC with non-brominated and non-chlorinated flame retardant systems. It is available Only in white diffused effect(WH8B111X) meeting UL-94 V0 at 2mm for thin wall application.. |
|||
CTE, linear, Transverse to Flow | 73.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
40.6 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® FXD9945A PC (Asia Pacific) UV stabilzed Visualfx FR PC with non-brominated and non-chlorinated flame retardant systems. It is available Only in white diffused effect(WH8B111X) meeting UL-94 V0 at 2mm for thin wall application.. |
|||
CTE, linear, Transverse to Flow | 73.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
40.6 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Faradex NS0039XP PC+ABS (Europe-Africa-Middle East) LNP* FARADEX* NS0039XP is a compound based on PC/ABS resin containing Stainless Steel Fiber, Flame Retardant. Added features include: Electrically Conductive, EMI/RFI Shielding, Flame retardant.Thi.. |
|||
CTE, linear, Transverse to Flow | 73.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
40.6 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP DL001 PC (Europe-Africa-Middle East) LNP* LUBRICOMP* DL001 is a compound based on Polycarbonate resin containing PTFE. Added features include: Internally Lubricated. |
|||
CTE, linear, Transverse to Flow | 73.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
40.6 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Lubricomp DL002E PC (Europe-Africa-Middle East) LNP* Lubricomp* DL002E is a compound based on Polycarbonate resin containing PTFE. Added features include: Internally Lubricated, Easy Molding.This data was supplied by SABIC-IP for the Europe-Afric.. |
|||
CTE, linear, Transverse to Flow | 73.0 - 164 µm/m-°C | 40.6 - 91.1 µin/in-°F | Average value: 120 µm/m-°C Grade Count:7 |
Overview of materials for Thermoset Polyurethane, Liquid This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Liquid". Each property range of values reported is minimum and maximum values of.. |
|||
CTE, linear, Transverse to Flow | 73.0 µm/m-°C @Temperature 20.0 °C |
40.6 µin/in-°F @Temperature 68.0 °F |
|
Eastman Eastar DN007 PCTG Copolyester
(discontinued **) ISO data as provided by the manufacturer, Eastman Chemical |
|||
CTE, linear, Transverse to Flow | 73.1 µm/m-°C @Temperature 23.0 - 80.0 °C |
40.6 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® FXD163R PC (Europe-Africa-Middle East) FXD163R is a Lexan PC Transparent grade in our VisualFX Portfolio. It is a light Diffusion effect, developed for today´s Aesthetic Differentiation Needs. Color package may effect properties, Ap.. |
|||
CTE, linear, Transverse to Flow | 73.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
40.6 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® FXD9945A PC (Europe-Africa-Middle East) UV stabilzed Visualfx FR PC with non-brominated and non-chlorinated flame retardant systems. It is available Only in white diffused effect(WH8B111X) meeting UL-94 V0 at 2mm for thin wall application.. |
|||
CTE, linear, Transverse to Flow | 73.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
40.6 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP RL004 PA 66 (Europe-Africa-Middle East) LNP* Lubricomp* RL004 is a compound based on Nylon 66 resin containing PTFE. |
|||
CTE, linear, Transverse to Flow | 73.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
40.6 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP STAT-KON DEL329E PC (Asia Pacific) LNP* Stat-kon* DEL329E is a compound based on Polycarbonate resin containing PTFE, Flame Retardant, Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant, .. |
|||
CTE, linear, Transverse to Flow | 73.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
40.6 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP DX99077 PC (Europe-Africa-Middle East) LNP* Thermocomp* DX99077 is a compound based on Polycarbonate resin containing Flame Retardant, Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant, Non-.. |
|||
CTE, linear, Transverse to Flow | 73.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
40.6 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP KF005 Acetal Copolymer LNP THERMOCOMP* KF005 is a compound based on Acetal Copolymer resin containing 25% Glass Fiber. Added features of this material include: Chemically Coupled. |
|||
CTE, linear, Transverse to Flow | 73.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
40.6 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP RF007H PA 66 LNP* Thermocomp* RF007H is a compound based on Nylon 66 containing glass fiber. Added feature includes: Healthcare. |
|||
CTE, linear, Transverse to Flow | 73.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
40.6 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP RF007SXP PA 66 LNP* THERMOCOMP* RF007SXP is a compound based on Nylon 66 containing 35% Glass Fiber. Added feature of this material includes: Heat Stabilized. |
|||
CTE, linear, Transverse to Flow | 73.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
40.6 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP RFB71S PA 66 (Europe-Africa-Middle East) LNP* Thermocomp* RFB71S is a compound based on Nylon 66 resin containing Glass Fiber, Glass Bead. Added features of this material include: Heat Stabilized. |
|||
CTE, linear, Transverse to Flow | 73.0 µm/m-°C @Temperature 20.0 °C |
40.6 µin/in-°F @Temperature 68.0 °F |
|
Eastman Eastar DN003 PCTG Copolyester ISO data as provided by the manufacturer, Eastman Chemical |
|||
CTE, linear, Transverse to Flow | 73.0 µm/m-°C @Temperature 20.0 °C |
40.6 µin/in-°F @Temperature 68.0 °F |
|
Covestro Bayblend® KU 2-1481 Polycarbonate/ABS Blend Increased thermal stability during processing, slightly higher modulus of elasticity and slightly decreased low-temperature toughness compared to BAYBLEND T 85 MN.Information provided by Bayer.As of.. |
|||
CTE, linear, Transverse to Flow | 73.0 µm/m-°C @Temperature 20.0 °C |
40.6 µin/in-°F @Temperature 68.0 °F |
|
Covestro Baydur® 60 Polyurethane Rigid integral skin polyurethane foam for engineering components. The integral distribution of density gives a higher flexural modulus. If required, the property level can be improved by increasing .. |
|||
CTE, linear, Transverse to Flow | 73.0 µm/m-°C @Temperature -40.0 - 23.0 °C |
40.6 µin/in-°F @Temperature -40.0 - 73.4 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Rynite® FR530 BK507 Polyethylene Terephthalate (PET)
(Unverified Data**) 30% Glass Reinforced Flame Retardant Polyethylene Terephthalate Rynite FR530 BK507 is a 30% glass reinforced flame retardant modified polyethylene terephthalate resin.Information provided by DuPont .. |
|||
CTE, linear, Transverse to Flow | 73.0 µm/m-°C @Temperature -40.0 - 23.0 °C |
40.6 µin/in-°F @Temperature -40.0 - 73.4 °F |
DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® 77G43L BK031 Nylon 612
(Unverified Data**) 43% Glass Reinforced Polyamide 612Information provided by DuPont Performance Polymers |
|||
CTE, linear, Transverse to Flow | 73.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
40.6 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Staramide AG8 PA66, 40% Glass Fiber Reinforced, Injection Molding Staramide AG8 is a 40% Glass Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
CTE, linear, Transverse to Flow | 73.0 µm/m-°C @Temperature -40.0 - 23.0 °C |
40.6 µin/in-°F @Temperature -40.0 - 73.4 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Rynite® FR530L BK507 Polyethylene Terephthalate (PET) Rynite FR530 BK507 is a 30% glass reinforced flame retardant modified polyethylene terephthalate resin.Information provided by DuPont Performance Polymers |