Thermal Properties Metric English Comments
CTE, linear 90.0 µm/m-°C

@Temperature 23.0 - 100 °C
50.0 µin/in-°F

@Temperature 73.4 - 212 °F
Murtfeldt Murlubric® [FS] Oil Modified Nylon 6
Murlubric® is a modified cast polyamide that mineral oil is integrated into during polymerization. As a result, the material has self lubricating properties and retains its excellent characteristi..
CTE, linear 90.0 µm/m-°C

@Temperature 23.0 - 100 °C
50.0 µin/in-°F

@Temperature 73.4 - 212 °F
Murtfeldt Murlubric® Oil Modified Nylon 6
Murlubric® is a modified cast polyamide that mineral oil is integrated into during polymerization. As a result, the material has self lubricating properties and retains its excellent characteristi..
CTE, linear 90.0 µm/m-°C

@Temperature 23.0 - 100 °C
50.0 µin/in-°F

@Temperature 73.4 - 212 °F
Murtfeldt Murylon® 6 Cast Nylon 6
Murylon® 6 CAST has extremely low levels of residual stress thanks to the casting procedure used to produce it. This material is therefore ideally suited to extensively processed components.Specia..
CTE, linear 90.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
50.0 µin/in-°F

@Temperature 73.4 - 140 °F
Murtfeldt Murylon® B Nylon 6
Murylon® B natural has the best impact resistance of all Murylon materials. This material is especially suited for use in machine construction thanks to an excellent combination of mechanical prope..
CTE, linear 90.0 µm/m-°C

@Temperature 23.0 - 100 °C
50.0 µin/in-°F

@Temperature 73.4 - 212 °F
Murtfeldt Murylon® HT Nylon 46
The use of this highly temperature resistant polyamide enables reliable operation up to a constant service temperature of 155°C . The material retains its rigidity and creep strength over the entir..
CTE, linear 90.0 - 160 µm/m-°C

@Temperature 25.0 - 200 °C
50.0 - 88.9 µin/in-°F

@Temperature 77.0 - 392 °F
ASTM D696
Polikim EFALON® C-15 PTFE, 15% Glass Filled
C15 and C25 have less thermal expansion, higher wear resistance and less deformation under load compared to virgin Efalon® (PTFE). Applications: Seals, Seal rings, gaskets, valve sets, piston rings..
CTE, linear 90.0 - 110 µm/m-°C

@Temperature 25.0 - 200 °C
50.0 - 61.1 µin/in-°F

@Temperature 77.0 - 392 °F
ASTM D696
Polikim EFALON® K-35 PTFE, 35% Carbon Filled
K25 and K35 have less thermal expansion, higher wear resistance, less deformation under load properties compared to virgin Efalon® (PTFE). Applications: Bearings, piston rings, gaskets, seal rings...
CTE, linear 90.0 - 96.0 µm/m-°C

@Temperature 0.000 - 50.0 °C
50.0 - 53.3 µin/in-°F

@Temperature 32.0 - 122 °F
ASTM E831-00
Proto3000 WaterShed® XC 11122 Stereolithography (SLA) Prototyping Polymer
WaterShed XC is a low viscosity liquid photopolymer that produces strong, tough, water-resistant, ABS-like parts. Most importantly parts created with WaterShed 11122 are nearly colorless, and look ..
CTE, linear 90.0 µm/m-°C

@Temperature >=143 °C
50.0 µin/in-°F

@Temperature >=289 °F
Average above Tg; ISO 11359
Victrex® PEEK 450CA40 Polyetheretherketone, 40% Carbon Fibre Reinforced
Product Description:High performance thermoplastic material, 40% carbon fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, ..
CTE, linear 90.0 µm/m-°C

@Temperature >=143 °C
50.0 µin/in-°F

@Temperature >=289 °F
Average above Tg; ISO 11359
Victrex® PEEK 90CA30 Polyetheretherketone, 30% Carbon Fibre Reinforced
Product Description:High performance thermoplastic material, 30% carbon fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, very easy flow, FDA food cont..
CTE, linear 90.0 µm/m-°C

@Temperature >=152 °C
50.0 µin/in-°F

@Temperature >=306 °F
Average above Tg; ISO 11359
Victrex® PEEK -HT™ 22CA30 PolyEtherKetone, 30% Carbon Fibre Reinforced
Product Description:High performance thermoplastic material, 30% carbon fibre reinforced PolyEtherKetone (PEK), semi crystalline, granules for injection moulding, standard flow, FDA food contact com..
CTE, linear 90.0 µm/m-°C

@Temperature 93.3 - 238 °C
50.0 µin/in-°F

@Temperature 200 - 460 °F
ASTM D696
Ensinger ENSILON® 6/6 Extruded Nylon 6/6 (PA66)  (discontinued **)
ENSILON materials have high mechanical strength and superior resistance to wear and organic chemicals.Ensilon grades have been replaced by Tecamid.Information supplied by Ensinger, Inc.
CTE, linear 90.0 µm/m-°C

@Temperature -20.0 °C
50.0 µin/in-°F

@Temperature -4.00 °F
ASTM D696
Micropol Isoplas P501 Crosslinkable Polyethylene
Information provided by Micropol Limited
CTE, linear 90.0 µm/m-°C

@Temperature -20.0 °C
50.0 µin/in-°F

@Temperature -4.00 °F
ASTM D696
Micropol Isoplas P651 Crosslinkable Polyethylene
Information provided by Micropol Limited
CTE, linear 90.0 µm/m-°C

@Temperature -20.0 °C
50.0 µin/in-°F

@Temperature -4.00 °F
ASTM D696
Borealis BorPEX™ HE2515 High Density Polyethylene Compound for Silane Crosslinked Pipes
BorPEX HE2515 is a silane crosslinkable compound which is used together with a catalyst masterbatch (Cat-MB) to accelerate the moisture-induced crosslinking reaction. It is designed for flexible cr..
CTE, linear 90.0 µm/m-°C

@Temperature <=150 °C
50.0 µin/in-°F

@Temperature <=302 °F
ISO E 831
Wolf Kunststoff ZEDEX® ZX-530 A5D Polymer Alloy
Main Characteristics: Low Creep; Low moisture absorption; Flame retardant; Low impurity ions; Good machinability; FDA compliant LABS; Extremely low outgassing; Less expensive than PEEK; Stress resis..
CTE, linear 90.0 µm/m-°C

@Temperature -20.0 °C
50.0 µin/in-°F

@Temperature -4.00 °F
ASTM D696
Borealis BorPEX™ ME2510 Medium Density Polyethylene Compound for Crosslinked Pipes (Pex-B (Silane))
BorPEX ME2510 is a silane crosslinkable compound which is used together with a catalyst masterbatch (Cat-MB) to accelerate the moisture-induced crosslinking reaction. It is designed for crosslinkab..
CTE, linear 90.0 - 96.0 µm/m-°C

@Temperature 0.000 - 50.0 °C
50.0 - 53.3 µin/in-°F

@Temperature 32.0 - 122 °F
UV Postcure; ASTM E831-05
DSM Somos® BioClear
Parts created with Somos® BioClear are designed for medical applications that are non-implant and have limited contact with the body such as device prototyping. They are shatter-resistant so they w..
CTE, linear 90.0 - 95.7 µm/m-°C

@Temperature 100 - 150 °C
50.0 - 53.2 µin/in-°F

@Temperature 212 - 302 °F
ASTM E831-00
DSM Somos® NanoTool™ Resin for Stereolithography, UV Postcure
DescriptionNanoTool produces strong, stiff, high temperature resistant composite parts on conventional stereolithography machines. This third generation of Somos® ProtoComposite materials is heavi..
CTE, linear 90.0 - 96.0 µm/m-°C

@Temperature 0.000 - 50.0 °C
50.0 - 53.3 µin/in-°F

@Temperature 32.0 - 122 °F
ASTM E831-00
DSM Somos® WaterShed® XC 11122 Water-resistant resin for stereolithography
DescriptionWaterShed XC is a low viscosity liquid photopolymer that produces strong, tough, water-resistant, ABS-like parts. Most importantly parts created with WaterShed 11122 are nearly colorless..
CTE, linear 90.0 µm/m-°C

@Temperature 500 °C
50.0 µin/in-°F

@Temperature 932 °F
Dow SiLK™ D Semiconductor Dielectric Resin