Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 95.0 - 110 µm/m-°C @Temperature 25.0 - 200 °C |
52.8 - 61.1 µin/in-°F @Temperature 77.0 - 392 °F |
ASTM D696 |
Polikim EFALON® B-40 PTFE, 40% Bronze Filled Bronze-filled Efalon® (PTFE) has better heat insulation, less thermal expansion, higher wear resistance properties and less deformation under load compared to virgin Efalon®. Applications: bearing.. |
|||
CTE, linear | 90.0 - 110 µm/m-°C @Temperature 25.0 - 200 °C |
50.0 - 61.1 µin/in-°F @Temperature 77.0 - 392 °F |
ASTM D696 |
Polikim EFALON® K-35 PTFE, 35% Carbon Filled K25 and K35 have less thermal expansion, higher wear resistance, less deformation under load properties compared to virgin Efalon® (PTFE). Applications: Bearings, piston rings, gaskets, seal rings... |