Maximum Service Temperature, Air 150 °C

@Time <=86400 sec
302 °F

@Time <=24.0 hour
Murtfeldt Murdopol® Nylon 12
Murdopol® has extremely high shock and impact resistance characteristics and good emergency running characteristics thanks to its high wear resistance. The main advantage of this material is its f..
Maximum Service Temperature, Air 150 °C

@Time 7.20e+7 sec
302 °F

@Time 20000 hour
Murtfeldt Murinyl® Polyvinylidinefluoride
As a fluorinated plastic, Murinyl® is exceptionally resistant to chemicals, hydrolysis, and sterilization. Its properties change very little at high service temperatures and after long-term exposur..
Maximum Service Temperature, Air 150 °C

@Time 1.80e+7 sec
302 °F

@Time 5000 hour
Murtfeldt Murylon® HT Nylon 46
The use of this highly temperature resistant polyamide enables reliable operation up to a constant service temperature of 155°C . The material retains its rigidity and creep strength over the entir..
Maximum Service Temperature, Air 150 °C

@Time <=86400 sec
302 °F

@Time <=24.0 hour
Murtfeldt Murytal® H Acetal Homopolymer
In addition to the excellent properties of Murytal® C, Murytal® H is stronger and more rigid with a lower expansion coefficient.Special Properties:• High rigidity• Excellent ability to regain it..
Maximum Service Temperature, Air 150 °C

@Time 7.20e+7 sec
302 °F

@Time 20000 hour
IEC 60216/T1
Raschig Group MELOPAS® 156 MF Melamine
Glass fiber reinforced Melamine molding compound. This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU directives 2002/95 (RoHS), 200..
Maximum Service Temperature, Air 150 °C

@Time 7.20e+7 sec
302 °F

@Time 20000 hour
IEC 60216/T1
Raschig Group RESINOL® 87120 EPF Phenolic
Glass-fiber reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and very good mechanical properties. This product meets ..
Maximum Service Temperature, Air 150 °C

@Time 7.20e+7 sec
302 °F

@Time 20000 hour
IEC 60216/T1
Raschig Group RESINOL® 400 EPF Phenolic
Glass-fiber reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and very good mechanical properties. This product meets ..