Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C | 215 °F | Unannealed; ASTM D648 |
Multibase Multi-Pro® 1008 T Polypropylene Talc Filler, 10% by weight.Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C | 215 °F | ASTM D648 |
RheTech Products FT4700-00A Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: CladdingsBodyside moldingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C | 215 °F | ASTM D648 |
RheTech Products P102-00 Polypropylene, Black Applications: Consumer goodsIP structural componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C | 215 °F | ASTM D648 |
Polymer Resources PC/ASA-GP2 Polycarbonate/ASA Alloy Acrylonitrile Styrene Acrylate + PolycarbonatePreliminary DataProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.In.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C | 215 °F | ASTM D648 |
Polymer Resources PPX-GP4-WR Modified-PPO, General Purpose, Wear Resistant Modified-Polyphenylene Oxide, General Purpose, Wear Resistant, 215F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test s.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C | 215 °F | ASTM D648 |
RheTech Products HP516-01 7% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Black Applications: Interior trimCenter consolesHush panelsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C | 215 °F | Annealed, 0.125 in bars; ASTM D648 |
PolyOne Edgetek® AS-20GF/000 HI UV NAT Acrylonitrile Butadiene Styrene (ABS), Glass Filled
(discontinued **)& Description/Features:Glass Fiber ReinforcedHigh ImpactUV StabilizedNaturalUL 94 HBPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C | 215 °F | Unannealed; ASTM D648 |
PolyOne Stat-Tech™ AS-10SS/000 ABS - 10% Stainless Steel Fiber
(discontinued **) Data provided by PolyOne. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C | 215 °F | ASTM D648 |
Fiberfil® PP-61/CC/20 Polypropylene Copolymer, 20% Calcium Carbonate Information provided by FIBERFIL Engineered Plastics |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C | 215 °F | ASTM D648 |
Ineos T20N-00 Polypropylene Impact Copolymer This is a special high melt flow, nucleated, high impact copolymer polypropylene for injection molding applications. It offers excellent impact resistance and a high flexural modulus.ApplicationsCo.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C | 215 °F | Unannealed; ASTM D648 |
Techmer ES Elastoblend® PBT E IM SL3 Availability: North AmericaForms: PelletsAdditive: Impact Modifier and Silicone LubricantFeatures: Impact Modified and LubricatedInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C | 215 °F | Unannealed; ASTM D648 |
Techmer ES Electrablend® ABS CF10 FR BK 10% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 10% Filler by WeightFeatures: Flame RetardantAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C | 215 °F | Unannealed; ASTM D648 |
Techmer ES HiFill FR® ABS GF10 FR 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by WeightFeatures: Flame RetardantUL File Number: E157318Information provided by TP Composites, I.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C | 215 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® ABS GF10 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C | 215 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® ABS GF10 LE 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by WeightFeatures: Low ExtractablesInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C | 215 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® ABS GF5 5% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 5% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C | 215 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® ABS LG GF10 UV BK 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by WeightAdditive: UV StabilizerFeatures: Good UV Resistance and Low GlassAppearance: BlackInform.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C | 215 °F | ASTM D648 |
Spartech PE4325 Reinforced High Density Polyethylene Compound Spartech Polycom's filled high molecular weight, high density polyethylenes are specifically designed for blow molding and sheet extrusion /thermoforming of structural parts. These materials offer a.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C | 215 °F | ASTM D648 |
Spartech PP7120 Talc Filled High Impact Copolymer Good material choice for applications where low to medium levels of impact are required and where stiffness and heat deflection properties remain criticalInformation provided by Spartech |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C | 215 °F | Unannealed; ASTM D648 |
Techmer ES Electrablend® ABS 03011 BK MB Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/Reinfor.Features: Conductive, Electromagnetic Shielding (EMI) and Radio Frequency Shielding (RFI)Appearance: BlackIn.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C | 215 °F | Unannealed; ASTM D648 |
Techmer ES Electrablend® ABS SS7 BK MB 7% Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 7% Filler by WeightFeatures: ESD ProtectionAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C | 215 °F | Unannealed; ASTM D648 |
Techmer ES Electrablend® ABS SS7 MB 7% Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 7% Filler by WeightFeatures: ESD ProtectionInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C | 215 °F | ASTM D648 |
Washington Penn Homopolymer Polypropylene 30% Calcium Carbonate Filled Calcium carbonate-filled polypropylene compounds have been tailored specifically to meet the requirements of each of the major automobile producers. Grades are available to meet FDA food and drug pa.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C | 215 °F | ASTM D648 |
Aaron Industries AAROPRENE® CFIPP 2010 High Impact Calcium Carbonate Filled Polypropylene AAROPRENE® CFIPP 2000 Series Reinforced CompoundsMelt flow index may be specified. Color may be specified. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 - 123 °C | 215 - 253 °F | Average value: 114 °C Grade Count:10 |
Overview of materials for Acrylic/Polycarbonate Alloy This property data is a summary of similar materials in the MatWeb database for the category "Acrylic/Polycarbonate Alloy". Each property range of values reported is minimum and maximum values of ap.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C | 215 °F | ASTM D648 |
Polymer Resources PPX-GP4-WR Modified PPO, Wear Resistant with HDT of 215 F
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |