Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 67.0 - 195 °C | 153 - 383 °F | Average value: 142 °C Grade Count:5 |
Overview of materials for Thermoset Polyurethane, Liquid This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Liquid". Each property range of values reported is minimum and maximum values of.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 82.0 - 195 °C | 180 - 383 °F | Average value: 107 °C Grade Count:46 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled". Specific grades with glass content betwe.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 142 - 195 °C | 288 - 383 °F | Average value: 166 °C Grade Count:32 |
Overview of materials for Polycarbonate, High Heat This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, High Heat". Each property range of values reported is minimum and maximum values of appro.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 180 - 195 °C | 356 - 383 °F | V-notch; ISO R 75 |
Schwartz Technical Plastics LAMIGAMID® 400 Cast Polyamide 6, Elastomer Modified, Dry Application: gear-wheels, chain-wheels, hydrocyclones, housings, outrigger floatsInformation provided by Schwartz Technical Plastics GmbH |