Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

A. Schulman PP 1102-01 Polypropylene General Purpose, Molding Grade Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer A. Schulman, Inc.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman PP 1102-01 Polypropylene General Purpose, Molding Grade Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DescriptionPolypropylene PP 1102-01 is a general purpose, molding grade with UL 94 HB approval for use in large and thin wall applications. ApplicationPolypropylene PP 1102-01 meets FDA Regulation 21 CFR 177.1520 for all food contact applications.Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc
0.900 g/cc
ASTM D792
Melt Flow 12 g/10 min
12 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 95
95
ASTM D785
Tensile Strength, Yield 31.7 MPa
4600 psi
ASTM D638
Elongation at Break 8.0 %
8.0 %
ASTM D638
Flexural Modulus 1.31 GPa
190 ksi
ASTM D790
Izod Impact, Notched 0.267 J/cm
0.500 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 160 °C
320 °F
DSC
Deflection Temperature at 0.46 MPa (66 psi) 102 °C
216 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 62.0 °C
144 °F
ASTM D648
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved