Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 89.0 °C | 192 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
SABIC Innovative Plastics Cycolac® G320 ABS (Europe-Africa-Middle East) CYCOLAC G320 is a super high impact resistant ABS grade. It combines impact resistance with high stiffness, good temperature resistance and processability. It has a good fit in automotive interiors .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 89.0 °C | 192 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
SABIC Innovative Plastics Cycolac® GPM5500 ABS (Europe-Africa-Middle East) CYCOLAC GPM5500 is a multi purpose injection moulding grade, providing a favourable balance of engineering properties. CYCOLAC GPM5500 has a wide processing window. It is recommended for application.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 89.0 °C | 192 °F | ASTM D648 |
Network Polymers NPP 25-2002 Description: Copolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 89.0 °C | 192 °F | 120°C/h; ISO 75/1 |
Polykemi AB POLYabs XX0 ABS, Extrusion Grade Information provided by Polykemi AB |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 89.0 °C | 192 °F | |
Reliance Industries Polypropylene - Suzorite mica (untreated) filler Information provided by Reliance Industries |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 89.0 °C @Thickness 3.20 mm |
192 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Cycoloy® C6840 PC+ABS (Europe-Africa-Middle East) Cycoloy* C6840 resin is an injection moldable, flame retardant PC/ABS blend. It contains non-chlorinated & non-brominated flame retardant systems intended to meet governmental regulations and variou.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 89.0 °C | 192 °F | Unannealed; ASTM Data |
Americas Styrenics Styron® 495R High Impact Polystyrene
(discontinued **) Data provided by Dow Chemical.Americas Styrenics was formed in 2008 as a joint venture between Dow Chemical and Chevron Phillips Chemical Company. Styron was a Dow trade name before the JV formatio.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 89.0 °C | 192 °F | Unannealed; ASTM Data |
Americas Styrenics Styron® XL-8023VC High Impact Polystyrene
(discontinued **) STYRON® XL-8023 VC high impact polystyrene is designed to provide molders of VCR cassettes with the impact and gloss they require, at economics and processability highly advantaged over ABS resins... |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 89.0 °C | 192 °F | ASTM D648 |
LATI LATISTAT 30/R-05 High Impact Strength Polystyrene Base Conductive Plastic
(discontinued **) Description: Latistat materials have low specific resistivity. They feature partial electrical conductivity. Selected functional additives give materials with low specific resistivity and reasonable.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 89.0 °C | 192 °F | |
Ineos ABS Centrex® 813 ASA+AES Blend
(discontinued **) Key Features:UnfilledHigh impact or high impact modifiedLight stabilized or stable to lightU.V. stabilized or stable to weatherSuitable processing methods:Injection moldingInformation provided by Ba.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 89.0 °C | 192 °F | |
Ineos ABS Centrex® 811 ASA Blend
(discontinued **) Key Features:UnfilledHigh impact or high impact modifiedLight stabilized or stable to lightU.V. stabilized or stable to weatherSuitable processing methods:Injection moldingInformation provided by Ba.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 89.0 °C | 192 °F | |
Eastman Tenite 132E-28 Cellulose Acetate
(discontinued **) 28% Plasticized with 25% fiber grade ester.ISO data as provided by the manufacturer, Eastman Chemical. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 89.0 °C | 192 °F | ASTM D648 |
Flint Hills P5C4K-089 Random Copolymer Polypropylene Features: Good clarity. Product does not contain animal derived components. Phthalate-freeApplications: Cast FilmInformation provided by Flint Hills Resources. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 89.0 °C | 192 °F | ASTM D648 |
Flint Hills P5L2K-055 Polypropylene Random Copolymer Features: Excellent clarity. Product does not contain animal derived components. Phthalate-free.Applications: Injection molding: extrusion blow molding, injection blow molding, stretch blow moldin.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 89.0 °C @Thickness 6.40 mm |
192 °F @Thickness 0.252 in |
Unannealed; ASTM D648 |
LG Chemical AF342T ABS, Flame Retardant, High Impact Feature: Injection Molding, Flame Retardant, High ImpactApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 40039-93-8 and 1309-64-4Information provide.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 89.0 °C @Thickness 6.40 mm |
192 °F @Thickness 0.252 in |
Unannealed; ASTM D648 |
LG Chemical AF345 ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 40039-93-8 and 1309-64-4Information provided by LG Chemi.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 89.0 °C | 192 °F | |
Ineos ABS Lustran® 556 Key Features:UnfilledSuitable processing methods:Sheet extrusionThermoforming |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 89.0 °C | 192 °F | ISO 75-1,-2 |
Inno-Comp INNOPOL® CS 2-2000 TO Polypropylene Block-Copolymer Based Compound INNOPOL® CS 2-2000 TO is a polypropylene block-copolymer based compound. This grade is available in natural and custom colored form.INNOPOL® CS 2-2000 TO is developed for producing injection m.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 89.0 °C | 192 °F | annealed; ASTM D648 |
Lendell Parapet GR-00100 PMMA, High Impact |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 89.0 °C | 192 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP STAT-KON MX01767C PP LNP* STAT-KON* MX01767C is a compound based on Polypropylene containing Proprietary Filler(s). Added features of this grade include: Electrically Conductive, Clean Compounding System. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 89.0 °C | 192 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP THERMOCOMP 2Z004 ETFE LNP* THERMOCOMP* 2Z004 is a compound based on ETFE resin containing 20% Milled Glass. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 89.0 °C | 192 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP Thermocomp MX01767C PP LNP* Stat-Kon* MX01767C is a compound based on Polypropylene containing Proprietary Fillers. Charactiers of this grade are Statically Conductive, Clean Compound System.This data was supplied by SAB.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 89.0 °C @Thickness 6.40 mm |
192 °F @Thickness 0.252 in |
ASTM D648 |
Samsung Cheil Industries Starex® VE-0558 ABS, Unreinforced FR Flame-retardant ABS with excellent weather resistance that is used in the exterior of OA devices such as monitors, printers, fax machines, duplicators etc.Information provided by Samsung Cheil Indus.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 89.0 °C | 192 °F | ISO 75-2 |
Borealis BL2631 High Density Polyethylene BL2631 is a high density polyethylene homopolymer intended for blow molding of products requiring high toughness and stiffness. Applications: fresh milk bottles, and juice bottles.Information provi.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 89.0 °C | 192 °F | ISO 75-2 |
Borealis Daplen™ EE015U TPO Compound Daplen EE015U is a 10% mineral and elastomer modified polypropylene compound intended for injection molding. Daplen EE015U is a material with excellent impact /stiffness ratio. Thanks to its low th.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 89.0 °C | 192 °F | |
Eastman Eastar DN003 PCTG Copolyester ISO data as provided by the manufacturer, Eastman Chemical |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 89.0 °C | 192 °F | ASTM D648 |
Eastman Tenite 485E3720008 Cellulose Acetate Butyrate, Clear, Trsp Applications:Toys/Sporting goodsProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties including toughness, hardness, strength, surface gloss, clarity,.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 89.0 °C @Thickness 6.40 mm |
192 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics NORYL FN170X PPE+PS Foamable resin. All properties at 10% density reduction; 0.250"" thick test specimens. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 89.0 °C | 192 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP Stat-kon MX01767C PP LNP* Stat-Kon* MX01767C is a compound based on Polypropylene containing Proprietary Fillers. Charactiers of this grade are Statically Conductive, Clean Compound System.This data was supplied by SAB.. |