Thermal Properties Metric English Comments
CTE, linear 95.0 µm/m-°C

@Temperature 23.0 - 100 °C
52.8 µin/in-°F

@Temperature 73.4 - 212 °F
Murtfeldt Murylon® A Nylon 66
This material combines the excellent properties of the Murylon® range with additional high tensile and compressive strength, increased wear resistance, and a lower level of moisture absorption than..
CTE, linear 95.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
52.8 µin/in-°F

@Temperature 73.4 - 140 °F
Murtfeldt Murytal® ESD Acetal Copolymer, Conductive
Additives make this material conductive. The mechanical properties of the material are retained almost in their entirety. Special Properties:• High rigidity• Excellent ability to regain its form•..
CTE, linear 95.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
52.8 µin/in-°F

@Temperature 73.4 - 140 °F
Murtfeldt Murytal® H Acetal Homopolymer
In addition to the excellent properties of Murytal® C, Murytal® H is stronger and more rigid with a lower expansion coefficient.Special Properties:• High rigidity• Excellent ability to regain it..
CTE, linear 95.0 - 110 µm/m-°C

@Temperature 25.0 - 200 °C
52.8 - 61.1 µin/in-°F

@Temperature 77.0 - 392 °F
ASTM D696
Polikim EFALON® B-40 PTFE, 40% Bronze Filled
Bronze-filled Efalon® (PTFE) has better heat insulation, less thermal expansion, higher wear resistance properties and less deformation under load compared to virgin Efalon®. Applications: bearing..
CTE, linear 95.0 - 100 µm/m-°C

@Temperature 25.0 - 100 °C
52.8 - 55.6 µin/in-°F

@Temperature 77.0 - 212 °F
ASTM D696
Polikim EFALON® K-25 PTFE, 25% Carbon Filled
K25 and K35 have less thermal expansion, higher wear resistance, less deformation under load properties compared to virgin Efalon® (PTFE). Applications: Bearings, piston rings, gaskets, seal rings...
CTE, linear 95.0 µm/m-°C

@Temperature 160 - 250 °C
52.8 µin/in-°F

@Temperature 320 - 482 °F
TD; ASTM E831
Solvay Specialty Polymers Amodel® A-1115 HS Polyphthalamide (PPA) Resin, 15% Glass Reinforced, Dry As Molded  
AMODEL A-1115 HS resin is a 15% glass reinforced, heat stabilized polyphthalamide (PPA) which exhibits a high deflection temperature, high flexural modulus, and high tensile strength. Excellent cre..
CTE, linear 95.0 µm/m-°C

@Temperature 160 - 250 °C
52.8 µin/in-°F

@Temperature 320 - 482 °F
TD; ASTM E831
Solvay Specialty Polymers Amodel® A-1240 HS Polyphthalamide (PPA) Resin, 40% Mineral Reinforced, Dry As Molded &nbs
AMODEL A-1240 polyphthalamide (PPA) resins are 40% mineral filled resins that have high deflection temperature, flexural modulus, and tensile strength. They mold with low warpage, have excellent di..
CTE, linear 95.0 µm/m-°C

@Temperature >=162 °C
52.8 µin/in-°F

@Temperature >=324 °F
Average above Tg; ISO 11359
Victrex® ST™ ST45CA30 PolyEtherKetoneEtherKetoneKetone, 30% Carbon Fibre Reinforced
Product Description:High performance thermoplastic material, 30% carbon fibre reinforced PolyEtherKetoneEtherKetoneKetone (PEKEKK), semi crystalline, granules for injection moulding, standard flow, ..
CTE, linear 95.0 µm/m-°C

@Temperature 200 - 300 °C
52.8 µin/in-°F

@Temperature 392 - 572 °F
ASTM E831
3M Dyneon™ TF 4103 PTFE 15% Glass Fiber Filled  (discontinued **)
Type II PTFE. Applications include valve seats, bearings, seals/gaskets, moldings, piston rings.Data provided by Dyneon.
CTE, linear 95.0 µm/m-°C

@Temperature 23.9 - 100 °C
52.8 µin/in-°F

@Temperature 75.0 - 212 °F
Tra-Con Tra-Bond Ablebond 724-1 Polyurethane Adhesive
Ablebond 724-1 premixed and frozen, polyurethane adhesive is designed for good adhesion, providing strong resilient bonds to a wide variety of substrates.Information provided by Tra-Con Inc.
CTE, linear 95.0 µm/m-°C

@Temperature 30.0 - 50.0 °C
52.8 µin/in-°F

@Temperature 86.0 - 122 °F
3D Systems Accura® Xtreme White 200 Plastic
Ultra tough white plastic to replace CNC Machined polypropylene and ABS articles FeaturesExceptionally tough and durableUsed for challenging functional assembliesUsed for snap fit assembl..
CTE, linear 95.0 µm/m-°C

@Temperature 20.0 °C
52.8 µin/in-°F

@Temperature 68.0 °F
Cured property; alpha 2; Perkin Elmer TMS-2
Aptek 6550-A/B Epoxy Encapsulant
High thermal conductivity, microelectronic grade blob-top encapsulant. Ultra high purity. Excellent heat and moisture protection for sensitive chips/circuitry. Premixed frozen syringes available for..
Copyright © lookpolymers.com All Rights Reserved