Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 10% Calcium Carbonate (CaCO3) Filler
Manufacturer Aaron Industries Corporation
Trade Name AAROPRENE® CFIPP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aaron Industries AAROPRENE® CFIPP 2010 High Impact Calcium Carbonate Filled Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AAROPRENE® CFIPP 2000 Series Reinforced CompoundsMelt flow index may be specified. Color may be specified.
Physical Properties Metric English Comments
Specific Gravity 0.970 g/cc
0.970 g/cc
ASTM D792
Filler Content 10 %
10 %
Calcium Carbonate; ASTM D2584
Linear Mold Shrinkage 0.012 cm/cm
0.012 in/in
ASTM D955
Melt Flow 8.0 - 12 g/10 min

@Load 2.16 kg,
Temperature 230 °C
8.0 - 12 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength 25.2 MPa
3650 psi
ASTM D638
Flexural Modulus 1.45 GPa
210 ksi
ASTM D790
Izod Impact, Notched 0.897 J/cm
1.68 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 102 °C
215 °F
ASTM D648
Users viewing this material also viewed the following: