Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 47.0 °C | 117 °F | ASTM D648-06 |
Objet FullCure® 870 Vero Black Resin for Rapid Prototyping Information provided by American Precision Prototyping, LLC |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 47.0 °C | 117 °F | ASTM D648 |
NOVA Chemicals Novapol® TR-0735-U Hexene MDPE Rotational Molding Resin Good impact resistance, Excellent processabilityApplications: Toys, Complex custom parts, Home and garden items, MailboxesAdditives: Processing antioxidants, UV stabilizersInformation provided by NO.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 47.0 °C | 117 °F | ASTM D648 |
NOVA Chemicals Novapol® TR-0735-UG Hexene MDPE Rotational Molding Resin Features: Good impact properties Excellent processabilityNSF listed for Stds. 14, 24 and 61 Applications: ToysComplex custom partsHome and garden itemsMailboxesInformation provided by Nova Chemicals.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 47.0 °C | 117 °F | ASTM D648 |
NOVA Chemicals Novapol® PR-0636-UG Butene MDPE Rotational Molding Resin
(discontinued **) Very good processability, Very good ESCR, Good impact properties, NSF listed for Stds. 14, 24, and 61Applications: Toys, General purpose custom molding, Carts, Playground equipmentAdditives: Process.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 47.0 °C | 117 °F | ASTM D648 |
NOVA Chemicals Sclair® TD-7915-UG Hexene MDPE Rotational Molding Resin
(discontinued **) Excellent low temperature impact properties, Excellent ESCR, Wide process window, NSF listing for Stds. 14, 24, and 61 pending, Retention of impact at long cook timesApplications: IBCs, Toys, Genera.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 47.0 - 77.8 °C | 117 - 172 °F | Average value: 54.8 °C Grade Count:14 |
Overview of materials for Medium Density Polyethylene (MDPE), Molded This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Molded". Each property range of values reported is minimum and maxim.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 47.0 °C | 117 °F | ASTM D648 |
LyondellBasell Petrothene® GA564189 Linear Low Density Polyethylene, Injection Molding Grade PETROTHENE GA564189 exhibits good stiffness and low temperature toughness. Typical applications include trash cans, industrial containers, housewares and toys. Regulatory Status: GA564189 meets the .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 47.0 °C | 117 °F | |
Teknor Apex TEKRON® 4300-B88 2UV Grade Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 47.0 °C | 117 °F | |
Teknor Apex TEKRON® 4300-B88 UV Grade Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 47.0 °C @Thickness 3.20 mm |
117 °F @Thickness 0.126 in |
ISO 75 |
A. Schulman FORMION™ FI 401 Ionomer Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 47.0 °C @Thickness 3.20 mm |
117 °F @Thickness 0.126 in |
ISO 75 |
A. Schulman FORMION™ FI 401 Ionomer Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 47.0 °C @Thickness 3.20 mm |
117 °F @Thickness 0.126 in |
ISO 75 |
A. Schulman FORMION™ FI 401 Ionomer Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 47.0 °C @Thickness 3.20 mm |
117 °F @Thickness 0.126 in |
ISO 75 |
A. Schulman FORMION™ FI 401 Ionomer Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 47.0 °C @Thickness 3.20 mm |
117 °F @Thickness 0.126 in |
ISO 75 |
A. Schulman FORMION™ FI 401 Ionomer Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 47.0 °C @Thickness 3.20 mm |
117 °F @Thickness 0.126 in |
ISO 75 |
A. Schulman FORMION™ FI 401 Ionomer Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 47.0 °C | 117 °F | ASTM D648 |
Covestro Baydur® SFR-243 Polyurethane Composite RRIM Foam, MDI-based 2-Component Liquid System 0.25 in. thickness.Information provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – C.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 47.0 - 50.0 °C | 117 - 122 °F | ASTM D648-98c |
DSM Somos® 9420 Epoxy Resin for Stereolithography DescriptionDSM Somos® 9420 is a liquid photopolymer that produces robust, functional and accurate parts using stereolithography machines. The material offers superior chemical resistance and a wid.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 47.0 °C | 117 °F | ASTM D648 |
DuPont™ Surlyn® 9950 Ionomer Resin, Zinc Surlyn® 9950 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The amount of MAA and neutr.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 47.0 °C | 117 °F | ISO 75-1/-2 |
DuPont Performance Polymers Hytrel® HTR6108 TPC-ET
(Unverified Data**) Hytrel® HTR6108 is a medium modulus grade, specially designed for good flexibility and low permeability to hydrocarbon fuels and oils. It has nominal hardness of 61D and can be processed by various.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 47.0 °C | 117 °F | ASTM D648 |
3D Systems Accura® Xtreme White 200 Plastic Ultra tough white plastic to replace CNC Machined polypropylene and ABS articles FeaturesExceptionally tough and durableUsed for challenging functional assembliesUsed for snap fit assembl.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 47.0 °C | 117 °F | |
Arkema Group Orgalloy® LE 60THM Flexible Nylon Alloy (Conditioned) LE series, flexible polyamide alloys: processability on PE screw, low moisture absorption, chemical resistance (no known solvents).higher in rigidity than LE 6000. For film, hollow vessel blow moldi.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 47.0 °C | 117 °F | ASTM D648 |
NOVA Chemicals Sclair® TD-7915-U Hexene MDPE Rotational Molding Resin
(discontinued **) Excellent low temperature impact properties, Excellent ESCR, Wide process window, NSF listing for Stds. 14, 24, and 61 pending, Retention of impact at long cook timesApplications: IBCs, Toys, Genera.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 47.0 - 76.0 °C | 117 - 169 °F | Average value: 64.0 °C Grade Count:21 |
Overview of materials for Medium Density Polyethylene (MDPE), Rotational Molded This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Rotational Molded". Each property range of values reported is minimu.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 47.0 - 204 °C | 117 - 399 °F | Average value: 156 °C Grade Count:4 |
Overview of materials for Nylon, Flexible Alloy This property data is a summary of similar materials in the MatWeb database for the category "Nylon, Flexible Alloy". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 47.0 °C | 117 °F | ASTM D648 |
NOVA Chemicals Novapol® PR-0636-U Butene MDPE Rotational Molding Resin
(discontinued **) Very good processability, Very good ESCR, Good impact properties, NSF listed for Stds. 14, 24, and 61Applications: Toys, General purpose custom molding, Carts, Playground equipmentAdditives: Process.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 47.0 - 100 °C | 117 - 212 °F | Average value: 77.4 °C Grade Count:7 |
Overview of materials for Thermoset Polyurethane Foam, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane Foam, Unreinforced". Each property range of values reported is minimum and maximu.. |