Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 233 °C | 451 °F | ASTM D648 |
Nilit Polynil® P240HSLV High Viscosity, Heat Stabilized Nylon 66 Description: Polynil P240 HSLV was developed for injection molding applications, where a combination of heat aging resistance, abrasion resistance and impact strength is needed, such as chain tensio.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 233 °C | 451 °F | 20% Glass Laminate; unspecified load |
TSE Industries EcoSPRAY® 350c Flame-Retardant Polyurethane Resin TSE-EcoSPRAY® 350c is an “Environmentally-Preferred Product” or EPP. It is a Thixotropic flame retardant polyurethane resin free of Styrene, and is an “ultra-low” emitting resin during applica.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 233 °C | 451 °F | 21% Glass Spray-up Laminate |
TSE Industries EcoSPRAY® 350c Flame-Retardant Polyurethane Resin TSE-EcoSPRAY® 350c is an “Environmentally-Preferred Product” or EPP. It is a Thixotropic flame retardant polyurethane resin free of Styrene, and is an “ultra-low” emitting resin during applica.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 233 °C | 451 °F | 20% Glass RTM Laminate |
TSE Industries EcoSPRAY® 350c Flame-Retardant Polyurethane Resin TSE-EcoSPRAY® 350c is an “Environmentally-Preferred Product” or EPP. It is a Thixotropic flame retardant polyurethane resin free of Styrene, and is an “ultra-low” emitting resin during applica.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 233 °C | 451 °F | ASTM D648 |
Samyang Tramid® 210 Polyamide, General Purpose Strong with excellent thermal resistance. Abrasion resistance, chemical resistance and oil resistance are excellent.210 is a general purpose grade.Applications:Automotive gear level housingConnecto.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 233 °C | 451 °F | ASTM D648 |
Samyang Tramid® 210F Polyamide, High Productivity Strong with excellent thermal resistance. Abrasion resistance, chemical resistance and oil resistance are excellent.210F is a high productivity grade.Applications:ConnectorsCable tiesHarness clipsT.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 233 °C | 451 °F | ASTM D648 |
Samyang Tramid® 210P Polyamide, High Productivity Strong with excellent thermal resistance. Abrasion resistance, chemical resistance and oil resistance are excellent.210P is a high productivity grade.Applications:ConnectorsCable tiesHarness clipsT.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 233 °C @Thickness 3.20 mm |
451 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP THERMOCOMP RB004 PA 66 LNP* THERMOCOMP* RB004 is a compound based on Nylon 66 containing Glass Beads. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 233 °C | 451 °F | 20% Glass Laminate; unspecified load |
TSE Industries EcoSPRAY® 350c Flame-Retardant Polyurethane Resin TSE-EcoSPRAY® 350c is an “Environmentally-Preferred Product” or EPP. It is a Thixotropic flame retardant polyurethane resin free of Styrene, and is an “ultra-low” emitting resin during applica.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 233 °C | 451 °F | 21% Glass Spray-up Laminate |
TSE Industries EcoSPRAY® 350c Flame-Retardant Polyurethane Resin TSE-EcoSPRAY® 350c is an “Environmentally-Preferred Product” or EPP. It is a Thixotropic flame retardant polyurethane resin free of Styrene, and is an “ultra-low” emitting resin during applica.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 233 °C | 451 °F | 20% Glass RTM Laminate |
TSE Industries EcoSPRAY® 350c Flame-Retardant Polyurethane Resin TSE-EcoSPRAY® 350c is an “Environmentally-Preferred Product” or EPP. It is a Thixotropic flame retardant polyurethane resin free of Styrene, and is an “ultra-low” emitting resin during applica.. |