Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 90.0 - 100 °C
194 - 212 °F
ISO 75-2
Prodways PLASTCure Model 200 3D Printing Polymer
High temperature resistance.Thermoforming applicationsInformation provided by Genistar.
Deflection Temperature at 0.46 MPa (66 psi) 82.8 - 100 °C
181 - 212 °F
Average value: 94.2 °C Grade Count:37
Overview of materials for Polystyrene, Heat Resistant Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Heat Resistant Grade". Each property range of values reported is minimum and maximum values..
Deflection Temperature at 0.46 MPa (66 psi) 88.0 - 100 °C
190 - 212 °F
Average value: 94.8 °C Grade Count:3
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Carbon Black Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Carbon Black Filled". Each property range of values reported is m..
Deflection Temperature at 0.46 MPa (66 psi) 80.0 - 100 °C
176 - 212 °F
Average value: 92.0 °C Grade Count:12
Overview of materials for Ethylene Vinyl Alcohol (EVOH)
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Alcohol". Each property range of values reported is minimum and maximum values of appropr..
Deflection Temperature at 0.46 MPa (66 psi) 90.0 - 100 °C
194 - 212 °F
ASTM D1525, HDT Method B
Loxim 800 00 HB Polypropylene Compound, Flame Retardant
Information provided by Loxim Industries
Deflection Temperature at 0.46 MPa (66 psi) 95.0 - 100 °C
203 - 212 °F
C.O.I.M. EXTER S® S 107 Orthophthalic Resin
Description: The Exter S product line contains a large number of unsaturated polyester resin products with an array of properties and applications.Specific Notes for ESTER S® S 107: Resin for trans..
Deflection Temperature at 0.46 MPa (66 psi) 84.0 - 100 °C
183 - 212 °F
Average value: 94.7 °C Grade Count:3
Overview of materials for Polystyrene, Extrusion Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Extrusion Grade". Each property range of values reported is minimum and maximum values of a..
Deflection Temperature at 0.46 MPa (66 psi) 76.0 - 100 °C
169 - 212 °F
Average value: 85.1 °C Grade Count:9
Overview of materials for Styrene/Methyl Methacrylate Copolymer (SMMA)
This property data is a summary of similar materials in the MatWeb database for the category "Styrene/Methyl Methacrylate Copolymer (SMMA)". Each property range of values reported is minimum and max..
Deflection Temperature at 0.46 MPa (66 psi) 47.0 - 100 °C
117 - 212 °F
Average value: 77.4 °C Grade Count:7
Overview of materials for Thermoset Polyurethane Foam, Unreinforced