Polymer Property : CTE, linear = 61.1 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 95.0 - 110 µm/m-°C

@Temperature 25.0 - 200 °C
52.8 - 61.1 µin/in-°F

@Temperature 77.0 - 392 °F
ASTM D696
Polikim EFALON® B-40 PTFE, 40% Bronze Filled
Bronze-filled Efalon® (PTFE) has better heat insulation, less thermal expansion, higher wear resistance properties and less deformation under load compared to virgin Efalon®. Applications: bearing..
CTE, linear 90.0 - 110 µm/m-°C

@Temperature 25.0 - 200 °C
50.0 - 61.1 µin/in-°F

@Temperature 77.0 - 392 °F
ASTM D696
Polikim EFALON® K-35 PTFE, 35% Carbon Filled
K25 and K35 have less thermal expansion, higher wear resistance, less deformation under load properties compared to virgin Efalon® (PTFE). Applications: Bearings, piston rings, gaskets, seal rings...