Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 88.9 °C | 192 °F | ASTM D648 |
RheTech Products RCC220-01 20% Calcium Carbonate Reinforced Polypropylene Copolymer, Black, Recycled Content Applications: I/P hush panelsSplash shieldsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 89.0 °C | 192 °F | ASTM D648 |
Network Polymers NPP 25-2003 Description: Copolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 89.0 °C | 192 °F | ASTM D648 |
Network Polymers NPP 25-2102 Description: Copolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 89.0 °C @Thickness 3.20 mm |
192 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Cycoloy® C6840 PC+ABS Cycoloy* C6840 resin is an injection moldable, flame retardant PC/ABS blend. It contains non-chlorinated & non-brominated flame retardant systems intended to meet governmental regulations and variou.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 89.0 °C @Thickness 3.20 mm |
192 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Cycoloy® C6840 PC+ABS (Asia Pacific) Cycoloy* C6840 resin is an injection moldable, flame retardant PC/ABS blend. It contains non-chlorinated & non-brominated flame retardant systems intended to meet governmental regulations and variou.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 89.0 °C | 192 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP Faradex NS0039 PC/ABS (Asia Pacific) LNP* Faradex* NS0039 is a compound based on PC/ABS resin containing Flame Retardant, Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding, Flame Reta.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 89.0 °C @Thickness 3.20 mm |
192 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Cycoloy® C6840 PC+ABS (Europe-Africa-Middle East) Cycoloy* C6840 resin is an injection moldable, flame retardant PC/ABS blend. It contains non-chlorinated & non-brominated flame retardant systems intended to meet governmental regulations and variou.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 89.0 °C | 192 °F | ASTM D648 |
LATI LATISTAT 30/R-05 High Impact Strength Polystyrene Base Conductive Plastic
(discontinued **) Description: Latistat materials have low specific resistivity. They feature partial electrical conductivity. Selected functional additives give materials with low specific resistivity and reasonable.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 89.0 °C | 192 °F | |
Ineos ABS Centrex® 814 ASA Blend
(discontinued **) Key Features:UnfilledHigh impact or high impact modifiedLight stabilized or stable to lightU.V. stabilized or stable to weatherSuitable processing methods:Injection moldingInformation provided by Ba.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 89.0 °C @Thickness 6.40 mm |
192 °F @Thickness 0.252 in |
Unannealed; ASTM D648 |
LG Chemical AF345 ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 40039-93-8 and 1309-64-4Information provided by LG Chemi.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 89.0 °C | 192 °F | |
Ineos ABS Lustran® 1152 Key Features:UnfilledHigh impact or high impact modifiedSuitable processing methods:Sheet extrusionThermoforming |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 89.0 °C | 192 °F | |
Ineos ABS Lustran® 648 Key Features:UnfilledHigh impact or high impact modifiedSuitable processing methods:Injection molding |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 89.0 °C | 192 °F | |
Ineos ABS Lustran® LGM Key Features:UnfilledSuitable processing methods:Injection molding |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 89.0 °C | 192 °F | ISO 75-1,-2 |
Inno-Comp INNOPOL® CS 2-2000 TO Polypropylene Block-Copolymer Based Compound INNOPOL® CS 2-2000 TO is a polypropylene block-copolymer based compound. This grade is available in natural and custom colored form.INNOPOL® CS 2-2000 TO is developed for producing injection m.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 88.9 °C | 192 °F | Unannealed; ASTM D648 |
Techmer ES HiFill FR® ABS FR AS Availability: North AmericaForms: PelletsAdditive: AntistaticFeatures: Antistatic and Flame RetardantInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 89.0 °C | 192 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP STAT-KON MX01767C PP LNP* STAT-KON* MX01767C is a compound based on Polypropylene containing Proprietary Filler(s). Added features of this grade include: Electrically Conductive, Clean Compounding System. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 88.9 °C | 192 °F | Unannealed; ASTM D648 |
Techmer ES Plastiblend® ABS 8007 Availability: North AmericaForms: PelletsFeatures: General Purpose and High FlowInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 89.0 °C | 192 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP Thermocomp MX01767C PP LNP* Stat-Kon* MX01767C is a compound based on Polypropylene containing Proprietary Fillers. Charactiers of this grade are Statically Conductive, Clean Compound System.This data was supplied by SAB.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 89.0 °C | 192 °F | ISO 75 |
Styrolution PS 476L HIPS Styrolution PS 476L is a normal flow and very high impact Polystyrene. It gives good mechanical and heat resistance properties while providing with easy processability and short cycle time.Normal fl.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 89.0 °C | 192 °F | ISO 75 |
Styrolution PS 495F HIPS Styrolution PS 495F is a high flow, high impact polystyrene with a good heat resistance and a high stiffness.High flow HIPSGood heat resistance with high stiffnessSuitable for gas-assisted injection.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 89.0 °C | 192 °F | ASTM Test |
Styrolution Terluran® GP-35 ABS Terluran GP-35 is a very high flow grade of ABS for injection molding with good resistance to impact and heat deflection.Information provided by STYROLUTION, which is a joint venture between BASF an.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 89.0 °C | 192 °F | annealed; ASTM Test |
Styrolution Terlux® 2812 TR MABS Terlux 2812 TR is a transparent grade of MABS for injection molding with high flowability.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 89.0 °C | 192 °F | ISO 75-2 |
Borealis Borcom™ WE007AE Polypropylene Borcom™ WE007AE is a polypropylene microcomposite intended for injection molding. The product is available in natural color. This material has an excellent balance between impact strength and stif.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 89.0 °C | 192 °F | ASTM D648 |
Total PPC M6823MZ Metallocene Isostatic Propylene Polymer TOTAL Petrochemicals Polypropylene M6823MZ is an isostatic form of copolymer polypropylene made via TOTAL Petrochemicals proprietary metallocene catalyst technology.Clarity. M6823MZ incorporates th.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 89.0 °C | 192 °F | ASTM D648 |
Total PPR 6827MZ Polypropylene, Random Copolymer - High Flow Clarified - for Injection Molding Clarity. TOTAL Polypropylene 6827MZ exhibits superior clarity and produces molded parts with improved impact compared with parts molded from homopolymer polypropylene.Antistat. 6827MZ contains an a.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 88.9 °C | 192 °F | annealed; ASTM D648 |
Arkema Group Solarkote® PB Acrylic For PVC/acrylic alloys Information provided by Arkema Group |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 88.9 °C | 192 °F | annealed; ASTM D648 |
Arkema Group Solarkote® A200 Acrylic Superior UV protection and weatherability, ASTM Classification PMMA 0233V1Information provided by Arkema Group |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 88.9 °C | 192 °F | ASTM D648 |
Ineos H19G-00 Polypropylene Homopolymer This is a homopolymer designed for extrusion processing and meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520.ApplicationsContinuous Filament YarnBCFSta.. |