Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 233 °C
451 °F
ASTM D648
Nilit Polynil® P240HSLV High Viscosity, Heat Stabilized Nylon 66
Description: Polynil P240 HSLV was developed for injection molding applications, where a combination of heat aging resistance, abrasion resistance and impact strength is needed, such as chain tensio..
Deflection Temperature at 0.46 MPa (66 psi) 233 °C
451 °F
20% Glass Laminate; unspecified load
TSE Industries EcoSPRAY® 350c Flame-Retardant Polyurethane Resin
TSE-EcoSPRAY® 350c is an “Environmentally-Preferred Product” or EPP. It is a Thixotropic flame retardant polyurethane resin free of Styrene, and is an “ultra-low” emitting resin during applica..
Deflection Temperature at 0.46 MPa (66 psi) 233 °C
451 °F
21% Glass Spray-up Laminate
TSE Industries EcoSPRAY® 350c Flame-Retardant Polyurethane Resin
TSE-EcoSPRAY® 350c is an “Environmentally-Preferred Product” or EPP. It is a Thixotropic flame retardant polyurethane resin free of Styrene, and is an “ultra-low” emitting resin during applica..
Deflection Temperature at 0.46 MPa (66 psi) 233 °C
451 °F
20% Glass RTM Laminate
TSE Industries EcoSPRAY® 350c Flame-Retardant Polyurethane Resin
TSE-EcoSPRAY® 350c is an “Environmentally-Preferred Product” or EPP. It is a Thixotropic flame retardant polyurethane resin free of Styrene, and is an “ultra-low” emitting resin during applica..
Deflection Temperature at 0.46 MPa (66 psi) 233 °C
451 °F
ASTM D648
Samyang Tramid® 210 Polyamide, General Purpose
Strong with excellent thermal resistance. Abrasion resistance, chemical resistance and oil resistance are excellent.210 is a general purpose grade.Applications:Automotive gear level housingConnecto..
Deflection Temperature at 0.46 MPa (66 psi) 233 °C
451 °F
ASTM D648
Samyang Tramid® 210F Polyamide, High Productivity
Strong with excellent thermal resistance. Abrasion resistance, chemical resistance and oil resistance are excellent.210F is a high productivity grade.Applications:ConnectorsCable tiesHarness clipsT..
Deflection Temperature at 0.46 MPa (66 psi) 233 °C
451 °F
ASTM D648
Samyang Tramid® 210P Polyamide, High Productivity
Strong with excellent thermal resistance. Abrasion resistance, chemical resistance and oil resistance are excellent.210P is a high productivity grade.Applications:ConnectorsCable tiesHarness clipsT..
Deflection Temperature at 0.46 MPa (66 psi) 233 °C

@Thickness 3.20 mm
451 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP THERMOCOMP RB004 PA 66
LNP* THERMOCOMP* RB004 is a compound based on Nylon 66 containing Glass Beads.
Deflection Temperature at 0.46 MPa (66 psi) 233 °C
451 °F
20% Glass Laminate; unspecified load
TSE Industries EcoSPRAY® 350c Flame-Retardant Polyurethane Resin
TSE-EcoSPRAY® 350c is an “Environmentally-Preferred Product” or EPP. It is a Thixotropic flame retardant polyurethane resin free of Styrene, and is an “ultra-low” emitting resin during applica..
Deflection Temperature at 0.46 MPa (66 psi) 233 °C
451 °F
21% Glass Spray-up Laminate
TSE Industries EcoSPRAY® 350c Flame-Retardant Polyurethane Resin
TSE-EcoSPRAY® 350c is an “Environmentally-Preferred Product” or EPP. It is a Thixotropic flame retardant polyurethane resin free of Styrene, and is an “ultra-low” emitting resin during applica..
Deflection Temperature at 0.46 MPa (66 psi) 233 °C
451 °F
20% Glass RTM Laminate
TSE Industries EcoSPRAY® 350c Flame-Retardant Polyurethane Resin
TSE-EcoSPRAY® 350c is an “Environmentally-Preferred Product” or EPP. It is a Thixotropic flame retardant polyurethane resin free of Styrene, and is an “ultra-low” emitting resin during applica..