Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP THERMOCOMP DX99077 PC (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Thermocomp* DX99077 is a compound based on Polycarbonate resin containing Flame Retardant, Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant, Non-Brominated & Non-Chlorinated Flame Retardant.
Physical Properties Metric English Comments
Density 1.22 g/cc
0.0441 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Elongation at Break 2.3 %
2.3 %
5 mm/min; ISO 527
Tensile Modulus 7.80 GPa
1130 ksi
1 mm/min; ISO 527
Flexural Yield Strength 172 MPa
24900 psi
2 mm/min; ISO 178
Flexural Modulus 6.30 GPa
914 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 7.00 kJ/m²
3.33 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 35.0 kJ/m²
16.7 ft-lb/in²
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 20.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
11.1 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
CTE, linear, Transverse to Flow 73.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
40.6 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 140 °C
284 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 136 °C
277 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
Flammability, UL94 V-0

@Thickness 1.60 mm
V-0

@Thickness 0.0630 in
UL 94
Electrical Properties Metric English Comments
Surface Resistance 1000 - 10000 ohm
1000 - 10000 ohm
ASTM D257